AH32 vs DH32 – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

AH32 and DH32 are two common shipbuilding/high-strength low-alloy (HSLA) steel grades used for hull structures, decks, and other load-bearing components in marine and offshore engineering. Engineers, procurement managers, and manufacturing planners frequently weigh trade-offs between strength, low-temperature toughness, weldability, and cost when selecting between them. Typical decision contexts include choosing a plate grade for temperate versus cold-climate service, balancing fabrication ease against required impact performance, and specifying material for welded structures where post-weld toughness is critical.

The principal practical distinction between AH32 and DH32 is their intended service temperature band and the associated toughness requirements: DH32 is specified and processed to deliver higher guaranteed impact toughness at lower service temperatures than AH32. As a result, DH32 often requires tighter control of composition and processing (thermo‑mechanical control processing, TMCP) to ensure reliable low-temperature performance, while AH32 is optimized for moderate-temperature service with generally similar static strength but less stringent low-temperature impact demands.

1. Standards and Designations

  • Major classification and national standards that include AH32 and DH32-style shipbuilding grades:
  • Classification societies: ABS, DNV/GL, Lloyd’s Register (equivalent notations appear across societies).
  • National standards: GB (China), JIS (Japan) and ISO technical documents; many societies provide equivalent grade symbols.
  • Material class: Both AH32 and DH32 are non‑stainless, low‑carbon microalloyed HSLA steels developed for structural applications in ships and offshore platforms. They are not tool steels or stainless grades.

2. Chemical Composition and Alloying Strategy

Element AH32 (typical strategy) DH32 (typical strategy)
C Low carbon for weldability and toughness Low carbon, often similar or slightly lower than AH32 to help low-temperature toughness
Mn Moderate Mn to provide strength and hardenability Moderate Mn, controlled to limit hardenability and reduce cold cracking risk
Si Small amounts as deoxidizer Small amounts as deoxidizer
P Kept low (impurity control) Kept low; strict limits for toughness
S Kept low (impurity control) Kept low; strict limits for toughness
Cr Generally minimal; used only if required Generally minimal; not a primary hardening alloy
Ni Not normally present in significant amounts Minimal or none in typical commercial formulations
Mo Not normally significant Not normally significant
V May be present as a microalloying element for strength May be used as microalloying to refine grain and improve toughness
Nb (Cb) Used as microalloy (grain refinement, precipitation strengthening) Often specified or precisely controlled to optimize low‑temperature toughness with TMCP
Ti Small amounts for deoxidation/precipitation control Small amounts; controlled to avoid adverse effects on toughness
B Typically absent or tightly controlled Typically absent or tightly controlled
N Controlled (low) to avoid nitride-related toughness reductions Controlled (low); quality control critical for higher toughness

Notes: - Both grades are designed as low-C microalloyed steels. The alloying strategy emphasizes controlled impurities (P, S, N) and microalloy additions (Nb, V, Ti) to achieve a fine-grained ferritic microstructure, enabling high strength with good toughness. - DH32 specifications tend to impose tighter controls on impurity levels and sometimes tighter ranges for microalloy additions to guarantee performance at lower temperatures.

3. Microstructure and Heat Treatment Response

  • Typical microstructures:
  • AH32: Fine-grained ferrite and polygonal ferrite with dispersed pearlite or bainitic components depending on TMCP. The microstructure is balanced for strength and ductility at moderate temperatures.
  • DH32: Similar ferritic‑pearlitic or ferritic‑bainitic microstructure, but processed (TMCP) to promote finer grain size and favorable transformation products that enhance low-temperature impact toughness.
  • Heat treatment and processing effects:
  • Normalizing: Increases uniformity and refines grain size relative to as-rolled material; can be applied to both grades but TMCP is more common and cost-effective for plate production.
  • Thermo‑mechanical controlled processing (TMCP): Widely used for both grades in modern plate mills. For DH32, TMCP schedules are often adjusted to achieve a higher fraction of acicular ferrite/bainitic microstructures and finer prior austenite grain size, improving toughness at lower temperatures.
  • Quench & temper: Not typical for large ship plates; if applied, raises strength but can reduce ductility and complicate weld procedures. Both grades are primarily produced via controlled rolling and accelerated cooling rather than full quench and temper cycles.

4. Mechanical Properties

Property AH32 (general expectation) DH32 (general expectation)
Tensile strength Comparable high strength typical of "32" class HSLA plates Comparable; not significantly higher than AH32 in static strength
Yield strength Similar to AH32 (plate-class yield level) Similar; DH32 matching yield class requirements
Elongation Good ductility typical of HSLA plates Good ductility; comparable to AH32
Impact toughness Specified for moderate low‑temperature performance Enhanced impact toughness at lower temperatures (primary differentiator)
Hardness Moderate (compatible with welding and forming) Similar; not designed as high-hardness steel

Interpretation: - Static strength properties (yield and tensile) for both grades are generally comparable because both belong to the same strength class; the key mechanical differentiation is impact toughness at lower temperatures where DH32 is specified to retain higher energy absorption. - Ductility and elongation are similar; the microalloying and TMCP control aim to maintain ductility while improving toughness in cold service for DH32.

5. Weldability

  • Weldability drivers: carbon content, effective hardenability (Mn and alloying), microalloying (Nb, V, Ti), and impurity levels (P, S, N). Higher hardenability and higher carbon equivalent (CE) increase cold-cracking risk and preheat requirements.
  • Common carbon equivalent and weldability indices to interpret qualitatively:
  • $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$
  • $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$
  • Interpretation:
  • Both AH32 and DH32 are engineered for good weldability: low carbon and controlled alloying keep $CE_{IIW}$ and $P_{cm}$ relatively low compared with quenched & tempered steels.
  • DH32’s stricter impurity control and TMCP-driven microstructure can reduce susceptibility to cold cracking, but some processing choices (microalloy content and thickness) can slightly raise hardenability compared to AH32. As a result, welding procedure specifications (preheat, interpass temperature, consumables, and post-weld heat treatment if required) should be based on plate thickness, welding energy, and CE/Pcm calculations.
  • Practical effect: Expect both grades to be readily weldable using standard procedures for ship plate steels, but DH32 may require modestly more conservative preheat/interpass control in thick sections or highly restrained joints when low-temperature toughness must be preserved.

6. Corrosion and Surface Protection

  • Both AH32 and DH32 are carbon/HSLA steels (non‑stainless). They rely on surface protection systems for corrosion resistance:
  • Common protections: blast-cleaning and primer/epoxy/polyurethane coatings, hot-dip galvanizing (for small components), and sacrificial anodes in marine environments for corrosion control on offshore structures.
  • Stainless-specific indices (e.g., PREN) are not applicable to these non-stainless plate steels. If stainless performance is required, a stainless grade with a PREN calculation would be selected:
  • Example of PREN for stainless alloys (not applicable here): $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • Selection notes:
  • Corrosion protection strategy is independent of AH32 vs DH32 choice; the latter choice is driven by mechanical/toughness requirements. For exposed hulls and harsh marine environments, choose coatings and cathodic protection appropriate to expected service life and maintenance intervals.

7. Fabrication, Machinability, and Formability

  • Fabrication:
  • Both grades form and bend well within typical plate-forming limits; springback and bend radii follow standard HSLA guidelines. DH32 may be slightly more demanding for very cold forming, given its focus on low-temperature toughness, but differences are small.
  • Machinability:
  • Both are not optimized for high-speed machining; machinability is typical of low‑carbon HSLA steels—good with appropriate tooling and coolant. Microalloy elements that increase strength can marginally reduce machinability.
  • Finishing:
  • Grinding, chamfering, and edge preparation follow standard practices. Welding consumable selection should match base-metal toughness and chemistry for both grades.

8. Typical Applications

AH32 (typical uses) DH32 (typical uses)
Hull plating and decks for temperate service conditions Hull plating and structural members intended for colder climates or arctic/near‑arctic service
General ship structural members where moderate low‑temperature toughness is sufficient Offshore platforms and vessels requiring guaranteed impact performance at lower temperatures
Superstructures and internal structures with less severe low‑temperature demand Areas with high toughness demand (e.g., double bottoms, inner bottom where brittle fracture risk is higher in cold)
Cost-sensitive projects where standard HSLA performance suffices Projects prioritizing low-temperature fracture safety and longer fracture arrest distances

Selection rationale: - Choose AH32 for cost-effective, high-strength structural applications in temperate environments where standard impact requirements are met. - Choose DH32 when design loading and service temperature require a higher guaranteed impact toughness margin at lower temperatures—this choice is a risk‑mitigation measure against brittle fracture in cold service.

9. Cost and Availability

  • Relative cost:
  • AH32 is typically slightly less expensive than DH32 on a per-ton basis because DH32 may require tighter steelmaking controls, more precise TMCP, and stricter inspection/testing for low-temperature toughness.
  • Availability by product form:
  • Plate and, in some markets, coils in AH32 and DH32 are commonly available from ship plate mills; availability depends on mill capability to deliver TMCP plates and on regional demand.
  • Lead times: DH32 can have longer lead times or minimum order quantities if mills need to schedule specific process control or additional testing.

10. Summary and Recommendation

Criterion AH32 DH32
Weldability High (standard HSLA practices) High, but may need slightly more conservative preheat/interpass in thick, restrained joints
Strength–Toughness balance Strong with good toughness for moderate temperatures Similar static strength with superior guaranteed low-temperature toughness
Cost Lower (generally) Higher (process and testing premiums)

Recommendation: - Choose AH32 if you require a robust, economical HSLA ship plate for temperate service where standard impact properties meet design requirements and where fabrication ease and cost are priorities. - Choose DH32 if the structure will operate in colder service environments or if design codes/clients require higher guaranteed impact toughness at lower temperatures; select DH32 when brittle-fracture risk mitigation and higher fracture-arrest capability are important.

Final practical note: Always consult the specific classification society or national standard specification for the precise chemical limits, mechanical property tables, and required impact test temperatures for AH32 and DH32 equivalents. Welding procedure specifications (WPS), heat input limits, and non‑destructive testing requirements should be developed using the actual plate mill certificates and project design temperature requirements.

Back to blog