ASP23 vs M2 – Composition, Heat Treatment, Properties, and Applications
Share
Table Of Content
Table Of Content
Introduction
Engineers and procurement professionals frequently must choose between conventional wrought or cast high-speed steels and powder-metallurgy (PM) variants when specifying tooling and wear components. The decision hinges on trade-offs such as raw material cost versus in-service life, ease of fabrication versus required performance, and resistance to fracture versus hardness retention at temperature. Typical contexts include cutting-tool selection, cold-forming dies, and wear-resistant inserts — where lifetime, reparability, and manufacturing cost all matter.
At a high level, the principal distinction is that one grade is a PM-processed high-speed steel designed for a cleaner, more uniform carbide distribution and improved toughness, while the other is the conventional wrought/cast high-speed steel widely used as a baseline. Because both target high hardness and hot hardness, they are often compared for tooling and wear applications where small microstructural differences produce large life-cycle impacts.
1. Standards and Designations
- M2
- Standards: AISI/SAE M2; EN designation commonly HSS M2 (EN ISO 4957), JIS SKH51 (approx. equivalent), GB T 12902 series equivalents.
-
Classification: High-speed tool steel (traditional, wrought/cast HSS).
-
ASP23
- Standards: ASP is a trade designation used by powder-steel manufacturers (e.g., Hitachi, Sumitomo, etc.). ASP23 is a powder metallurgy high-speed steel family; it may be listed in supplier datasheets rather than international standards by chemical name.
- Classification: Powder-metallurgy high-speed steel (PM-HSS), i.e., a PM variant within the high-speed/tool steel family.
Note: Both are tool steels / high-speed steels; neither is stainless or HSLA. ASP23 is a PM form of a high-speed steel chemistry comparable to M2 but produced to tighter cleanliness and microstructural control.
2. Chemical Composition and Alloying Strategy
Table: (for ASP23 the chemistry is nominally similar to M2; manufacturers control impurities and may add microalloying—see notes)
| Element | M2 (typical standard ranges) | ASP23 (PM HSS — nominal description) |
|---|---|---|
| C | 0.85–1.05% | Similar nominal carbon content (≈0.8–1.0%); PM control of C and dissolved carbon |
| Mn | 0.15–0.40% | Similar; kept low to control segregation |
| Si | 0.15–0.45% | Similar; controlled for deoxidation and strength |
| P | ≤0.03% | Tighter limits (lower P) to reduce embrittlement |
| S | ≤0.03% | Significantly lower S in PM grade to improve toughness |
| Cr | 3.75–4.5% | Similar Cr level for matrix strength/hardness |
| Ni | ≤0.25% | Typically negligible; controlled impurities |
| Mo | 4.5–5.5% | Similar Mo for secondary hardenability |
| V | 1.75–2.2% | Similar V; PM processing refines V-rich carbides |
| Nb | — / trace | May include trace Nb/Ti additions (ppm to small %) to stabilize carbides in PM processing |
| Ti | — / trace | As above; small additions possible |
| B | — / trace | Not typically a primary alloying element; sometimes present in trace amounts |
| N | Trace | Controlled and minimized in PM product to avoid nitride-induced embrittlement |
Note: Tungsten (W) is a major alloying element in both M2 and its PM equivalents (typically several percent). The table omits W per the requested column list, but W is critically important: standard M2 contains approximately 5–7% W as a primary hardening element. ASP23 retains tungsten as in the parent chemistry. Exact compositions for ASP23 are proprietary to the supplier, but the strategy is to match M2’s principal alloying for hot hardness while improving cleanliness and carbide size distribution.
How alloying affects properties - Carbon + W/Mo/Cr/V form a mixture of MC, M6C, and complex carbides that deliver hardness and wear resistance. - Chromium contributes to hardenability and temper resistance; molybdenum and tungsten increase hot hardness. - Vanadium forms hard vanadium carbides (MC) that resist abrasion; their distribution and size strongly influence toughness and grindability. - Lower impurities (S, P) and controlled microalloying (Nb, Ti) in PM steels limit brittle films and provide a more uniform microstructure, improving toughness without sacrificing hardness.
3. Microstructure and Heat Treatment Response
Microstructure under standard processing: - M2 (wrought/cast) - Typical microstructure after conventional processing: tempered martensite matrix with a bimodal carbide population — larger alloy carbides (M6C, M2C) and smaller vanadium-rich MC carbides. Carbides are coarser and may be segregated depending on solidification and forging. - ASP23 (PM) - PM processing produces a homogeneous, fine, and uniformly distributed carbide network with reduced segregation and fewer non-metallic inclusions. Carbides are finer, leading to better toughness and resistance to chipping.
Heat treatment behavior: - Normalizing: Used to refine cast/wrought structures; more effective on conventional M2 to break up segregation but cannot fully match PM homogeneity. - A typical hardening sequence for both: austenitize at elevated temperature (low-cycle austenitization appropriate to grade), oil or air quench (sometimes high-pressure gas for PM grades), followed by multiple tempering cycles to reach desired hardness and toughness balance. - Quenching & tempering response: - M2: Good hardenability; careful control of austenitizing temperature and tempering is required to balance retained austenite, hardness, and toughness. - ASP23: Because of reduced segregation and finer carbides, ASP23 typically gives improved toughness at equivalent hardness and may show more uniform response during tempering with less risk of soft spots. - Thermo-mechanical processing is less relevant to PM products (sintering/forging are used pre-finishing), while wrought M2 benefits from controlled forging and heat-treatment schedules to reduce coarse carbide clusters.
4. Mechanical Properties
Values for tool steels vary widely with heat treatment; the table below provides a comparative, application-oriented view rather than a single guaranteed specification.
| Property | M2 (conventional HSS) | ASP23 (PM HSS) |
|---|---|---|
| Tensile Strength | High (typical high-speed steel range) | Comparable to slightly higher due to uniform microstructure |
| Yield Strength | High | Comparable or slightly improved |
| Elongation | Low-to-moderate (tool steels: small %) | Similar or modestly improved (better toughness enables use in more demanding geometries) |
| Impact Toughness | Moderate to low (sensitive to carbide coarseness and inclusions) | Higher than M2 at equivalent hardness due to finer carbides and fewer inclusions |
| Hardness (HRC) | Typically up to ~62–66 HRC after hardening/tempering depending on temper cycles | Similar maximum hardness achievable; retains hardness more uniformly and often shows better toughness at a given HRC |
Interpretation - Strength and hardness capability are comparable because both share the same alloying basis; however, ASP23’s PM microstructure typically yields higher fracture toughness and improved resistance to catastrophic chipping. - Elongation in tool steels is inherently limited; PM-grade improvements are incremental but meaningful for tooling that sees shock loads or cyclic stresses.
5. Weldability
Weldability of high-speed steels is generally limited due to high hardenability and carbide-forming alloy content. Important considerations: - Carbon content and alloying raise hardenability and predispose the heat-affected zone (HAZ) to hard, brittle martensite. - Microalloying and low impurities in PM steels reduce segregation but do not eliminate weld-induced cracking risk.
Useful indices (qualitative interpretation): - Carbon equivalent (IIW): $$ CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15} $$ Higher $CE_{IIW}$ implies greater propensity for HAZ hardness and cracking — underscores need for preheat/interpass control. - Pcm: $$ P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000} $$ Higher $P_{cm}$ indicates increased cracking risk and need for special welding procedures.
Qualitative guidance: - Both M2 and ASP23 require preheating, controlled interpass temperatures, and post-weld heat treatment if welding is unavoidable. - ASP23’s lower impurity content helps reduce weld cracking tendencies marginally, but its high alloy content means welding is still challenging and typically avoided for critical tooling — brazing, soldering, or mechanical joining is often preferred. - For repair welding, choose filler metals designed for high-speed steels and plan stress-relief tempering.
6. Corrosion and Surface Protection
- Neither M2 nor ASP23 is stainless; corrosion resistance is modest and primarily governed by chromium content (~4% level), which is insufficient for true corrosion environments.
- Typical protection methods:
- Surface coatings (PVD/CVD, TiN, AlTiN) for cutting tools to reduce wear and corrosion in service.
- Barrier coatings (nickel, chrome plating), painting, or galvanizing for non-tooling components where feasible.
- Local carburizing/nitriding is generally not typical because high alloy content and carbides limit diffusion effectiveness.
- PREN is not applicable to these non-stainless alloys. For stainless grades you would use: $$ \text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N} $$ — but this index does not apply to M2/ASP23.
7. Fabrication, Machinability, and Formability
- Cutting and grinding:
- ASP23 (PM) typically shows improved grindability and more uniform tool wear because carbide sizes are smaller and more evenly distributed.
- M2 may have coarser carbides that can produce higher abrasive wear on grinding wheels and less predictable tool life.
- Machinability (pre-hardening)
- Both grades are easier to machine in annealed or “soft” condition; PM steels can be slightly more difficult to machine because of the homogenous hard particulate distribution if not fully annealed.
- Formability and bending
- Both have poor ductility compared with structural steels; forming is limited and must be done in annealed condition with adequate springback allowances.
- Finishing
- ASP23’s finer carbide structure often leads to superior surface finish after grinding/polishing for cutting tools.
8. Typical Applications
| ASP23 (PM HSS) | M2 (Conventional HSS) |
|---|---|
| Cutting inserts and high-performance cutting tools where uniform wear and toughness are critical | General-purpose high-speed cutting tools (drills, taps, endmills) with established supply chains |
| Dies and punches for medium-to-high wear, where fatigue resistance is required | Standard tooling in lower-cost applications or where PM advantages are unnecessary |
| Long-life reamers, micro-tools, and precision tools requiring consistent edge stability | Broad range of tools where cost sensitivity outweighs maximum lifetime |
| Specialized wear components where improved fracture toughness extends service life | Repairable tooling and legacy applications with well-understood heat treatment schedules |
Selection rationale: - Choose ASP23 when you need improved fracture toughness, consistent performance across tool lots, longer tool life, and superior resistance to chipping — especially for high-volume or high-risk operations. - Choose M2 when cost, availability, and conventional processing paths are primary constraints and when the known behavior of wrought/cast HSS is acceptable.
9. Cost and Availability
- Cost: PM steels (ASP23) are generally more expensive per kilogram than conventional M2 because powder production, atomization, sintering, and consolidation add process cost. However, lifecycle cost may favor PM due to reduced downtime and longer tool life.
- Availability: M2 is widely available globally in bars, sheets, and finished tool blanks. ASP23 is available from major PM steel suppliers and distributors but may require longer lead times or minimum order quantities for special product forms; it is commonly available in tool blanks, pre-hardened bars, and sintered billets.
10. Summary and Recommendation
Summary table (qualitative)
| Attribute | ASP23 (PM HSS) | M2 (Conventional HSS) |
|---|---|---|
| Weldability | Poor — marginally better than M2 due to cleanliness | Poor — high cracking risk |
| Strength–Toughness balance | Excellent at equivalent hardness (better toughness) | Good strength, lower toughness at same hardness |
| Cost (raw material) | Higher | Lower |
Conclusions and recommendations - Choose ASP23 if: - You require longer tool life, improved fracture toughness, and predictable performance across production lots. - The application is cutting or forming with high shock loads or where reduced downtime justifies higher material cost. - You need superior grindability and more uniform carbide distribution for precision tools.
- Choose M2 if:
- Budget and immediate availability are primary drivers and the application is well-served by conventional HSS.
- The tooling geometry and loading conditions are not prone to chipping or catastrophic fracture and established heat-treatment protocols are followed.
- You require a widely available, well-understood baseline steel for legacy processes.
Final note: Both grades rely on careful heat treatment and process control to realize performance. For mission-critical tooling, confirm supplier datasheets for the exact ASP23 chemistry and request heat-treatment recommendations and empirical performance data (tool life tests) versus M2 in the specific operation before final selection.