Introduction

Alloy 718 and its variant 718H are frequently specified where a combination of high strength, corrosion resistance, and elevated-temperature performance is required — for example, in aerospace rotating components, gas turbines, high-pressure valves, and nuclear applications. Engineers, procurement managers, and manufacturing planners commonly face a selection dilemma: prioritize the baseline chemistry and heat-treatment flexibility (ease of fabrication and post-weld processing) or accept a higher-delivered strength/age condition that reduces required post-processing but limits formability and welding choices.

The principal practical distinction between the two grades lies not in a wholesale change of alloy family but in the delivered metallurgical state and its effect on pre-hardening (pre-aged) condition. In other words, 718H is typically offered with a delivery condition or slight chemistry tweak intended to provide higher as-received strength or improved high-temperature stability, whereas standard 718 is the base UNS N07718 Alloy 718 chemistry and is most commonly supplied in solution-treated or soft-annealed conditions for downstream processing and final age-hardening.

1. Standards and Designations

  • Common universal designations:
  • UNS: N07718 (Alloy 718)
  • Common aerospace/manufacturing specifications that reference Alloy 718: various AMS (Aerospace Material Specifications) and ASTM specifications for bars, forgings, plate, and weld filler. (Buyers should specify the exact AMS/ASTM/EN/GB/JIS number required for their application.)
  • Classification: Nickel-based precipitation-hardening superalloy (not a carbon or low-alloy steel).
  • Typical product forms covered by standards: bar, forgings, plate, sheet, pipe, and welding filler (rod/wire).

Note: 718H is normally an industry or mill designation indicating either a composition variant or—more commonly—a different delivery/heat-treated condition. Always confirm the specific standard/heat-treatment callout in purchase and engineering documents.

2. Chemical Composition and Alloying Strategy

The table below shows typical composition ranges for standard Alloy 718. 718H normally retains the same base chemistry (Ni–Cr–Fe with Nb, Mo, Ti, and Al) with only small adjustments sometimes made by producers (for example, slightly higher carbon or controlled trace elements) to improve creep strength or precipitation behavior. Because mill practices vary, final ordered specifications must be checked.

Element Typical Alloy 718 (range, wt%) Notes regarding 718H
C 0.03 – 0.08 718H may be specified with a slightly higher upper C limit in some specs for improved high‑temperature strength; confirm on PO.
Mn ≤ 0.35 Minor alloying only.
Si ≤ 0.35 Deoxidizer/tramp control.
P ≤ 0.015 Impurity control.
S ≤ 0.015 Impurity control.
Cr 17.0 – 21.0 Corrosion and oxidation resistance.
Ni Balance (~50 – 55) Base element; provides matrix and high-temperature strength.
Mo 2.8 – 3.3 Solid-solution strengthening; supports carbide/phase stability.
V typically trace Not a deliberate major addition.
Nb (+Ta) 4.75 – 5.5 (as Nb+Ta) Key for $\gamma''$ precipitation (strength).
Ti 0.65 – 1.15 Works with Al to form strengthening precipitates.
B ≤ 0.006 Small additions improve grain boundary strength.
N ≤ 0.05 Usually low; affects nitride formation.

How the alloying strategy works: - Ni provides the matrix phase (austenitic matrix in Ni alloys) and high-temperature base strength. - Cr gives oxidation/corrosion resistance. - Nb (and Ta), Ti, and Al form fine coherent precipitates (primarily $\gamma''$ and some $\gamma'$) that provide the majority of age-hardening strength. - Mo contributes to solid-solution strengthening and high-temperature creep resistance. - Microalloying elements (B, C) and low levels of N influence grain-boundary cohesion and creep fracture behavior.

3. Microstructure and Heat Treatment Response

  • Typical 718 microstructure (solution-treated or annealed condition): a predominantly $\gamma$ (Ni-based matrix) with carbides and a background of coarse grain structure if not mechanically worked. After age-hardening, a fine dispersion of $\gamma''$ (Ni3Nb) coherent platelets and some $\gamma'$ (Ni3(Al,Ti)) precipitates governs yield strength.
  • 718 heat treatment routes:
  • Solution treatment (e.g., 980–1020 °C) followed by controlled cooling to dissolve precipitates, then age-hardened (single or double aging cycles) to precipitate $\gamma''$ and $\gamma'$.
  • Thermo-mechanical processing (forgings/rolling) followed by solution and age to refine grains and optimize fatigue and creep strength.
  • 718H microstructure/response:
  • 718H is usually processed or heat-treated to produce a firmer as-delivered condition (partial aging or a stabilized microstructure) intended to improve as-received strength and/or high-temperature stability. This reduces the degree of solutioning available for downstream mechanical forming or the extent of further age hardening that is practical without re-solution treatment.
  • If 718H has altered carbon or trace element limits, those changes primarily affect carbide precipitation and grain boundary chemistry, which in turn affect creep-rupture and high-temperature long-term stability.

Practical implication: Standard 718 offers broader post-delivery processing latitude (easier to form, weld, or re-heat treat), while 718H reduces processing steps by arriving in a higher-strength/stabilized state at the cost of some formability and welding freedom.

4. Mechanical Properties

Property values for Alloy 718 depend strongly on processing and age condition. The table below provides qualitative and typical-range guidance; exact values must be taken from the applicable specification or mill test report.

Property Typical Alloy 718 (solution-treated and age-hardened) Typical 718H (as-delivered pre-hardened/stabilized)
Tensile Strength (UTS) High; typical ranges depend on age treatment (often 1000–1400 MPa range) Comparable or slightly higher in as-delivered condition due to pre-aging
Yield Strength (0.2% offset) High (often >700–1000 MPa depending on aging) Typically higher as-delivered; lower potential for further increase by aging
Elongation (in 50 mm) Moderate (8–20%, dependent on condition) Lower ductility compared to soft-annealed 718, due to higher strength
Impact Toughness Good at room temperature if properly heat treated; can drop with coarse grain or over-aging May be reduced compared with soft 718 if produced in a harder state
Hardness Varies with aging (commonly ~30–40 HRC in peak-aged conditions when converted) As-delivered hardness typically higher; less change with subsequent aging without re-solution

Interpretation: - Which is stronger? In as-delivered form, 718H is typically stronger. After full controlled age-hardening, standard 718 can reach similar peak properties if it has been solution-treated and properly aged. - Which is tougher/more ductile? Standard 718 provided in a soft/solution-treated state or properly tempered condition will offer better formability and higher ductility prior to final aging. 718H trades some ductility for as-received strength and stability.

5. Weldability

Weldability of nickel-based Alloy 718 family is generally good compared with high-hardness steels, but care is required due to age-hardening, potential segregation, and control of delta-phase or Laves phase formation. - Key welding factors: base carbon equivalent effects are less used for Ni alloys than for steels, but hardenability from Nb/Ti and carbon-controlled precipitates matters. Precipitate formation near the weld can embrittle or harden heat-affected zones. - Useful qualitative indices: - For steels one uses carbon equivalents; for Ni alloys, consider segregation and precipitate-forming elements. - Nevertheless, when comparing weldability, practitioners may use standard steel formulas as a qualitative reference. For example: $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$ - Interpretation (qualitative): higher values suggest more preheat/postheat and controlled cooling are needed. 718 alloys require controlled preheat/interpass and post-weld heat treatment to avoid deleterious precipitate formation and to restore designed mechanical properties. - Practical note: 718H, delivered in a pre-hardened/partially aged state, can be less tolerant of welding without full re-solution and re-age treatment. If extensive welding is needed, specify solution-annealed 718 or plan post-weld solution and age heat-treatment.

6. Corrosion and Surface Protection

  • Alloy 718 family: good general corrosion resistance and excellent resistance to oxidation in many environments up to intermediate temperatures. Not stainless-class “superior” for highly oxidizing or chlorinated environments where specialized alloys are required.
  • Surface protection for non-stainless or degraded surfaces: mechanical finishing, protective coatings, or specialized plating can be used depending on service.
  • PREN (Pitting Resistance Equivalent Number) typically applies to stainless alloys; for Ni-based alloys this index is not commonly used. For reference, PREN is: $$ \text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N} $$ but this is not an established performance metric for Alloy 718.
  • 718 and 718H share broadly similar corrosion behavior because the base Cr and Ni content are essentially unchanged. Slight chemistry or heat-treatment differences that modify precipitates (carbides, Laves phase) can affect localized corrosion susceptibility and grain-boundary behavior over service life, particularly in aggressive environments.

7. Fabrication, Machinability, and Formability

  • Machinability: Nickel superalloys are tougher to machine than low-alloy steels. Both 718 and 718H are similar in cutting characteristics, but 718H’s higher as-delivered hardness can reduce tool life and require heavier duty tooling parameters.
  • Formability: Standard solution-treated 718 (soft) is more amenable to cold forming and shaping. 718H in a pre-hardened state will be less formable and may require hot working or re-solution treatment before significant forming.
  • Finishing: Surface grinding, polishing, and EDM are common. Heat treatments and residual stresses should be considered for tight tolerance components.

8. Typical Applications

Alloy 718 (standard) Alloy 718H
Aerospace rotating parts where post-fabrication aging is performed by the manufacturer or user; components requiring high strength after controlled age treatment; forgings and bars intended for machining and subsequent heat treatment. Components specified to arrive in a higher-strength or stabilized condition (e.g., valves, fittings, or components for which in-plant aging is impractical); applications requiring improved as-delivered creep stability.
Repairable components where welding and re-heat treatment are planned Parts where reduced need for further processing is prioritized; field installations with limited capacity for post-weld solution and aging
High-strength applications where designers call out full solution and aging cycles for best properties Situations where procurement wants as-received higher strength and dimensional stability; sometimes used where long-term high-temperature service is expected without further aging cycles

Selection rationale: - Choose standard 718 when downstream forming, welding, or tailored age-hardening is needed. - Choose 718H when buyers require a higher as-delivered strength/stability and when subsequent thermal cycles are impractical or when mill-proven stability is required for long-term elevated-temperature service.

9. Cost and Availability

  • Relative cost: Both are nickel-based superalloys and carry high raw-material costs; 718H may command a modest premium if the mill performs additional stabilization/processing or if it requires tighter control of trace elements.
  • Availability: Alloy 718 in standard specifications is widely available globally in bars, forgings, plate, and weld filler. 718H availability is more mill-specific and may have limited certification options or longer lead times depending on required heat treatment and documentation.
  • Product form matters: bars and forgings are commonly stocked; custom sizes or special heat-treated conditions (718H) may require longer lead times.

10. Summary and Recommendation

Attribute 718 (standard) 718H
Weldability Good with standard precautions; easier if supplied in solution-annealed condition More restrictive; pre-hardened state can complicate welding without post-weld solution/age
Strength–Toughness balance Flexible: can be tailored by heat treatment to balance strength and toughness Higher as-received strength; may have reduced ductility and toughness relative to soft 718
Cost Baseline for Alloy 718 Slight premium possible for pre-stabilized/aged product

Conclusion — clear guidance: - Choose 718 (standard UNS N07718) if you need flexibility: if significant forming, machining, or welding will be done before final heat treatment, or if you plan to perform controlled solution treatment and aging in your facility to achieve peak properties. - Choose 718H if you need a component that arrives in a higher-strength or stabilized state (reduced need for subsequent heat treatment), if long-term high-temperature stability in service is prioritized, or if procurement constraints require a ready-to-use, higher-strength delivery condition — but plan for reduced formability and more restrictive welding/post-weld procedures.

Final note: Because “718H” can be a mill or purchaser-specific designation, always specify required chemistry, mechanical properties, heat-treatment, and post-weld requirements in purchase documents. Request mill test reports and heat-treatment records and confirm whether the delivered material is solution-annealed, fully aged, or pre-stabilized so that fabrication and service performance are predictable.

Back to blog

2 comments

This is a fascinating comparison, especially regarding how 718H reduces downstream processing at the cost of welding flexibility. I’m currently looking into 718H for a high-pressure valve project where we need that extra as-delivered strength, but I’m concerned about the long-term scalability of our quality management system when handling these specialized, mill-specific alloy certifications. Does the complexity of tracking these specific heat-treatments significantly impact the overall operational budget compared to standard 718? I’ve been reading about how hidden operational layers and regulatory tracking drive up project costs in other complex, high-stakes industries here https://guiadebetnacionalbrasil.com and it made me wonder if there’s a similar “hidden cost” logic when scaling production with 718H due to the more restrictive certification requirements you mentioned?

Carla

This is an excellent breakdown of the metallurgical differences between 718 and 718H. I’m currently looking into 718H for a high-pressure valve project where we need that extra as-delivered strength, but I’m concerned about the long-term scalability of our current management system when handling these specialized alloy workflows. Since the article mentions that 718H is often a mill-specific designation that requires tighter documentation, do you think the complexity of tracking these specific heat-treatments significantly impacts the overall operational budget compared to standard 718? I’ve been reading about how hidden operational layers drive up project costs in other complex industries here https://igaming-solution.com/guides/igaming-software-cost/ and it made me wonder if there’s a similar “hidden cost” logic when scaling production with 718H due to the more restrictive welding and certification requirements you mentioned?

Scott

Leave a comment