15-5 PH Stainless Steel is a precipitation-hardening stainless steel that combines high strength and corrosion resistance with good fabricability. Classified as a martensitic stainless steel, it contains significant amounts of chromium and nickel, along with copper, which enhances its hardening response. The primary alloying elements include:

  • Chromium (Cr): Provides corrosion resistance and contributes to the steel's hardness.
  • Nickel (Ni): Enhances toughness and ductility, improving the steel's overall performance.
  • Copper (Cu): Aids in precipitation hardening, increasing strength without compromising corrosion resistance.

Characteristics and Properties

15-5 PH exhibits several notable characteristics:

  • High Strength: Achieves high tensile and yield strength, making it suitable for demanding applications.
  • Corrosion Resistance: Offers excellent resistance to a variety of corrosive environments, including atmospheric conditions and some acidic environments.
  • Good Fabricability: Can be easily machined and welded, which is advantageous in manufacturing processes.

Advantages and Limitations

Pros Cons
High strength-to-weight ratio Limited high-temperature performance
Excellent corrosion resistance May require post-weld heat treatment
Good machinability and weldability Higher cost compared to some other stainless steels

Historically, 15-5 PH has been widely used in aerospace, chemical processing, and other industries where high strength and corrosion resistance are critical. Its market position is strong, particularly in applications requiring a combination of mechanical properties and resistance to harsh environments.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS S15500 USA Closest equivalent to AISI 630
AISI/SAE 15-5 PH USA Precipitation hardening grade
ASTM A564 USA Specification for precipitation hardening stainless steels
EN 1.4545 Europe Similar properties but may have slight compositional differences
JIS SUS630 Japan Comparable grade with minor differences

The differences between these equivalent grades often lie in their specific compositions and mechanical properties, which can affect their performance in particular applications. For instance, while UNS S15500 and AISI 630 are similar, slight variations in nickel and copper content can influence corrosion resistance and strength.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
Chromium (Cr) 15.0 - 17.5
Nickel (Ni) 3.0 - 5.0
Copper (Cu) 3.0 - 5.0
Manganese (Mn) 1.0 max
Silicon (Si) 1.0 max
Carbon (C) 0.07 max
Phosphorus (P) 0.04 max
Sulfur (S) 0.03 max

The primary role of chromium is to enhance corrosion resistance, while nickel improves toughness and ductility. Copper plays a crucial role in the precipitation hardening process, significantly increasing the strength of the steel without compromising its corrosion resistance.

Mechanical Properties

Property Condition/Temper Test Temperature Typical Value/Range (Metric - SI Units) Typical Value/Range (Imperial Units) Reference Standard for Test Method
Tensile Strength Annealed Room Temp 930 - 1,100 MPa 135 - 160 ksi ASTM E8
Yield Strength (0.2% offset) Annealed Room Temp 620 - 850 MPa 90 - 123 ksi ASTM E8
Elongation Annealed Room Temp 10 - 15% 10 - 15% ASTM E8
Hardness (Rockwell) Annealed Room Temp 30 - 40 HRC 30 - 40 HRC ASTM E18
Impact Strength Quenched & Tempered -40°C 40 J 29.5 ft-lbf ASTM E23

The combination of high tensile and yield strength makes 15-5 PH suitable for applications that require structural integrity under mechanical loading. Its good elongation values indicate that it can withstand deformation without fracturing, which is essential in dynamic applications.

Physical Properties

Property Condition/Temperature Value (Metric - SI Units) Value (Imperial Units)
Density Room Temp 7.8 g/cm³ 0.283 lb/in³
Melting Point - 1,400 - 1,500 °C 2,552 - 2,732 °F
Thermal Conductivity Room Temp 16 W/m·K 92 BTU·in/ft²·h·°F
Specific Heat Capacity Room Temp 500 J/kg·K 0.12 BTU/lb·°F
Electrical Resistivity Room Temp 0.73 µΩ·m 0.0000013 Ω·in

The density of 15-5 PH makes it a lightweight option for applications where weight savings are critical. Its thermal conductivity is moderate, which is beneficial in applications where heat dissipation is necessary, while its specific heat capacity indicates good thermal stability.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides 3.5% 25°C/77°F Good Risk of pitting
Sulfuric Acid 10% 25°C/77°F Fair Susceptible to stress corrosion cracking
Acetic Acid 5% 25°C/77°F Excellent Resistant to localized corrosion
Atmospheric - - Excellent Good for outdoor applications

15-5 PH exhibits excellent resistance to atmospheric corrosion and is suitable for marine environments. However, it is susceptible to pitting in chloride-rich environments and stress corrosion cracking in the presence of sulfuric acid. Compared to grades like 304 and 316 stainless steels, 15-5 PH offers superior strength but may have lower resistance to certain corrosive agents, particularly in high-chloride environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 300°C 572°F Suitable for high-temperature applications
Max Intermittent Service Temp 400°C 752°F Can withstand short-term exposure to higher temperatures
Scaling Temperature 600°C 1,112°F Begins to lose mechanical properties

At elevated temperatures, 15-5 PH maintains good oxidation resistance but may experience a reduction in mechanical properties. Care should be taken in applications involving prolonged exposure to high temperatures, as this can lead to decreased strength and potential scaling.

Fabrication Properties

Weldability
Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
TIG ER 630 Argon Preheat recommended
MIG ER 630 Argon Post-weld heat treatment may be required

15-5 PH is generally considered weldable, but preheating and post-weld heat treatment are often necessary to avoid cracking and ensure optimal mechanical properties. The use of appropriate filler metals is crucial to maintain corrosion resistance and strength in the weld area.

Machinability
Machining Parameter [15-5 PH] [AISI 1212] Notes/Tips
Relative Machinability Index 60% 100% Requires slower cutting speeds
Typical Cutting Speed (Turning) 30 m/min 50 m/min Use carbide tools for best results

Machinability is moderate, and while it can be machined effectively, slower cutting speeds and specialized tooling are recommended to achieve optimal results and prevent tool wear.

Formability

15-5 PH can be cold formed, but its work hardening characteristics may limit the extent of deformation. Hot forming is also possible, but care must be taken to avoid excessive temperatures that could lead to loss of mechanical properties.

Heat Treatment
Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Solution Annealing 1,000 - 1,100°C / 1,832 - 2,012°F 1 hour Air cool Dissolves precipitates
Aging 480 - 620°C / 896 - 1,148°F 4 - 8 hours Air cool Increases strength through precipitation hardening

The heat treatment process involves solution annealing followed by aging, which enhances the steel's strength through the formation of fine precipitates. This process significantly alters the microstructure, leading to improved mechanical properties.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Aerospace Aircraft components High strength, corrosion resistance Critical for safety and performance
Chemical Processing Valve bodies Corrosion resistance Essential for harsh environments
Oil & Gas Pump shafts High strength, toughness Required for demanding conditions
Medical Devices Surgical instruments Biocompatibility, corrosion resistance Safety and reliability are paramount

Other applications include:

    • Marine hardware
    • Food processing equipment
    • Automotive components

15-5 PH is chosen for applications requiring a combination of high strength and corrosion resistance, particularly in environments where mechanical integrity is critical.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property [15-5 PH] [AISI 304] [AISI 316] Brief Pro/Con or Trade-off Note
Key Mechanical Property High strength Moderate strength Moderate strength 15-5 PH offers superior strength
Key Corrosion Aspect Good in many environments Excellent in most Excellent in chlorides 15-5 PH may corrode in chlorides
Weldability Moderate Good Good 15-5 PH requires careful handling
Machinability Moderate Good Good 15-5 PH is less machinable
Formability Moderate Good Good 15-5 PH is less formable
Approx. Relative Cost Higher Moderate Moderate Cost reflects performance benefits
Typical Availability Moderate High High 15-5 PH is less common

When selecting 15-5 PH, considerations include its cost-effectiveness, availability, and specific performance requirements. While it may be more expensive than other stainless steels, its unique combination of properties often justifies the investment, especially in high-performance applications. Safety and reliability are paramount in industries like aerospace and medical, where 15-5 PH's properties can significantly impact performance and durability.

In summary, 15-5 PH stainless steel is a versatile material that excels in applications requiring high strength and corrosion resistance, making it a preferred choice in demanding environments.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS S15500, ASTM A564, EN 1.4545, JIS SUS630). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

Leave a comment