TP304 vs TP316 – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

TP304 and TP316 are two of the most commonly specified austenitic stainless steels for tubing and plate products. Engineers, procurement managers, and fabricators frequently decide between them when balancing corrosion resistance, weldability, mechanical performance, and cost. Typical decision contexts include: selecting a material for process piping exposed to chlorides, specifying heat exchangers or structural tubing for offshore installations, and choosing sanitary equipment for food and pharmaceutical manufacture.

The fundamental practical distinction is that one grade includes an alloying element that enhances resistance to pitting and crevice corrosion in chloride-containing environments, while the other is the more economical, widely available general-purpose austenitic stainless steel. Because they are otherwise similar in metallurgy and fabrication behavior, comparing TP304 and TP316 often comes down to corrosion environment, life-cycle cost, and specific fabrication constraints.

1. Standards and Designations

  • Common ASTM/ASME: TP304 and TP316 are used in ASTM A312/A213/A269/A240 family designations for stainless tubing and plate. In ASME practice the "TP" prefix indicates tube product specification (e.g., TP304).
  • UNS/EN/JIS/GB equivalents:
  • TP304 ≈ UNS S30400; EN 1.4301 (AISI 304); JIS SUS304; GB 06Cr19Ni10.
  • TP316 ≈ UNS S31600; EN 1.4401/1.4404 (AISI 316/316L); JIS SUS316; GB 00Cr17Ni14Mo2 (variants may differ).
  • Material class: Both are austenitic stainless steels (non-magnetic in fully annealed condition) — not carbon steel, alloy steel, tool steel, or HSLA.

2. Chemical Composition and Alloying Strategy

Table: Typical nominal composition ranges (weight %) for TP304 and TP316. Values are representative; refer to the specific product standard or mill certificate for guaranteed limits.

Element TP304 (typical ranges) TP316 (typical ranges)
C ≤ 0.08 (standard) ≤ 0.08 (standard)
Mn ≤ 2.0 ≤ 2.0
Si ≤ 0.75 ≤ 0.75
P ≤ 0.045 ≤ 0.045
S ≤ 0.03 ≤ 0.03
Cr 17.5 – 19.5 16.0 – 18.0
Ni 8.0 – 10.5 10.0 – 14.0
Mo 0 – trace 2.0 – 3.0
V typically ≤ 0.05 typically ≤ 0.05
Nb (Cb) typically ≤ 0.1 (not present in unstabilized grades) ≤ 0.1 (unless stabilized grade)
Ti typically ≤ 0.7 (only in stabilized variants) ≤ 0.7 (only in stabilized variants)
B trace trace
N trace to 0.11 (depends on specification) trace to 0.11 (depends on spec)

Notes: - TP316’s deliberate addition of molybdenum (Mo) and often slightly higher nickel content is the key alloying difference that targets improved localized corrosion resistance (pitting and crevice corrosion) and sustained performance in chloride-bearing environments. - Carbon content influences sensitization during welding; low-carbon variants (304L, 316L) and stabilized grades (with Ti or Nb) mitigate intergranular corrosion after high-temperature exposure. - Small amounts of nitrogen (where present) raise strength and improve pitting resistance.

How alloying affects performance: - Chromium (Cr): forms the passive chromium oxide film that gives stainless steels their basic corrosion resistance. - Nickel (Ni): stabilizes the austenitic structure, increases toughness and ductility, and improves general corrosion resistance. - Molybdenum (Mo): increases resistance to pitting and crevice corrosion, especially in chloride-containing media. - Carbon, Ti, Nb: affect carbide precipitation behavior and resistance to intergranular attack after welding.

3. Microstructure and Heat Treatment Response

  • Microstructure: Both TP304 and TP316 are fully austenitic (face-centered cubic) in the annealed condition. There is no martensitic phase when properly solution annealed.
  • Typical processing routes: hot rolling followed by solution anneal and rapid quench to restore corrosion resistance and ductility.
  • Response to thermal cycles:
  • Solution annealing (typically 1,020–1,100 °C depending on spec) dissolves chromium carbides and returns a homogeneous austenitic matrix.
  • Slow cooling through approximately 450–850 °C can cause chromium carbide precipitation at grain boundaries (sensitization) in higher-carbon variants; this reduces intergranular corrosion resistance.
  • Low-carbon (L) and stabilized (Ti or Nb) variants control carbide precipitation; 316L is commonly specified where welding will be extensive and sensitization is a concern.
  • Hardenability: Austenitic stainless steels are not hardened by quenching; they are strengthened primarily by cold work or by alloy additions (e.g., N). Thermo-mechanical treatments do not produce significant martensite without deformation-induced transformation.

4. Mechanical Properties

Table: Typical mechanical property ranges for annealed material (representative; consult product spec for guaranteed minimums). Units: MPa and %.

Property TP304 (annealed typical) TP316 (annealed typical)
Tensile strength (UTS) ~500 – 700 MPa ~500 – 700 MPa
Yield strength (0.2% offset) ~200 – 350 MPa ~200 – 350 MPa
Elongation (A%) ≥ 40% (commonly 40–60%) ≥ 40% (commonly 40–60%)
Impact toughness (Charpy, room T) High, notch-sensitive data often not specified High, similar to TP304
Hardness (annealed) Typically 70–95 HRB (approx.) Typically 70–95 HRB (approx.)

Interpretation: - In the annealed condition, TP304 and TP316 show very similar mechanical properties. Differences in alloying (Mo, slightly higher Ni in 316) have only modest effects on tensile and yield values; nitrogen content and cold work have larger effects on strength. - Both grades retain excellent toughness down to low temperatures because of the stable austenitic microstructure. - If higher strength is needed, cold work or nitrogen-bearing variants can be selected; for cryogenic service, austenitics are often favorable because of retained toughness.

5. Weldability

  • General weldability: Both TP304 and TP316 weld readily by common fusion and resistance methods (TIG, MIG, SMAW). The austenitic structure avoids hard, brittle martensite formation typical of carbon steels.
  • Carbon and sensitization: Carbon promotes chromium carbide precipitation after exposure to sensitizing temperatures; to reduce risk use low-carbon variants (304L/316L) or stabilized grades.
  • Weldability indices: Useful for qualitative interpretation of weld cracking risk and preheating needs:
  • Example carbon equivalent (IIW): $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$
  • Example $P_{cm}$ for weldability: $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$
  • Qualitative interpretation:
  • Both grades give low hardenability values relative to ferritic steels; preheating is generally unnecessary and can increase the risk of sensitization.
  • TP316 may be marginally easier to avoid hot cracking because higher Ni promotes ductility in the weld metal; however, filler selection and control of weld thermal cycles are more important than the base grade.
  • Use matching or overmatching filler (e.g., ER316/316L) where service demands pitting resistance or where base metal is TP316.

6. Corrosion and Surface Protection

  • Stainless behavior: Both grades rely on a chromium-rich passive oxide film. For general aqueous environments, both perform well.
  • Pitting and crevice corrosion:
  • Use the Pitting Resistance Equivalent Number (PREN) to compare localized corrosion resistance: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • Because TP316 contains molybdenum (and often similar or higher Ni), its PREN is meaningfully higher than TP304’s, improving resistance to chloride-induced pitting and crevice corrosion.
  • When indices are not applicable:
  • PREN and similar metrics are not applicable to general uniform corrosion situations (where Cr and passive film stability dominate), nor are they a substitute for laboratory testing in a given application.
  • Surface protection for non-stainless steels: Not applicable here, but for non-stainless alternatives, galvanizing, painting, and polymer linings would be considered.

7. Fabrication, Machinability, and Formability

  • Machinability:
  • Austenitic stainless steels are work-hardening and can be “gummy”; both grades are more difficult to machine than mild steel.
  • TP316 is typically slightly more challenging to machine than TP304 because of the higher nickel and molybdenum content which increase toughness and work-hardening tendency.
  • Formability:
  • Both grades have excellent formability in the annealed condition; 304 is often marginally easier to form.
  • Springback and strain hardening must be accounted for; tooling and lubrication selection are important.
  • Surface finishing:
  • Both respond to polishing, electropolishing, and passivation. TP316’s improved resistance to pitting makes it preferable when the finished surface must resist chloride attack.
  • Recommendations:
  • For heavy gauge forming or tight-radius bending, consider annealing after forming or select a grade with slightly lower work-hardening tendency to reduce the risk of cracking.

8. Typical Applications

TP304 (common uses) TP316 (common uses)
Food processing equipment, countertops, kitchenware Marine hardware, seawater piping, offshore components
Architectural trim, interior building finishes Chemical process equipment with chloride exposure
General-purpose tubing and heat exchangers in non-chloride environments Medical implants (specific variants), pharmaceutical equipment requiring higher resistance to localized attack
HVAC components, domestic water systems (where chlorides are low) Heat exchangers and condensers exposed to brackish water or chloride-laden environments

Selection rationale: - Choose TP304 where general corrosion resistance, formability, and cost are primary drivers and chloride exposure is low or controlled. - Choose TP316 where service involves chlorides, sulfides, or more aggressive aqueous chemistries, and where localized corrosion would be life-limiting.

9. Cost and Availability

  • Relative cost: TP316 is typically more expensive than TP304 due to the added molybdenum and often higher nickel content. Price differences vary with commodity metal markets (Ni and Mo prices fluctuate).
  • Availability by product form:
  • TP304 is generally more widely available in a broad range of forms and surface finishes.
  • TP316 is widely available as well but certain sizes, surface finishes, or specialty mill products (e.g., 316L, 316Ti) may have longer lead times and higher premium.
  • Procurement note: For large projects, locking in long-lead material and specifying acceptable substitutes (e.g., 316L vs 316) helps manage cost volatility.

10. Summary and Recommendation

Table: Summary comparison (qualitative)

Attribute TP304 TP316
Weldability Excellent (use 304L for heavy welding) Excellent (use 316L for heavy welding)
Strength – Toughness Good, similar to TP316 in annealed condition Good, similar to TP304; slightly higher toughness retention in some chemistries
Corrosion resistance (general) Very good Very good
Localized corrosion (pitting/crevice) Moderate in chloride environments Superior (due to Mo and Ni)
Machinability Good for austenitic SS (work-hardening) Slightly less favorable than TP304
Cost Lower (more economical) Higher (premium due to Mo/Ni)

Conclusions — choose based on environment and life-cycle needs: - Choose TP304 if: cost sensitivity is high, the environment is non-chloride or only mildly corrosive, and the application values formability and broad availability (e.g., foodservice equipment, architectural elements, general process piping not exposed to chlorides). - Choose TP316 if: the service environment contains chlorides or other agents that promote pitting/crevice corrosion, long-term resistance to localized attack is required, or the application is marine, offshore, or chemical processing where molybdenum-enhanced resistance justifies the premium.

Final practical guidance: - For welded assemblies in chloride service specify low-carbon variants (304L / 316L) or stabilized grades to avoid sensitization. - When in doubt about chloride exposure or where maintenance is difficult, err toward TP316 despite the higher upfront cost — life-cycle savings often justify the choice. - Always confirm material selection against the exact process fluid, temperature, and mechanical loading conditions; when corrosion risk is critical, perform application-specific corrosion testing or consult corrosion specialists.

Back to blog