Titanium Steel

Titanium Steel - Premium Stainless Steel Alloy

Titanium Steel is an advanced stainless steel alloy incorporating titanium for enhanced corrosion resistance and mechanical properties. This premium grade combines the excellent formability of austenitic stainless steel with superior resistance to intergranular corrosion and stress corrosion cracking, making it ideal for demanding applications in corrosive environments.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum melting and controlled atmosphere processing to produce Titanium Steel with exceptional purity and homogeneity. Our advanced solution annealing and passivation processes ensure optimal microstructural stability and maximum corrosion resistance, critical for food processing, medical, and chemical applications.

Key Applications

  • Chemical processing equipment and reactors
  • Food and beverage processing machinery
  • Medical instruments and surgical devices
  • Marine hardware and offshore platforms
  • Architectural facades and decorative elements

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including pitting corrosion testing, intergranular corrosion evaluation, and comprehensive passivation film analysis. Our Titanium Steel meets FDA, 3-A Sanitary Standards, NACE, and major international specifications, ensuring reliability in critical applications requiring superior corrosion resistance.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Titanium Steel exhibits a stabilized austenitic microstructure with titanium carbide precipitates that prevent chromium carbide formation at grain boundaries. The titanium addition provides excellent resistance to intergranular corrosion and sensitization, while maintaining superior formability and weldability characteristics typical of 18-8 stainless steels.

Heat Treatment Process

MetalZenith employs solution annealing at 1040-1120°C followed by rapid cooling to achieve optimal carbide dissolution and titanium stabilization. Our controlled cooling process prevents harmful precipitate formation while ensuring complete austenite retention and maximum corrosion resistance.

Advanced Manufacturing Process

Our manufacturing process includes vacuum induction melting for superior cleanliness, controlled titanium addition for optimal stabilization, and precision hot rolling with controlled finishing temperatures. Post-processing includes solution annealing, descaling, and comprehensive passivation treatment to develop maximum corrosion resistance.

Specialized Quality Testing

MetalZenith conducts comprehensive testing including pitting potential measurement (>200mV vs SCE), intergranular corrosion testing per ASTM A262 Practice A, stress corrosion cracking evaluation in chloride environments, and passivation film thickness analysis. Additional testing includes sensitization resistance and carbide precipitation evaluation.

Application-Specific Technical Considerations

For chemical processing applications, Titanium Steel provides excellent resistance to nitric acid and organic acids. In food industry applications, the material meets FDA requirements with superior cleanability and bacterial resistance. Medical device applications benefit from biocompatibility and sterilization resistance. Marine applications utilize the enhanced chloride resistance, while architectural applications leverage the material's aesthetic durability and low maintenance requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.08
Chromium (Cr)17.0 - 20.0
Nickel (Ni)9.0 - 12.0
Titanium (Ti)5 × (C + N) - 0.70
Manganese (Mn)≤ 2.00
Silicon (Si)≤ 1.00
Phosphorus (P)≤ 0.045
Sulfur (S)≤ 0.030
Nitrogen (N)≤ 0.10

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 205
Tensile Strength (MPa)515 - 690
Elongation (%)≥ 40
Hardness (HRB)≤ 95
Pitting Resistance (PREN)≥ 24
Impact Energy at 20°C (J)≥ 120

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.93
Melting Point (°C)1400 - 1450
Thermal Conductivity (W/m·K)16.2
Thermal Expansion (×10??/K)17.3
Electrical Resistivity (μΩ·cm)72
Elastic Modulus (GPa)200

📏 Product Specifications

SpecificationDetails
Available FormsSheets, Plates, Bars, Tubes, Coils, Wire
Thickness Range0.5 - 50mm
Width Range1000 - 2000mm
Length Range2000 - 6000mm
Standards ComplianceASTM A240, AISI 321, EN 1.4541, JIS SUS321
Surface Finish2B, BA, No.4, HL, Mirror
Heat Treatment ConditionSolution Annealed and Passivated

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Titanium Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes vacuum induction melting and electroslag remelting processes with precise titanium addition control to achieve optimal microstructural uniformity. Our advanced processing ensures complete titanium dissolution and carbide stabilization, resulting in superior intergranular corrosion resistance and enhanced mechanical properties.

Comprehensive Corrosion Testing Protocol

MetalZenith conducts extensive corrosion testing including pitting potential measurement (ASTM G150), intergranular corrosion testing (ASTM A262), stress corrosion cracking evaluation (ASTM G123), and passivation film thickness analysis using XPS. Our rigorous testing ensures optimal performance in aggressive chemical environments.

Manufacturing Advantage 2
Manufacturing Advantage 3

Specialized Processing & Technical Support

MetalZenith offers customized solution annealing, precision cold working, and specialized surface finishing services tailored to specific application requirements. Our metallurgical experts provide comprehensive technical support for material selection, fabrication guidelines, and corrosion prevention strategies.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo