ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

Silver Steel

Silver Steel

Silver Steel High Carbon Tool Steel

Silver Steel is a premium high-carbon tool steel renowned for its exceptional hardness, wear resistance, and dimensional stability. This water-hardening steel grade is specifically engineered for precision tooling and structural components requiring superior mechanical properties and excellent machinability in the annealed condition.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs advanced vacuum melting and controlled forging processes to produce Silver Steel with exceptional cleanliness and uniform microstructure. Our precision heat treatment capabilities ensure optimal hardness distribution and dimensional stability, critical for high-precision structural applications and tooling requirements.

Key Applications

  • Precision structural components and machine frames
  • High-strength fasteners and connecting elements
  • Automotive structural parts and chassis components
  • Industrial machinery structural elements
  • Bridge construction high-stress components

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and complete metallurgical analysis. Our Silver Steel meets ASTM A681 and international tool steel standards, ensuring consistent performance in critical structural applications requiring high strength and reliability.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Silver Steel exhibits a fine pearlitic microstructure in the annealed condition, transforming to martensite upon water quenching. The high carbon content provides exceptional hardness potential, while the controlled alloy additions ensure uniform carbide distribution and enhanced hardenability for structural applications requiring superior strength-to-weight ratios.

Heat Treatment Process

MetalZenith employs controlled austenitizing at 760-780°C followed by water quenching and tempering at 150-200°C to achieve optimal hardness. For structural applications, stress relief annealing at 650-680°C ensures dimensional stability while maintaining excellent mechanical properties essential for load-bearing components.

Manufacturing Excellence

Our advanced production process includes vacuum degassing, controlled forging ratios, and precision heat treatment cycles. MetalZenith's quality systems ensure consistent grain structure, minimal segregation, and superior surface quality critical for structural applications in building construction and mechanical engineering.

Specialized Quality Testing

Comprehensive testing protocols include welding performance evaluation using standard procedures, forming capability assessment through bend testing, fatigue strength analysis under cyclic loading, and atmospheric corrosion resistance testing per ASTM standards. These tests ensure reliability in diverse structural environments.

Structural Application Engineering

For building construction, Silver Steel provides exceptional strength for high-stress connections and load-bearing elements. In bridge engineering, its fatigue resistance ensures long-term durability under dynamic loading. Mechanical manufacturing benefits from its precision machinability, while vehicle construction applications leverage its high strength-to-weight ratio for chassis components and safety-critical structures.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.95 - 1.05
Manganese (Mn)0.20 - 0.40
Silicon (Si)0.10 - 0.35
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.025
Chromium (Cr)0.10 - 0.30
Nickel (Ni)≤ 0.25
Copper (Cu)≤ 0.25

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 1800
Tensile Strength (MPa)2000 - 2200
Elongation (%)8 - 12
Impact Energy at 20°C (J)≥ 15
Hardness (HRC)60 - 65
Fatigue Strength (MPa)≥ 900

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.84
Melting Point (°C)1460 - 1500
Thermal Conductivity (W/m·K)42.7
Thermal Expansion (×10??/K)11.5
Elastic Modulus (GPa)210
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsRound Bars, Flat Bars, Plates, Sheets, Custom Forgings
Diameter Range3 - 300mm
Thickness Range1 - 80mm
Width Range10 - 500mm
Length Range500 - 6000mm
Standards ComplianceASTM A681, DIN 1.2210, BS 1407
Heat Treatment ConditionAnnealed, Hardened & Tempered
Surface FinishBlack, Turned, Ground, Polished

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Silver Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes state-of-the-art vacuum induction melting followed by controlled forging processes to achieve exceptional steel cleanliness and uniform carbide distribution. Our advanced metallurgical processing ensures superior mechanical properties and dimensional stability essential for structural applications.

Comprehensive Structural Testing

Our Silver Steel undergoes extensive testing including fatigue strength analysis, welding performance evaluation, forming capability assessment, and atmospheric corrosion resistance testing. These specialized tests ensure optimal performance in demanding structural applications across building construction and mechanical engineering.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Technical Support

MetalZenith provides tailored heat treatment services, precision machining, and comprehensive technical support for structural applications. Our engineering team offers application-specific guidance for optimal material selection and processing parameters to meet your exact structural requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo