Technical Specifications
Product Overview
Metallurgical Characteristics
S50C exhibits a predominantly pearlitic microstructure with fine carbide distribution when properly heat treated. The medium carbon content provides an optimal balance between strength and ductility, while the controlled manganese content enhances hardenability and structural uniformity. MetalZenith's controlled cooling processes ensure consistent grain size and carbide morphology for superior structural performance.
Heat Treatment Process
MetalZenith employs precision heat treatment cycles including normalization at 850-900°C followed by controlled cooling, or quenching from 820-860°C with tempering at 550-650°C. Our computer-controlled furnaces maintain precise temperature uniformity ±5°C, ensuring consistent mechanical properties and optimal microstructural development throughout the material cross-section.
Manufacturing Process Excellence
Our S50C production utilizes electric arc furnace melting with secondary refining, continuous casting, and controlled rolling processes. Advanced inclusion control and degassing techniques ensure superior cleanliness and structural integrity. Real-time quality monitoring throughout production guarantees consistent chemical composition and mechanical properties.
Specialized Quality Testing
MetalZenith conducts comprehensive testing specific to structural applications: welding performance evaluation including HAZ toughness testing, forming capability assessment through bend tests, fatigue strength determination under cyclic loading conditions, and atmospheric corrosion resistance testing per ASTM standards. These specialized tests ensure S50C steel meets demanding structural engineering requirements.
Structural Application Engineering
For building construction, S50C provides excellent load-bearing capacity with predictable stress-strain behavior. In bridge engineering, the material's fatigue resistance and weldability ensure long-term structural integrity. For machinery manufacturing, the combination of strength and machinability enables complex component fabrication. In vehicle construction, S50C offers optimal strength-to-weight ratios for chassis and frame applications, while general engineering benefits from its versatile processing capabilities and reliable mechanical properties.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.47 - 0.53 |
| Manganese (Mn) | 0.60 - 0.90 |
| Silicon (Si) | 0.15 - 0.35 |
| Phosphorus (P) | ≤ 0.030 |
| Sulfur (S) | ≤ 0.035 |
| Chromium (Cr) | ≤ 0.20 |
| Nickel (Ni) | ≤ 0.20 |
| Copper (Cu) | ≤ 0.30 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Yield Strength (MPa) | ≥ 355 |
| Tensile Strength (MPa) | 610 - 760 |
| Elongation (%) | ≥ 17 |
| Impact Energy at 20°C (J) | ≥ 39 |
| Hardness (HB) | 179 - 229 |
| Fatigue Strength (MPa) | 290 - 320 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density (g/cm3) | 7.85 |
| Melting Point (°C) | 1460 - 1520 |
| Thermal Conductivity (W/m·K) | 51.9 |
| Thermal Expansion (×10??/K) | 11.5 |
| Elastic Modulus (GPa) | 210 |
| Poisson's Ratio | 0.27 - 0.30 |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Plates, Bars, Rods, Structural Sections, Forgings |
| Thickness Range | 5 - 200mm |
| Width Range | 100 - 3000mm |
| Length Range | 1000 - 12000mm |
| Standards Compliance | JIS G4051, ASTM A29, DIN C50, GB 45# |
| Heat Treatment Condition | Normalized, Quenched & Tempered, Annealed |
| Surface Finish | Hot Rolled, Cold Drawn, Machined, Polished |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing S50C Steel
Advanced Heat Treatment Technology
MetalZenith utilizes precision-controlled quenching and tempering processes with computerized temperature monitoring to achieve optimal microstructural refinement in S50C steel. Our advanced heat treatment facilities ensure consistent hardness distribution and enhanced mechanical properties throughout the material cross-section.
Comprehensive Structural Testing
Our quality assurance program includes specialized testing for structural applications: welding performance evaluation, forming capability assessment, fatigue strength testing under cyclic loading, and atmospheric corrosion resistance analysis. These tests ensure S50C steel meets demanding structural engineering requirements.
Custom Processing & Engineering Support
MetalZenith provides tailored heat treatment schedules, precision machining, and custom forming services for S50C steel components. Our technical team offers comprehensive engineering support including stress analysis, joint design consultation, and application-specific material optimization for structural projects.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
สอบถามด่วน
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications