SPCC vs SPCD – Composition, Heat Treatment, Properties, and Applications
Share
Table Of Content
Table Of Content
Introduction
SPCC and SPCD are two widely used JIS cold-rolled carbon steel grades specified for sheet and strip products. Engineers, procurement managers, and manufacturing planners frequently face a selection dilemma between these grades when designing for stamping, deep drawing, and other sheet-metal operations: should the design favor slightly higher strength and general utility (cost and availability), or prioritize superior formability for tight-draw parts? The comparison hinges on production intent—SPCC is a general-purpose cold-rolled commercial steel, while SPCD is formulated with an emphasis on improved formability for drawing operations. This functional distinction is why the two are commonly compared in tooling, stamping, and automotive body-panel decisions.
1. Standards and Designations
- JIS: SPCC and SPCD are JIS-designated cold-reduced carbon steel grades (commonly referenced in JIS G3141 for cold-reduced sheets and strips).
- EN: Equivalent product families are covered by EN 10130 (cold-rolled non-alloy steel), with specific DC grades (DC01–DC05) mapping to various JIS grades by application rather than exact chemistry.
- ASTM/ASME: Comparable families include ASTM A1008 / A366 (cold-rolled mild steels) used for similar cold-forming tasks.
- GB (China): GB/T standards include cold-rolled non-alloy steels with designations analogous in application but not identical in naming.
- Classification: Both SPCC and SPCD are low-carbon, non-alloy (carbon) steels intended for cold forming. They are not alloy, stainless, tool, or HSLA steels.
2. Chemical Composition and Alloying Strategy
Both SPCC and SPCD are intentionally low-alloy, low-carbon steels. SPCD is produced with a chemistry and mill process tuned to boost drawability (lower effective carbon and tighter control of impurities/soluble elements), while SPCC provides balanced properties for general stamping.
Table: qualitative comparison of element presence and role
| Element | SPCC (general cold-rolled) | SPCD (improved drawability) |
|---|---|---|
| C (Carbon) | Low (commercial grade) — slightly higher than SPCD | Very low to low — optimized for formability |
| Mn (Manganese) | Low to moderate — deoxidation and strength control | Low — controlled to reduce strength and increase ductility |
| Si (Silicon) | Trace to low — deoxidizer | Trace — typically similar to SPCC |
| P (Phosphorus) | Controlled impurity (kept low) | Tightly controlled and often lower than SPCC |
| S (Sulfur) | Controlled impurity (may be present) | Controlled and minimized for forming quality |
| Cr, Ni, Mo, V, Nb, Ti, B | Generally not added (trace only) | Generally not added (trace only) |
| N (Nitrogen) | Low, controlled in melt | Low, controlled; sometimes lower for better surface and ductility |
How alloying affects properties - Carbon and manganese primarily influence strength and hardenability. Lower carbon improves ductility and formability but reduces as-rolled strength. - Silicon and manganese act as deoxidizers; their levels affect surface quality and mechanical balance. - Sulfur and phosphorus are impurities that embrittle or reduce ductility when elevated; SPCD typically has tighter control for deep drawing. - Microalloying is not a typical strategy for these grades; both rely on cold work, annealing, and process control rather than alloy additions to reach target properties.
3. Microstructure and Heat Treatment Response
Microstructure under standard processing: - Both grades in the annealed/soft-rolled condition are dominated by ferrite with limited pearlite islands (low-carbon ferrite-pearlite structure). SPCD often has an even lower pearlite fraction because of its reduced carbon and controlled cooling, delivering a more uniform, fine-grained ferritic matrix that favors ductility. - Cold-rolling introduces strain and dislocation density which is then relieved and recrystallized by annealing. Anneal schedules (temperature and hold time) are chosen to balance grain size, yield strength, and surface quality.
Heat treatment response: - These are not heat-treatable in the sense of quench-and-temper steels; they do not respond to hardening by martensitic transformation because of low carbon and lack of alloying elements that raise hardenability. - Typical tailored processing routes for improved properties are: - Recrystallization anneal (to restore ductility after cold work). - Continuous annealing or batch annealing to produce different surface scales and mechanical balances. - For special deep-drawing product forms, tight process control (cold rolling reduction, precise anneal, and skin-pass finishing) yields the target microstructure and mechanical balance. - Thermo-mechanical processing is limited because alloy content is low; mechanical property differences are achieved mainly by cold work and anneal conditions.
4. Mechanical Properties
Table: comparative mechanical-property descriptors
| Property | SPCC | SPCD | Notes |
|---|---|---|---|
| Tensile strength | Moderate — suitable for general stampings | Slightly lower or similar — optimized toward higher elongation | Final values depend on temper, thickness, and anneal |
| Yield strength | Moderate | Slightly lower | SPCD aims for lower yield to reduce springback and enable deep drawing |
| Elongation (ductility) | Good | Higher | SPCD prioritized for superior elongation and uniformity |
| Impact toughness | Adequate for sheet applications | Similar — generally comparable | Not a primary differentiator at ambient temperatures |
| Hardness | Moderate | Slightly lower | Reflects the lower carbon and reduced cold work requirement in SPCD |
Explanation - SPCD typically yields better formability (higher total and uniform elongation) at the cost of slightly reduced yield/tensile strength compared to SPCC. For stamped components needing tight radii and high draw depth, SPCD provides fewer tears and lower earing. - Both grades’ mechanical properties vary by coil temper (fully annealed vs. skin-passed), thickness, and supplier-specific processing.
5. Weldability
Both SPCC and SPCD offer good weldability relative to higher-carbon steels because of their low carbon equivalent and minimal alloy content. Weldability considerations: - Carbon content and residue alloying determine susceptibility to HAZ hardening and cold-cracking; both grades are low-carbon, reducing these risks. - Hardening/hardenability contributions from Mn and other elements are low in these grades.
Useful weldability indices (qualitative interpretation only): - Carbon equivalent (IIW): $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ Lower $CE_{IIW}$ implies simpler preheat/post-heat and lower cracking risk. Both SPCC and SPCD are expected to have low values. - Pcm index: $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$ Lower $P_{cm}$ indicates easier weldability and lower need for special weld procedures. Again, both grades should score well.
Practical guidance: - Preheat is rarely required for sheet-gauge material of either grade for typical short welds; thicker sections or high restraint assemblies may still require weld procedure qualification. - Residual stress and distortion management are typical concerns—use appropriate fixturing and spot-weld sequencing in assembly work.
6. Corrosion and Surface Protection
- Neither SPCC nor SPCD is stainless; corrosion resistance is typical of unalloyed carbon steel and requires protective coatings for long-term performance.
- Common protection strategies: hot-dip galvanizing, electro-galvanizing, phosphating followed by paint, coil coating, or mechanical plating.
- When stainless or corrosion resistance metrics such as PREN matter, those indices do not apply to these carbon steels. For reference, PREN is: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$ This is relevant only for stainless alloys, not SPCC/SPCD. Choose galvanizing or organic coatings to achieve environmental durability.
7. Fabrication, Machinability, and Formability
- Cutting: both cut well with standard shearing and laser processes; SPCD’s lower yield strength can reduce burr size for certain thicknesses.
- Bending/forming: SPCD outperforms SPCC in deep drawing and severe forming because of higher ductility and better control of forming defects (wrinkling, necking). SPCC is acceptable for general stamping, mild draws, and hemming.
- Machinability: as low-carbon steels, both machine similarly; cold-rolled surface finish can affect tooling wear and chatter—select tooling and cutting parameters accordingly.
- Surface finish and coating adherence: SPCD and SPCC are both available in bright anneal and oiled finishes; cleaner surfaces and consistent oxide scales on SPCD can improve paint and coating adhesion in automotive use.
8. Typical Applications
| SPCC (typical uses) | SPCD (typical uses) |
|---|---|
| General automotive body panels, panels with moderate drawing | Deep-drawn automotive inner panels, fuel tanks, appliance shells with severe draws |
| Light structural panels, furniture components | Complex drawn parts requiring high uniform elongation and minimal tearing |
| Trim, brackets, general stamping | High-draw kitchenware or containers, deep housings |
Selection rationale: - Choose SPCC when the part requires balanced strength, economy, and general stampability without extreme drawing requirements. - Choose SPCD when the part has deep draws, tight radii, or complex shapes where maximum ductility and uniform deformation are essential.
9. Cost and Availability
- Both grades are common stock items in coil, sheet, and slitted forms. SPCC tends to be more widely stocked as a general-purpose cold-rolled grade and can be marginally less expensive due to broader demand and simpler inventory flows.
- SPCD may carry a small premium for specific deep-drawing coils or tighter process control products. Availability is generally good in regions with automotive and appliance supply chains; lead times vary by mill and coating options.
10. Summary and Recommendation
Summary table
| Attribute | SPCC | SPCD |
|---|---|---|
| Weldability | Excellent (low CE) | Excellent (low CE) |
| Strength–Toughness balance | Moderate strength / good toughness | Slightly lower strength / higher ductility |
| Cost | Generally lower / widely available | Slight premium for deep-drawing control |
Recommendations - Choose SPCC if you require a cost-effective, general-purpose cold-rolled sheet for moderate forming, stamping, and welded assemblies where slightly higher strength and wide availability are priorities. - Choose SPCD if your part requires superior deep-drawing performance, higher uniform elongation, and the lowest risk of drawing defects (tears, necking) — typical for deep-drawn automotive or appliance components.
Final note: exact grade selection should be validated with supplier data sheets and prototype trials. Mechanical properties, surface finish, and coatability depend on mill practice, anneal cycles, and specific temper designations; always specify required temper/anneal and surface treatment in procurements to ensure repeatable production outcomes.