A333 Gr6 vs A106 Gr.B – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

ASTM A333 Grade 6 and ASTM A106 Grade B are two commonly specified carbon-steel pipe grades in pressure piping, oil & gas, and general process industries. Engineers and procurement professionals frequently weigh these grades against one another when choosing pipe or plate for systems that balance cost, weldability, mechanical performance, and service temperature. Typical decision contexts include selection for cryogenic or low-temperature service versus higher-temperature conveyance, and priorities such as guaranteed impact toughness versus fabrication economy.

The principal practical distinction is the guaranteed low-temperature impact performance of A333 Grade 6 versus the general-purpose, elevated-temperature focus of A106 Grade B. Because both are plain-carbon/low-alloy steels with similar strength levels, the comparison centers on toughness at temperature, specified testing and acceptance criteria, and downstream implications for welding, inspection, and protective measures.

1. Standards and Designations

  • ASTM/ASME:
  • A333 Grade 6 — “Seamless and Welded Steel Pipe for Low-Temperature Service.” Often used for low-temperature or cryogenic applications where impact toughness at a specified low temperature is required.
  • A106 Grade B — “Seamless Carbon Steel Pipe for High-Temperature Service.” Common for refinery, petrochemical and process piping where elevated temperature strength and economy are primary considerations.
  • EN (European): Comparable but not identical equivalents exist in EN standards (e.g., P265/275/355 family) — selection requires cross-referencing mechanical and impact requirements.
  • JIS/GB: Japanese and Chinese standards include low-temperature variants; direct equivalence must be verified by mechanical and impact specifications.
  • Classification: Both are carbon/low-alloy steels (not stainless, not tool steel, not HSLA in the strict sense). A333 Grade 6 is a low-temperature carbon steel with mandatory impact testing; A106 Grade B is a general-purpose carbon steel for elevated or ambient temperature service.

2. Chemical Composition and Alloying Strategy

The two grades are deliberately simple in chemistry: they rely on carbon and manganese as the primary strength contributors, with tight limits on phosphorus and sulfur to avoid embrittlement and hydrogen-related problems. Alloying elements beyond C, Mn, Si are either absent or present only in trace amounts.

Table: Typical chemical composition (wt%) — consult mill test report (MTR) and the applicable ASTM specification for contract-level values. The table shows representative limits commonly cited in industry practice.

Element A333 Gr 6 (typical limits) A106 Gr B (typical limits)
C ≤ 0.30 (max) ≤ 0.30 (max)
Mn ≈ 0.30–1.20 (typical) ≈ 0.29–1.06 (typical)
Si ≤ 0.10–0.35 ≤ 0.10–0.35
P ≤ 0.035 (max) ≤ 0.035 (max)
S ≤ 0.035 (max) ≤ 0.035 (max)
Cr generally trace generally trace
Ni generally trace generally trace
Mo generally trace generally trace
V, Nb, Ti, B, N not specified / trace in most melts not specified / trace in most melts

Notes: - Values are indicative typical limits and industry practice; exact contractual limits are determined by the relevant ASTM specification and purchaser requirements. - A333 Gr6 chemistry is controlled to ensure low-temperature toughness; this commonly implies slightly tighter cleanliness and low impurity levels rather than substantial alloy additions. - Neither grade is designed as stainless or highly alloyed; corrosion resistance must be achieved by coatings, linings, or selection of stainless alloys if needed.

How alloying affects properties: - Carbon increases strength and hardness but lowers weldability and toughness if excessive. - Manganese contributes to hardenability and tensile strength and helps counteract sulfur’s embrittling effect by forming manganese sulfides. - Silicon is a deoxidizer and may marginally increase strength. - Alloying elements such as Cr, Ni, Mo increase hardenability and high-temperature strength if present; they are not significant in these base grades.

3. Microstructure and Heat Treatment Response

Typical microstructures: - Both grades are normally supplied in the as-rolled or normalized condition for piping. The microstructure is predominantly ferrite-pearlite for conventional mill processing. - A333 Grade 6 is often normalized or thermally treated/controlled during production to ensure a fine-grained ferrite–pearlite structure with good impact toughness at low temperatures. - A106 Grade B is usually supplied as normalized or as-rolled, intended for higher temperature strength and dimensional stability rather than cryogenic toughness.

Effect of heat treatments: - Normalizing refines grain size, improving toughness and making mechanical properties more uniform; both grades benefit from normalizing. - Quenching and tempering is not standard for these grades, but through higher alloying and controlled heat treatment, strength can be increased at the cost of ductility and toughness; this is not typical for pipe specified to A106 or A333. - Thermo-mechanical processing (controlled rolling) can enhance strength and toughness in both steels by grain refinement and precipitate control, and is more common where material is specified for higher strength with toughness.

4. Mechanical Properties

Representative mechanical property ranges for typical commercial product forms (pipe) are given below. Always verify the applicable ASTM table for contract minimums and MTR values.

Property A333 Gr 6 (typical) A106 Gr B (typical)
Tensile strength (UTS) ~415–550 MPa (typical range) ~415–550 MPa (typical range)
Yield strength (0.2% offset) ~240–350 MPa (depends on wall/thickness) ~240–350 MPa (depends on wall/thickness)
Elongation (in 2 in / 50 mm) ≥ 20–30% (varies by size) ≥ 20–30% (varies by size)
Impact toughness (Charpy V-notch) Specified minimum at low temp (e.g., -29°C to -46°C depending on spec) Usually no guaranteed low-temp impact requirement (tested at ambient if at all)
Hardness Moderate (typical HRC low/high HB ranges) Moderate

Interpretation: - In tensile/yield terms, both grades occupy similar bands; neither is a high-strength microalloyed plate by design. - A333 Gr 6 is specified to retain acceptable notch toughness at designated low temperatures; this is its defining mechanical advantage versus A106 Gr B. - A106 Gr B lacks mandatory low-temperature impact acceptance; its toughness at low temperature is not guaranteed without additional testing or specification.

5. Weldability

Weldability depends mainly on carbon equivalent (CE) and process heat input control. For plain carbon steels like A333 Gr6 and A106 GrB, weldability is generally good for standard fusion welding with appropriate preheat and procedure, but low-temperature service requires more stringent control to avoid cold-cracking and loss of toughness in the heat-affected zone.

Useful weldability indices: - The IIW carbon equivalent: $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ - The more conservative $P_{cm}$: $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$

Qualitative interpretation: - Both grades typically have low carbon and modest manganese, producing moderate CE values that imply routine welding is feasible with standard consumables. - For A333 Gr6 (low-temperature service), preheat, controlled interpass temperature, and post-weld heat control are often specified to protect HAZ toughness; welding procedures must be qualified for the required low-temperature impact performance. - A106 GrB is common and easily weldable for ambient and elevated-temperature services; however, when used in low-temperature environments, additional testing/controls are needed because base-metal toughness is not guaranteed.

6. Corrosion and Surface Protection

  • Neither A333 Gr6 nor A106 GrB are corrosion-resistant steels. Corrosion protection is achieved via painting, coatings, linings, cathodic protection, or galvanizing where appropriate.
  • PREN (pitting resistance equivalent number) applies to stainless grades and is not relevant to these carbon steels: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • Selection for corrosive environments should consider upgrade to stainless or corrosion-resistant alloys; for neutral aqueous or atmospheric exposures, coatings and cathodic protection are standard solutions.

7. Fabrication, Machinability, and Formability

  • Machinability: Both grades machine similarly since chemistry is comparable; machinability is typical for low-carbon steels. Cutting speeds and tooling should be set for moderate-strength carbon steel.
  • Formability and bending: Both form well in the annealed/as-rolled or normalized condition. A333 Gr6’s tighter toughness requirements mean mill rolling/heat treatment control is more careful, but field forming is comparable.
  • Welding, post-weld heat treatment (PWHT): PWHT is seldom required for either grade unless specified for service conditions (e.g., to reduce residual stresses or for high-temperature service). For low-temperature service with A333, procedure qualification to retain HAZ toughness is important.

8. Typical Applications

A333 Grade 6 A106 Grade B
Cryogenic or low-temperature piping and pressure vessels where Charpy impact at low temperature is specified (e.g., LNG piping, cold feed lines, refrigerated systems) High-temperature steam lines, process piping, refinery piping, general-purpose conduit for fluids at ambient to elevated temperatures
Offshore and subsea lines where low-temperature toughness and resistance to brittle fracture are required Transmission lines, boiler tubes, and process piping where elevated temperature strength and economy are priorities
Any piping application where specified low-temperature impact testing is contractually required Wide range of industrial piping where standard A106 chemical and mechanical properties meet design and cost targets

Selection rationale: - Choose A333 Gr6 where the design temperature approaches or goes below the ductile–brittle transition temperature and low-temperature impact toughness must be guaranteed by specification and testing. - Choose A106 GrB where operating temperature is ambient to elevated and the purchaser favors a commonly available, economical, high-volume pipe grade.

9. Cost and Availability

  • A106 Grade B is one of the most widely produced and stocked seamless carbon-steel pipes globally; therefore, it tends to be more economical and easier to procure in a broad range of sizes and schedules.
  • A333 Grade 6 may carry a premium because of the additional low-temperature impact testing requirements and any extra mill processing (normalizing, controlled rolling, stricter quality control). Availability is generally good but may be more limited in unusual sizes or short lead times.
  • Product form matters: seamless vs welded vs ERW; large-diameter or heavy-wall sections will influence lead time and cost for both grades.

10. Summary and Recommendation

Summary table (qualitative)

Criterion A333 Gr 6 A106 Gr B
Weldability Good, but welding procedure must preserve HAZ toughness for low-temp service Good for general applications; standard welding procedures typically sufficient
Strength–Toughness balance Similar tensile/yield; superior guaranteed low-temperature toughness Similar tensile/yield; toughness not guaranteed at low temperatures
Cost Moderate — may be higher due to testing and processing Generally lower — widely available, economical

Recommendation: - Choose A333 Grade 6 if your application requires guaranteed impact toughness at low temperatures, if brittle fracture risk must be minimized, or if the specified design temperature is in the low-temperature/cryogenic range. Also choose A333 Gr6 when contractually required low-temperature testing or notch toughness acceptance criteria are mandated. - Choose A106 Grade B if you need an economical, widely available seamless carbon-steel pipe for ambient to elevated temperature service where low-temperature toughness is not a primary requirement, and where standard welding and fabrication practices suffice.

Final note: Both ASTM A333 Gr6 and A106 GrB are workhorse carbon-steel grades. The correct choice depends not on nominal tensile numbers alone but on the required lower service temperature, specified impact testing, welding procedure qualifications, and lifecycle corrosion-protection strategy. Always reference the applicable ASTM/ASME tables, request Mill Test Reports, and qualify welding procedures when service conditions approach the material’s toughness limits.

Back to blog

Leave a comment