304 vs 204Cu – Composition, Heat Treatment, Properties, and Applications
Share
Table Of Content
Table Of Content
Introduction
Choosing between 304 and 204Cu is a frequent procurement and design dilemma for engineers and manufacturing planners: should you pay for higher nickel content and the long track record of 304, or specify a lower‑nickel, copper‑bearing alternative that can cut material cost while preserving key properties? Typical decision contexts include corrosion vs. cost tradeoffs, weldability and post‑weld performance, and whether cold working or forming requirements change the effective strength envelope.
The principal technical distinction is that 204Cu is an economical, copper‑bearing austenitic stainless steel designed to reduce nickel content while using copper (and sometimes nitrogen/manganese) for solid‑solution and precipitation strengthening. 304 is the conventional austenitic stainless with higher nickel for stable austenite and broad environmental resistance. These two grades are compared because they occupy the same austenitic stainless class but pursue different alloying strategies (nickel vs. copper/manganese/nitrogen) to meet design objectives.
1. Standards and Designations
- 304:
- Common designations: AISI 304, UNS S30400, EN 1.4301, JIS SUS304, GB 06Cr19Ni10.
- Classification: Austenitic stainless steel (general purpose stainless).
- Covered by standards such as ASTM A240/A480 (plate/sheet/bar), ASME SA240, EN 10088 family.
- 204Cu:
- Common designations: UNS S20430, often referred to as Type 204Cu in commercial literature; check local standard equivalents.
- Classification: Austenitic stainless steel, low‑nickel, copper‑alloyed, often specified as an economical alternative to 304.
- Covered by various commercial specifications and some ASTM forms; availability and standard coverage can be less ubiquitous than 304—verify the specific product standard for each form.
2. Chemical Composition and Alloying Strategy
Table below summarizes typical composition ranges used commercially. These are representative ranges drawn from common specifications; always confirm exact composition in the purchasing specification.
| Element | 304 (typical range, wt%) | 204Cu (typical range, wt%) |
|---|---|---|
| C | ≤ 0.08 | ≤ 0.08 |
| Mn | ≤ 2.0 | ~1.5–3.0 |
| Si | ≤ 1.0 | ≤ 1.0 |
| P | ≤ 0.045 | ≤ 0.04 |
| S | ≤ 0.03 | ≤ 0.03 |
| Cr | 18.0–20.0 | ~18.0–19.0 |
| Ni | 8.0–10.5 | ~3.5–5.0 |
| Mo | 0 | 0 |
| V | trace | trace |
| Nb (Cb) | none | none |
| Ti | none | none |
| B | trace | trace |
| N | ≤ 0.10 | ~0.03–0.20 |
| Cu | ~0 | ~1.0–3.0 |
How alloying affects properties - Nickel (Ni) stabilizes the austenitic phase, improves toughness and corrosion resistance—especially in chloride environments—and enhances formability. 304’s higher Ni content gives it stable austenite without relying on high Mn/N. - Copper (Cu) in 204Cu provides solid‑solution strengthening and improved resistance in certain acidic environments (e.g., sulfuric acid) and can enhance resistance to some forms of localized corrosion or biofouling in specific conditions. - Nitrogen (N) and manganese (Mn) are used in low‑Ni alloys to stabilize austenite and provide strength by interstitial solution and strain‑ageing effects. - Chromium (Cr) provides general oxidation and corrosion resistance through passive film formation; both grades have comparable Cr.
3. Microstructure and Heat Treatment Response
- Typical microstructures:
- Both 304 and 204Cu are fully austenitic in annealed condition when specified chemical limits are met. Microstructure is generally equiaxed austenite with possible small amounts of ferrite depending on composition and cooling.
- Response to processing:
- Annealing (solution anneal) at nominal austenitizing temperatures followed by rapid cooling yields ductile, corrosion‑resistant austenite for both grades.
- Cold working increases dislocation density and raises strength while reducing ductility. 204Cu often achieves higher work‑hardening rate due to combined effects of Cu and N, so comparable cold work levels can produce higher yield/tensile strength than 304.
- Normalizing is not normally used for austenitic stainless steels; conventional quench and temper cycles used in ferritic/HSLA alloys are not applicable. Both steels are not hardenable by conventional thermal quenching; strengthening is achieved by cold work and minor precipitation phenomena.
- Thermo‑mechanical processing (rolling, controlled cooling) affects grain size and texture; both grades benefit from controlled processing to tailor formability and surface quality.
4. Mechanical Properties
The following table provides comparative performance characteristics in commonly supplied (annealed/solution‑treated) condition. Exact values vary with product form, cold work, and supplier.
| Property | 304 (annealed) | 204Cu (annealed/typical behavior) |
|---|---|---|
| Tensile strength | Good, balanced ductile tensile strength | Comparable to slightly lower or similar; can increase notably with cold work |
| Yield strength | Moderate, good ductility | Slightly higher yield in some conditions due to Cu/N solid‑solution strengthening |
| Elongation (ductility) | High ductility (excellent formability) | Generally high but marginally lower than 304 at comparable cold work levels |
| Impact toughness | Very good at room temperature | Very good at room temperature; comparable to 304 |
| Hardness | Moderate (soft in annealed condition) | Slightly higher hardness potential after work hardening |
Explanation - 304 exhibits a balance of strength and ductility with excellent toughness owing to higher nickel content and stable austenite. - 204Cu uses copper and nitrogen/manganese for strengthening; this makes it able to reach similar tensile levels when cold worked and in some annealed conditions may show modestly higher yield. Ductility remains good but may be slightly reduced relative to 304 at similar work levels.
5. Weldability
- General points:
- Both grades are commonly welded by standard processes (GMAW/MIG, GTAW/TIG, SMAW). Preheat is generally not required for thin sections.
- Lower carbon limits help avoid carbide precipitation and sensitization during slow cooling, but welding procedure controls are still important for corrosion-critical components.
- Effect of composition:
- 304’s higher Ni makes it forgiving with respect to weld microstructure and reduces risk of solidification cracking in many conditions.
- 204Cu has lower Ni and higher Mn/Cu/N may change solidification mode and hot cracking susceptibility; some filler metals and welding parameters may need to be adjusted. Use a matching filler or a 308/309L type filler depending on application and required corrosion resistance.
- Hardenability and carbon equivalent indices:
- For qualitative interpretation of weldability, use indices such as: $$ CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15} $$ $$ P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000} $$
- Interpretation: higher $CE_{IIW}$ or $P_{cm}$ indicate increased propensity for hardening and cracking during welding and may require pre‑/post‑weld heat treatments or controlled cooling. 204Cu’s lower Ni but elevated Cu and Mn will alter the indices relative to 304; qualitatively, 204Cu can be welded successfully but requires qualified procedures and attention to filler selection and post‑weld cleaning.
- Practical note: when welding 204Cu in corrosion‑critical applications, qualify the weld procedure and test for joint corrosion performance; filler selection often opts for Ni‑containing fillers to maintain corrosion performance.
6. Corrosion and Surface Protection
- Stainless behavior:
- Both alloys rely on chromium‑rich passive film for corrosion resistance in atmospheric and many aqueous environments.
- 304 is a well‑proven general‑purpose stainless with good resistance to oxidizing environments, food processing, and many chemicals. It is not as resistant as Mo‑bearing grades (e.g., 316) in chloride/pitting environments.
- Role of copper:
- Copper in 204Cu can improve resistance to certain reducing acids (notably sulfuric acid) and can help with biofouling resistance in specific service conditions. However, copper does not substitute for molybdenum concerning pitting resistance in chloride environments.
- Pitting Resistance Equivalent Number (PREN):
- For pitting ranking, the PREN is commonly used: $$ \text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N} $$
- Interpretation: because both 304 and 204Cu lack Mo, PREN values are modest; nitrogen in 204Cu can increase PREN somewhat, but PREN remains substantially lower than Mo‑alloyed stainless steels. PREN is most useful for comparing alloys with Mo present; for Cu‑bearing grades, PREN provides limited insight into acid behavior.
- Surface protection for non‑stainless components:
- If components are not stainless (not applicable here), typical protections include galvanizing, painting, or conversion coatings. For 304/204Cu, surface finishing, passivation, and appropriate cleaning are the usual protective strategies.
7. Fabrication, Machinability, and Formability
- Forming and bending:
- 304 has excellent formability and deep‑drawing characteristics in annealed condition.
- 204Cu is also formable, but because it work hardens readily, springback and the force required can be higher for equivalent deformations.
- Machinability:
- Austenitic stainless steels are generally more difficult to machine than carbon steels due to work hardening and low thermal conductivity. 204Cu may machine similarly or slightly better than 304 in certain conditions due to alloy differences, but tooling and feeds should be selected for austenitic stainless practice.
- Finishing:
- Both attain good surface finishes with standard finishing practices (grinding, polishing). Copper content may affect coloration slightly in some finishes but not typically a practical issue.
- Welding fabrication:
- Careful selection of filler metals, interpass temperatures, and joint design is required for both grades to avoid distortion and maintain corrosion resistance.
8. Typical Applications
| 304 (common uses) | 204Cu (common uses) |
|---|---|
| Food processing equipment, kitchenware, sinks, domestic appliances | Cost‑sensitive appliance components, decorative trim, automotive interior/exterior trim |
| Architectural and structural cladding, handrails | General corrosion‑resistant components where 304 is used but cost reduction is attractive |
| Heat exchangers, tanks, piping in non‑high chloride service | Heat exchangers and fittings in certain acidic services (sulfuric) where Cu provides benefit |
| Fasteners, springs (certain variants) | Components requiring higher strength after cold working and modest corrosion resistance |
Selection rationale - Choose 304 when a proven, widely standardized alloy with well‑documented corrosion behavior and broad availability is required—especially for food, sanitary, and many architectural applications. - Choose 204Cu when procurement cost is a significant driver, when nickel reduction is desirable, and when expected service environments are moderate (not severe pitting/chloride exposure) or are specifically compatible with Cu benefits.
9. Cost and Availability
- Cost:
- 204Cu is designed to reduce nickel content and therefore can be less expensive than 304 when nickel prices are high. Cost advantage is tied to market pricing of Ni and Cu.
- 304 has stable, well‑established pricing and supply chains; it is often more predictable in long‑term procurement.
- Availability:
- 304 is one of the most widely available stainless steels globally and offered in many product forms (sheet, coil, plate, bar, tubing, wire).
- 204Cu is increasingly offered in sheet, coil, and some bar/tube forms but may not be as universally stocked in all regions or product forms; lead times and minimum order quantities should be checked with suppliers.
10. Summary and Recommendation
Summary table (qualitative)
| Metric | 304 | 204Cu |
|---|---|---|
| Weldability | Excellent, well‑understood; forgiving | Good with qualified procedures; filler selection important |
| Strength – Toughness | Balanced strength and high toughness; excellent ductility | Comparable tensile, slightly higher yield with cold work; very good toughness |
| Cost | Moderate, well‑priced and stable supply | Generally lower material cost potential when Ni is expensive; supply varies |
Recommendation - Choose 304 if: - You need a well‑established, broadly standardized alloy with proven corrosion performance in general service, especially for food, sanitary, or long‑term outdoor architectural exposure. - Consistent global availability and material traceability are priorities. - You prefer a forgiving weld and fabrication window with broad filler metal and procedure options.
- Choose 204Cu if:
- Reducing nickel content and material cost is important, and the service environment is moderate (not severe chloride pitting) or benefits from copper’s electrochemical behavior (e.g., certain acid services).
- You expect substantial cold working or where slightly higher as‑worked yield is desirable.
- You are prepared to qualify welding procedures and confirm supply availability for the required product form.
Final note: both alloys are austenitic stainless steels with overlapping capabilities. The optimal choice depends on the specific corrosion environment, forming/welding plan, cost targets, and supply chain considerations. For specifications or critical components, require supplier certification of composition and mechanical tests and perform application‑specific corrosion or weld trials as necessary.