NDFEB N52 cube magnets are strong permanent magnets made from neodymium, iron, and boron. These small magnets are known for their great strength and many uses. N52 is the highest grade for neodymium magnets right now. It gives the strongest magnetic field. NDFEB N52 cube magnets can make magnetic fields up to 1.45 Tesla or 14,800 Gauss. This is much stronger than other types of magnets. Their small cube shape makes them perfect for many uses in industry, electronics, and projects at home.
| Property | Value for NDFEB N52 Cube Magnets |
|---|---|
| Material Composition | Neodymium (Nd), Iron (Fe), Boron (B) |
| Maximum Energy Product | 50-52 MGOe |
| Remanence (Br) | 14,200-14,800 Gauss |
| Coercivity (Hcb) | ≥11.6 kOe |
| Maximum Operating Temperature | 80°C (176°F) |
| Curie Temperature | 310°C (590°F) |
| Density | 7.4-7.6 g/cm³ |
NDFEB N52 cube magnets are used a lot in motors, generators, sensors, and green energy tech. Their strong magnetic fields help control things well and change energy efficiently in these devices. Speakers, headphones, and phone accessories also use N52 magnets. These magnets are small but powerful. Hobbyists like to use these magnets too. They make magnetic sculptures, floating experiments, and other fun projects with them.

The Science Behind NDFEB N52 Magnets
NDFEB N52 cube magnets are very strong. They get their strength from what they're made of and how they're made. These magnets contain neodymium, iron, and boron. The exact mix is usually 31% neodymium, 66% iron, and 1% boron, plus small amounts of other elements.
Making these magnets starts with melting the raw materials together. The molten alloy is then cooled quickly to form flakes. These flakes are ground into a fine powder and pressed into shape under a strong magnetic field. The pressed material is heated to very high temperatures, around 1000-1100°C, to fuse the particles. Finally, the magnets are heat-treated, shaped precisely, and coated for protection.
The strength of NDFEB N52 cube magnets comes from their crystal structure. During manufacturing, the magnetic domains in the material line up, creating a powerful magnetic field. N52 grade magnets can store more magnetic energy in a smaller space than any other magnet type.
| Property | Value for NDFEB N52 |
|---|---|
| Maximum Energy Product (BHmax) | 50-52 MGOe |
| Remanence (Br) | 14,200-14,800 Gauss |
| Coercivity (Hcb) | ≥11.6 kOe |
The N52 grade shows how strong the magnet is. It's the highest grade available for neodymium magnets right now. Lower grades like N35 or N42 are not as strong but might work for less demanding uses.
NDFEB N52 cube magnets have amazing magnetic properties. Their remanence, which measures leftover magnetism, is between 14,200 and 14,800 Gauss. This high remanence lets them create strong magnetic fields. Their coercivity, which shows how well they resist demagnetization, is at least 11.6 kOe.
To understand how strong these magnets are, think about this: a small 1/2-inch cube can lift over 30 pounds. This makes them much stronger than a ferrite magnet of the same size. Their strength-to-size ratio makes them perfect for uses where space is tight but strong magnetic fields are needed.

Advantages of NDFEB N52 Cube Magnets
NDFEB N52 cube magnets have many benefits. These magnets are very strong for their size, which makes them useful in many ways. A 1-inch N52 cube magnet can pull over 100 pounds.
NDFEB N52 cube magnets are also very durable. They keep their strength for a long time under normal use. Most of these magnets have a coating to stop rust and make them last longer.
Cube magnets have flat sides that make them easy to use. This shape helps in machines and sensors. Cube magnets also stack well, which is good for storage.
| Advantage | Description |
|---|---|
| Strength | High magnetic force in a small package |
| Durability | Resistant to demagnetization and corrosion |
| Precision | Flat surfaces for easy mounting and alignment |
| Versatility | Suitable for a wide range of applications |
These magnets can be used in many fields. They work well in electronics and green energy. Their strong fields help make power in wind turbines.
N52 cube magnets work well in heat up to 80°C (176°F). This makes them good for use in cars and factories. For hotter places, there are special types of these magnets.
NDFEB N52 cube magnets are better than other types. They are much stronger than ferrite or AlNiCo magnets of the same size. Using these magnets can make devices smaller and lighter.
Common Applications of NDFEB N52 Cube Magnets
NDFEB N52 cube magnets have many uses in different industries. These magnets play key roles in motors and generators for industrial use. Their strong fields help convert energy well in these machines. Many sensors also need N52 cube magnets to work right.
Consumer electronics often use NDFEB N52 cube magnets. They make speakers and headphones sound good while staying small. Hard drives use them to control read/write heads precisely. Phones have small N52 cube magnets in speakers and vibration parts.
The medical field uses NDFEB N52 cube magnets a lot. MRI machines need big neodymium magnets to make images. Some hearing aids use tiny N52 magnets to hold parts in place. These magnets help in many other medical tools too.
| Industry | Applications |
|---|---|
| Industrial | Motors, generators, sensors |
| Electronics | Speakers, hard drives, smartphones |
| Medical | MRI machines, hearing aids |
| Automotive | Electric motors, sensors |
| Renewable Energy | Wind turbines, generators |
Cars need NDFEB N52 cube magnets. Electric and hybrid cars use them in motors. Many car sensors work with N52 magnets. These include sensors for position, speed, and brakes.
Renewable energy relies on NDFEB N52 cube magnets. Wind turbines use big neodymium magnets to make power. Some new wave energy devices also use these strong magnets. They help turn wind and waves into electricity.
Hobbyists like to use NDFEB N52 cube magnets. People make magnetic sculptures and toys with them. These magnets work well in many projects, from simple to complex. Their strength makes them good for creative uses.
NDFEB N52 cube magnets show up in odd places. Some fishing reels use them for brakes. Magnetic therapy products often have these magnets, but they might not work. Magicians even use N52 cube magnets for tricks that seem impossible.

Handling and Safety Considerations
NDFEB N52 cube magnets are very strong. Their powerful fields can hurt you if you're not careful. Always keep these magnets away from children and pets. When working with N52 cube magnets, wear gloves and safety glasses.
Store them properly. Keep them in a cool, dry place away from electronics and magnetic items. Separate them to prevent damage. Use non-magnetic dividers for larger amounts. Wooden or plastic boxes work well for storage.
These magnets can harm medical devices. People with pacemakers should stay at least 6 inches away. The magnets might interfere with these devices. Ask a doctor if you're worried about magnet exposure.
| Safety Measure | Description |
|---|---|
| Personal Protection | Wear gloves and safety glasses |
| Storage | Use non-magnetic containers, keep magnets separated |
| Medical Precautions | Keep away from pacemakers and implanted devices |
| Handling | Use caution to avoid pinching, sudden attraction |
| Disposal | Follow local regulations for electronic waste |
NDFEB N52 cube magnets can harm electronics. Keep them away from computers, phones, and credit cards. Their strong fields can erase data or mess up devices. Check with airlines before flying with these magnets. Some have rules about shipping strong magnets.
Don't throw these magnets in the trash. Many areas treat them as electronic waste. Look up local rules for proper disposal. Some recycling centers will take these magnets.
Be careful when handling multiple N52 cube magnets. They can snap together quickly and hurt you or break. Use non-magnetic tools and work surfaces. This helps prevent accidents and keeps the magnets safe.
Choosing the Right NDFEB N52 Cube Magnet
Selecting the right NDFEB N52 cube magnet involves several factors. Size is key, as it affects the magnet's strength and use. Smaller cubes work well for precise tasks, while larger ones create stronger magnetic fields. The coating matters too.
Nickel plating resists corrosion, and epoxy or rubber coatings add protection and grip. Magnetization direction is crucial for good performance. NDFEB N52 cube magnets can be magnetized through thickness or along a face diagonal. The choice depends on how you plan to use it.
Axial magnetization is often better for focused magnetic fields. Diametric magnetization can create more complex field patterns.
| Factor | Considerations |
|---|---|
| Size | Application requirements, space constraints |
| Coating | Environmental conditions, handling needs |
| Magnetization | Field orientation, application specifics |
| Grade | Strength requirements, temperature range |
Pull force is important when choosing these magnets. It changes based on size and grade. A 1/2-inch N52 cube usually pulls about 20-25 pounds. Bigger cubes can pull over 100 pounds.
Choose a magnet with the right strength for your needs. Using too strong a magnet can cost more and be unsafe. Temperature needs also matter when picking a magnet. Normal N52 grade magnets work well up to 176°F.
For hotter uses, you might need special grades like N52H or N52SH. These keep their magnetic properties at high temperatures but are slightly weaker. Measuring magnet strength is key for quality control.
Gauss meters can check the magnetic field strength accurately. Pull force testers show practical strength measurements. These tools help ensure the magnets meet your needs.
Buying good NDFEB N52 cube magnets requires careful supplier selection. Good makers provide detailed specs and certifications. It's smart to test sample magnets before buying many.
Online shops are easy, but check that the magnets are real and good quality. People often make mistakes when choosing these magnets. They might pick ones that are too strong or too weak.
Not thinking about temperature, humidity, or chemicals can lead to magnet failure. It's important to consider all these factors when selecting NDFEB N52 cube magnets.
Maintenance and Care of NDFEB N52 Cube Magnets
Proper storage is crucial for maintaining NDFEB N52 cube magnets. Keep them in a cool, dry place away from moisture and heat. For long-term storage, use airtight containers with desiccants to prevent rust. Separate individual magnets with non-magnetic spacers to prevent damage.
Cleaning NDFEB N52 cube magnets requires gentle handling. Use a soft, lint-free cloth to remove dust and dirt. Avoid harsh chemicals or rough materials that could harm the coating. For tough dirt, use a mild soap solution, then dry the magnet well.
Preventing demagnetization is essential for these strong magnets. Keep them away from strong electromagnetic fields and high temperatures. The highest safe temperature for N52 grade magnets is usually 80°C (176°F). Exposure to higher temperatures can weaken the magnet forever.
| Care Aspect | Recommendation |
|---|---|
| Storage | Cool, dry place; use desiccants |
| Cleaning | Soft cloth; mild soap if needed |
| Temperature | Keep below 80°C (176°F) |
| Handling | Use non-magnetic tools |
Regular inspection helps find signs of wear or damage. Look for chips, cracks, or color changes in the coating. These could mean the magnet is rusting or breaking. If you see damage, replace the magnet to keep it working well and safely.
Proper handling techniques make NDFEB N52 cube magnets last longer. Use non-magnetic tools when working with them to avoid accidents and damage. Always keep magnets apart during transport to prevent chips or cracks from collisions.
Coating maintenance is key for longevity. Most NDFEB N52 cube magnets have a protective nickel or epoxy layer. Check this coating often for scratches or wear. If the coating is damaged, the magnet can rust and break down quickly.
By following these care tips, NDFEB N52 cube magnets can stay strong for many years. Regular upkeep ensures they keep working well in many uses, from factories to hobby projects.
Maintenance and Care of NDFEB N52 Cube Magnets
Proper care ensures the longevity of NDFEB N52 cube magnets. These strong magnets need specific storage conditions to stay powerful. A cool, dry place is best for keeping their magnetic properties. Humidity can cause rust, even with protective coatings on the magnets.
Using desiccants in storage containers helps. Cleaning these magnets is easy but needs care. A soft, lint-free cloth works well for removing dust. Don't use water or cleaning products if you can avoid it.
If needed, you can use a damp cloth, but dry the magnets right away. Temperature control is very important for these magnets. NDFEB N52 cube magnets can lose strength if they get too hot.
The highest safe temperature is usually 80°C (176°F). Going above this can permanently weaken the magnet. It's crucial to watch the temperature in places where heat might be an issue.
Regular checks help spot problems early. Look for any damage to the coating or signs of rust. Small chips or cracks can let air and moisture reach the magnet material. This can quickly weaken the magnet.
Replace damaged magnets soon to keep your system working well. Handling these magnets requires special tools and methods. Use plastic tools or non-magnetic tweezers when working with them.
This prevents accidental sticking and possible damage. Always keep magnets apart during transport or storage. Sudden collisions between magnets can cause chips or cracks.
Taking care of the coating is key for long-lasting performance. Most NDFEB N52 cube magnets have a nickel or epoxy coating. This layer protects against rust and physical harm. Check the coating often for any wear.
If the coating is damaged, think about recoating or replacing the magnet. Following these care tips can help NDFEB N52 cube magnets stay strong for years. Good maintenance ensures they keep working well in many uses.
These magnets are important in modern technology, from big machines to small electronics.