HFW vs SAWL – Composition, Heat Treatment, Properties, and Applications
Share
Table Of Content
Table Of Content
Introduction
High-frequency welded (HFW, often grouped with ERW-type processes) and submerged-arc welded longitudinal (SAWL) steel pipes are two common product families in the tube-and-pipe market. Engineers and procurement teams typically weigh trade-offs among manufacturability, in-service strength and toughness, weldability, corrosion resistance, and cost when selecting between them. Typical decision contexts include choosing between thinner-walled, cost‑efficient piping for distribution and structural use versus thicker-walled, higher‑integrity piping for transmission, high-pressure service, or more demanding mechanical requirements.
The principal operational distinction between these two families lies in their welding and manufacturing approach, which influences the wall-thickness range they serve and the alloying/processing strategies used to meet mechanical and toughness targets. Because manufacturing method drives thermal cycles, available wall thicknesses, and allowable alloy content, HFW and SAWL are commonly compared in pipeline, structural, and pressure-system design work.
1. Standards and Designations
Both HFW and SAWL pipes are produced to multiple international standards; the actual material grade is often specified separately from the joining process. Common standards include:
- ASTM / ASME: ASTM A53, ASTM A500, ASTM A106 (seamless reference), ASME B36.10/B36.19 (dimensions), API 5L (linepipe specification covering both welded and seamless).
- EN: EN 10217 (welded steel tubes for pressure purposes), EN 10219 (cold formed welded structural hollow sections), EN 10204 (inspection documents).
- JIS: JIS G3454, G3452 (welded steel pipes for water and gas).
- GB (China): GB/T 3091 (seamless/welded steel tubes for low-pressure fluid transportation), GB/T 9711 (line pipes).
Classification by metallurgical family: - HFW products: typically carbon or low-alloy steels (mild steel, low-carbon weldable steels), sometimes microalloyed for strength. - SAWL products: typically carbon and microalloyed linepipe steels and low-alloy steels; often used with higher strength grades and thicker walls. - Neither is an inherently stainless or tool steel product; stainless variants exist using SAW but are less common for standard HFW/SAWL commercial offerings.
2. Chemical Composition and Alloying Strategy
Table: Typical compositional tendencies (qualitative) for HFW vs SAWL
| Element | HFW (typical) | SAWL (typical) |
|---|---|---|
| C | Low to moderate (emphasize weldability) | Low to moderate; microalloy variants may have similar C with enhanced strength |
| Mn | Moderate (deoxidation and strength) | Moderate to higher (improves hardenability and strength) |
| Si | Low (descaling/deoxidation) | Low to moderate (deoxidation; can be slightly higher in SAW consumables) |
| P | Controlled low | Controlled low |
| S | Controlled low | Controlled low |
| Cr | Typically low (not stainless) | May be present in small amounts in some alloys |
| Ni | Typically low | Low; may be present in selected linepipe alloys |
| Mo | Typically none or trace | May be present in microalloy/linepipe grades for strength/toughness |
| V | Usually low/trace | Often used as microalloying element for strength/toughness |
| Nb (Nb/Ta) | Rare in commodity HFW tubes | Common in microalloyed SAWL linepipe steels (improves strength/toughness) |
| Ti | Trace (deoxidation/stabilization) | Possible trace for stabilization |
| B | Trace if used (hardenability control) | Trace in some linepipe steels |
| N | Controlled low | Controlled low; relevant for precipitation and toughness control |
Explanation: - HFW products are often optimized for thin-wall manufacture and high-throughput coil-to-pipe welding; compositions emphasize low carbon and controlled alloying to maximize weldability and ductility. - SAWL pipes, especially when targeted for higher-strength linepipe grades, frequently use microalloying (Nb, V, Ti) and controlled Mn/trace Mo to raise strength via precipitate strengthening and controlled rolling/thermal cycles while maintaining toughness.
3. Microstructure and Heat Treatment Response
Typical microstructures and processing behavior differ because the welding method and production equipment impose different thermal cycles and allow different processing routes.
- HFW: Produced from coil strip with rapid high-frequency welding. Typical base metal microstructure is ferrite–pearlite or fine-grained ferrite with dispersed bainite for microalloyed variants. Limited in-line heat treatment capability on thin-walled HFW lines; manufacturers often use controlled annealing or temper rolling rather than extensive quench-temper cycles.
- SAWL: Produced from plate or wider strip using submerged-arc welding in one or more passes. SAW processes allow thicker wall builds and can accommodate preheat/postheat and controlled PWHT (post-weld heat treatment) more readily. Microstructure of SAWL base metal can be fine ferrite–pearlite, bainite, or mixed microstructures depending on plate chemistry and thermo‑mechanical rolling; microalloyed plates respond well to controlled rolling to produce fine-grained tough microstructures.
Heat-treatment responses: - Normalizing/refining cycles improve grain size and toughness in both; SAWL production lines and finishing mills more commonly implement normalizing or controlled cooling on thicker plates. - Quench and temper is typically applied to plate before SAWL in high-strength linepipe grades but is not common for standard HFW thin-wall product. - Thermo-mechanical controlled processing (TMCP) is used for SAWL and high-quality HFW material when specifications require higher yield strength with retained toughness.
4. Mechanical Properties
Table: Qualitative comparison of mechanical properties
| Property | HFW (typical thin-wall products) | SAWL (thicker, linepipe-type products) |
|---|---|---|
| Tensile Strength | Moderate | Moderate to high (microalloyed/strengthened plates allow higher values) |
| Yield Strength | Moderate | Moderate to high (controlled rolling or microalloying raises yield) |
| Elongation | Generally good (ductile thin-wall) | Good, but depends on grade and thickness; higher-strength variants may have lower elongation |
| Impact Toughness | Good at ambient for typical grades; lower for cold-service unless specified | Often engineered for superior toughness (especially for low-temperature or high-pressure service) |
| Hardness | Low to moderate (easier machining/forming) | Can be higher in strengthened grades; harder to machine/form when thicker |
Interpretation: - SAWL products can achieve higher strength–toughness balances because plate production allows more aggressive alloying and thermal control. HFW excels in ductility and consistent thin-wall geometry but is generally constrained in achieving very high-strength grades without affecting weldability.
5. Weldability
Weldability is a central differentiator because HFW and SAWL are themselves welded products; understanding their susceptibility to hydrogen cracking, hardening, and thermal cycle sensitivity is crucial.
Key factors: carbon equivalent and parent-metal hardenability; microalloying affects susceptibility to HAZ hardening.
Useful indexes: - Carbon equivalent (IIW): $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ - Pcm (for evaluation of cold cracking susceptibility): $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$
Qualitative interpretation: - HFW: Because production targets thin walls and high-volume welding, base steels are chosen with lower $CE_{IIW}$ and $P_{cm}$ to ensure easy welding and low susceptibility to HAZ hardening. HFW seams are formed by high-frequency induction heating and pressure, so they are tolerant of low-carbon chemistries. - SAWL: SAW welding uses a melting arc and multiple weld passes; higher alloy content in plate can increase hardenability, raising carbon-equivalent indices. However, SAWL production can apply preheat, interpass control, and PWHT where required to manage hydrogen cracking risk and HAZ toughness. SAWL consumables (wires and flux) can be selected to match chemistry and dilution to control weld metal properties.
Practically: - For field welding and tie‑ins, HFW pipe (thin-wall) is easier to weld using common procedures. SAWL pipe often requires more attention to preheat/interpass temperatures for high-strength grades or thick walls and may have more stringent welding procedure qualification requirements.
6. Corrosion and Surface Protection
- Non-stainless steels (both HFW and SAWL) rely on coatings and cathodic protection for corrosion control: hot-dip galvanizing, fusion-bonded epoxy (FBE) coatings, three-layer polyethylene coatings, oil coatings, painting systems, and internal linings for fluid service.
- SAWL linepipe used for buried or subsea services will commonly receive multi-layer external coatings plus internal corrosion mitigation measures.
- Where stainless alloys are used with SAW processes (less common for commodity HFW/SAWL), apply PREN for localized corrosion resistance: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
- PREN is not applicable to carbon steel grades; use it only for duplex/austenitic stainless steels.
Practical note: Selection of coating and internal protection is driven more by service environment and risk analysis than by the welding method itself.
7. Fabrication, Machinability, and Formability
- HFW (thin-wall): Easier bending, forming, and cold expansion. Better machinability and punching characteristics due to lower hardness, but thin wall limits certain mechanical operations. Suitable for tight-radius bending and fittings common in distribution networks.
- SAWL (thicker wall): Heavier, less forgiving for tight forming; requires larger tooling and may require heat-assisted forming for thick plates. Machining of thicker, microalloyed steels can be more demanding; careful control of cut speeds and tooling is needed.
Welding and repair: - HFW field welds are straightforward for butt welding, but thin walls require controlling burn-through and fit-up. - SAWL thicker walls may require multi-pass welding and qualified WPS, but thicker wall also affords more margin for heat input and mechanical repair.
8. Typical Applications
| HFW (common uses) | SAWL (common uses) |
|---|---|
| Small- to medium-diameter thin-wall piping for water, gas distribution, HVAC, structural tubes, and general mechanical tubing | Large-diameter transmission pipelines, high-pressure linepipe, offshore pipelines, process piping with thicker walls, and sections requiring higher strength/toughness |
| Low-pressure conduit, scaffolding, furniture, and automotive tubular components | Long-distance hydrocarbon transport, trunklines, subsea risers (with appropriate coatings), and onshore high-pressure pipelines |
Selection rationale: - Choose HFW when economy, thin-wall geometry, and ease of forming are priorities and service pressures/loads are moderate. - Choose SAWL when wall thickness, higher design pressures, and enhanced strength/toughness or rigorous welding controls are required.
9. Cost and Availability
- Cost: HFW products are typically lower cost per unit length for small-to-medium diameters because of high-volume coil processing and simpler welding. SAWL pipes are costlier for equivalent diameters at higher wall thickness due to plate production, welding passes, and greater material usage.
- Availability: HFW is widely available in commodity sizes and quick lead times. SAWL availability depends on plate mill capacity and welding line capabilities; long-lead items are common for specialized linepipe or high‑specification grades.
- Product form: HFW often supplied from coil-to-tube mills; SAWL supplied from plate-to-pipe lines or wide-strip mills with associated heat-treatment options.
10. Summary and Recommendation
Table: Summary comparison
| Characteristic | HFW | SAWL |
|---|---|---|
| Weldability | Excellent for thin-wall, lower CE | Good but requires preheat/interpass control for thicker/high-strength grades |
| Strength–Toughness balance | Moderate strength, high ductility | Broader range; can achieve higher strength with engineered toughness |
| Cost | Lower for thin-wall applications | Higher for thicker, high-specification linepipe |
Recommendation: - Choose HFW if you need economical, thin-walled tubing for distribution, structural, or low-to-moderate pressure service where high weldability and good formability are primary requirements. - Choose SAWL if you require thicker walls, higher yield/tensile capacity, improved HAZ and notch toughness for transmission or high-pressure service, or when the project demands plate-derived mechanical properties and controlled thermal processing.
Concluding note: Selection should be driven by the combination of design pressure, wall-thickness requirement, weld- and field‑joining strategy, toughness at operating temperature, and lifecycle protection needs. Specify chemistry limits, heat-treatment/finish requirements, and welding procedure qualifications up front to ensure the chosen manufactured product (HFW or SAWL) meets the project’s metallurgical and mechanical performance targets.