ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

MS 1400

MS 1400

MS 1400 Martensitic Steel - Advanced High-Strength Solution

MS 1400 is a premium martensitic steel grade engineered for applications demanding exceptional strength, hardness, and wear resistance. This advanced high-strength steel (AHSS) combines superior mechanical properties with excellent formability, making it ideal for automotive, aerospace, and industrial applications where weight reduction and structural integrity are critical.

MetalZenith's Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art controlled cooling technology and precision heat treatment processes to produce MS 1400 with consistent microstructure and optimal mechanical properties. Our advanced vacuum degassing systems ensure ultra-low inclusion content, while our proprietary quenching and tempering protocols deliver uniform hardness distribution throughout the material cross-section.

Key Applications & Industries

  • Automotive structural components and safety-critical parts
  • Aerospace landing gear and high-stress components
  • Industrial machinery and heavy equipment manufacturing
  • Oil and gas drilling equipment and downhole tools
  • Construction equipment and agricultural machinery

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015, ISO 14001:2015, and IATF 16949:2016 certifications. Every batch of MS 1400 undergoes comprehensive testing including chemical analysis, mechanical property verification, microstructural examination, and non-destructive testing to ensure compliance with international standards and customer specifications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

MS 1400 features a predominantly martensitic microstructure with fine carbide precipitates, achieved through controlled austenitization at 900-950°C followed by rapid quenching and precise tempering at 200-400°C. The optimized carbon content and alloying elements ensure excellent hardenability while maintaining adequate toughness for demanding applications.

Heat Treatment Process

MetalZenith employs a sophisticated heat treatment protocol involving vacuum or protective atmosphere heating to prevent decarburization, followed by controlled quenching in polymer or oil media. The subsequent tempering process is precisely controlled using automated furnace systems with ±5°C temperature accuracy to achieve target mechanical properties consistently.

Manufacturing Process

Production begins with electric arc furnace melting followed by secondary refining through ladle furnace and vacuum degassing to achieve ultra-low sulfur and phosphorus content. Continuous casting ensures homogeneous chemical composition, while controlled rolling and accelerated cooling optimize the final microstructure. Advanced process control systems monitor critical parameters throughout production.

Quality Standards & Testing

Every batch undergoes comprehensive testing including optical emission spectroscopy for chemical analysis, tensile and impact testing per ASTM E8 and E23 standards, hardness verification using Rockwell C scale, and microstructural examination. Non-destructive testing including ultrasonic inspection ensures internal soundness. Certificates of compliance are provided with detailed test results and traceability documentation.

Processing Recommendations

For optimal formability, maintain processing temperatures below 150°C to prevent tempering effects. Welding requires preheating to 200-300°C and post-weld heat treatment to restore mechanical properties. Machining should utilize carbide tools with appropriate cutting speeds and feeds to manage work hardening characteristics inherent to martensitic steels.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.10 - 0.16
Manganese (Mn)1.40 - 1.80
Silicon (Si)0.15 - 0.50
Phosphorus (P)≤ 0.020
Sulfur (S)≤ 0.010
Chromium (Cr)0.20 - 0.60
Nickel (Ni)0.10 - 0.40
Molybdenum (Mo)0.05 - 0.25
Aluminum (Al)0.020 - 0.080
Titanium (Ti)0.010 - 0.050
Boron (B)0.0005 - 0.0050
Nitrogen (N)≤ 0.008

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Rm)1400 - 1600 MPa
Yield Strength (Rp0.2)≥ 1200 MPa
Elongation (A80)≥ 6%
Reduction of Area (Z)≥ 25%
Hardness (HRC)42 - 48
Impact Energy (KV at 20°C)≥ 25 J
Impact Energy (KV at -40°C)≥ 15 J
Fatigue Limit (107 cycles)600 - 700 MPa
Young's Modulus (E)210 GPa
Poisson's Ratio (ν)0.30
Shear Modulus (G)81 GPa

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)42 W/m·K
Thermal Expansion Coefficient (20-100°C)11.5×10-6/K
Thermal Expansion Coefficient (20-200°C)12.2×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity (20°C)0.18 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity (20°C)11.6×10-6 m²/s

📏 Product Specifications

SpecificationAvailable Options
Product FormsHot rolled sheet, Cold rolled sheet, Plate, Strip, Bar, Tube
Sheet Thickness0.5 - 6.0 mm
Plate Thickness6.0 - 50.0 mm
Width Range600 - 2100 mm
Bar Diameter10 - 300 mm
Surface FinishHot rolled, Cold rolled, Pickled, Oiled, Galvanized
Edge ConditionMill edge, Slit edge, Trimmed edge
Standards ComplianceASTM A514, EN 10025-6, JIS G3106, GB/T 16270
Dimensional Tolerance±0.02 mm (thickness), ±2.0 mm (width)
Flatness Tolerance≤ 2 mm/m
Coil Weight5 - 35 tons
Delivery ConditionQuenched and Tempered (QT)

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing MS 1400

Manufacturing Advantage 1

Advanced Controlled Cooling Technology

MetalZenith employs proprietary controlled cooling systems with precise temperature monitoring and automated quenching processes, ensuring optimal martensitic transformation and consistent mechanical properties throughout the material cross-section for superior performance reliability.

Comprehensive Quality Control Systems

Our integrated quality management system features real-time chemical composition monitoring, automated mechanical testing, and advanced microstructural analysis using scanning electron microscopy, guaranteeing every batch meets stringent international standards and customer specifications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Global Supply Chain

MetalZenith offers tailored heat treatment protocols, precision machining services, and flexible sizing options backed by our global distribution network, ensuring timely delivery of customized MS 1400 solutions to meet specific application requirements worldwide.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo