S235JR is a non-alloy structural steel grade widely used in construction and general engineering applications. This hot-rolled steel offers excellent weldability, formability, and cost-effectiveness, making it the preferred choice for building structures, bridges, and general fabrication work requiring reliable mechanical properties and good workability.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs controlled hot rolling processes with precise temperature control to produce S235JR steel with consistent mechanical properties and excellent surface quality. Our advanced rolling technology ensures optimal grain structure and enhanced formability, critical for structural applications requiring complex fabrication.

Key Applications

  • Building structures and construction frameworks
  • Bridge construction and infrastructure projects
  • Mechanical manufacturing and equipment fabrication
  • Vehicle chassis and automotive components
  • General engineering and structural steelwork

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, weldability assessments, and dimensional verification. Our S235JR steel meets EN 10025-2 standards and various international specifications, ensuring consistent performance in structural applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

S235JR exhibits a ferritic-pearlitic microstructure typical of low-carbon structural steels. The controlled carbon content ensures excellent weldability while maintaining adequate strength for structural applications. The fine grain structure achieved through controlled rolling provides optimal balance between strength and ductility, essential for construction applications.

Heat Treatment Process

MetalZenith employs controlled hot rolling at temperatures between 1050-1200°C followed by controlled cooling to achieve optimal mechanical properties. Normalizing treatment at 850-950°C may be applied for enhanced uniformity and stress relief, particularly for thick sections used in critical structural applications.

Manufacturing Process

Our advanced manufacturing process includes continuous casting, controlled hot rolling with precise temperature monitoring, and quality inspection at every stage. MetalZenith's state-of-the-art rolling mills ensure consistent dimensional accuracy and surface quality essential for structural fabrication.

Structural Quality Testing

Comprehensive testing protocols include weldability assessment per AWS D1.1 standards, bend testing for formability evaluation, fatigue testing under cyclic loading conditions, and atmospheric corrosion resistance testing. Impact testing ensures adequate toughness for structural applications in various temperature conditions.

Application Engineering

For building structures, S235JR provides excellent load-bearing capacity with superior weldability for complex connections. In bridge engineering, its fatigue resistance and atmospheric corrosion properties ensure long-term durability. For mechanical manufacturing, the steel's formability enables complex shapes while maintaining structural integrity. Vehicle manufacturing benefits from its lightweight strength ratio and crash energy absorption characteristics.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.17
Manganese (Mn)≤ 1.40
Silicon (Si)≤ 0.40
Phosphorus (P)≤ 0.040
Sulfur (S)≤ 0.040
Nitrogen (N)≤ 0.012
Copper (Cu)≤ 0.55

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 235
Tensile Strength (MPa)360 - 510
Elongation (%)≥ 26
Impact Energy at 20°C (J)≥ 27
Hardness (HB)120 - 155
Fatigue Strength (MPa)180 - 220

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.85
Melting Point (°C)1450 - 1520
Thermal Conductivity (W/m·K)54.0
Thermal Expansion (×10??/K)12.0
Elastic Modulus (GPa)210
Poisson's Ratio0.30

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Beams, Channels, Angles, Bars
Thickness Range3 - 100mm
Width Range1000 - 3000mm
Length Range6000 - 12000mm
Standards ComplianceEN 10025-2, ASTM A36, JIS G3101
Delivery ConditionHot Rolled, Normalized
Surface FinishMill Scale, Shot Blasted, Pickled

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing S235JR

Manufacturing Advantage 1

Controlled Hot Rolling Technology

MetalZenith utilizes advanced controlled hot rolling processes with real-time temperature monitoring and precise cooling rates to achieve optimal grain structure in S235JR steel. Our sophisticated rolling technology ensures consistent mechanical properties and excellent surface finish throughout the material thickness.

Comprehensive Structural Testing

Our quality assurance program includes specialized testing for structural applications: weldability testing per AWS standards, bend testing for formability assessment, fatigue strength evaluation, and atmospheric corrosion resistance testing. This ensures reliable performance in demanding structural environments.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Fabrication Services

MetalZenith offers comprehensive custom processing services including precision cutting, forming, welding preparation, and surface treatment. Our technical support team provides expert guidance on structural design considerations and fabrication best practices for optimal project outcomes.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo