ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

HSLA 350

HSLA 350

Premium HSLA 350 High Strength Low Alloy Steel

MetalZenith's HSLA 350 represents the pinnacle of high-strength low-alloy steel engineering, delivering exceptional mechanical properties with superior weldability and formability. Our advanced manufacturing processes ensure consistent quality and performance for demanding structural and automotive applications.

MetalZenith Manufacturing Excellence

Our state-of-the-art production facilities utilize controlled rolling and accelerated cooling technologies to achieve optimal microstructure refinement. MetalZenith's proprietary thermomechanical processing ensures precise control of grain size and precipitation hardening, resulting in superior strength-to-weight ratios and enhanced toughness characteristics.

Key Applications & Industries

  • Automotive chassis components and structural reinforcements
  • Construction equipment and heavy machinery frames
  • Bridge construction and infrastructure projects
  • Pressure vessels and storage tank applications
  • Mining equipment and agricultural machinery

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and adheres to ASTM A656, EN 10149, and JIS G3106 standards. Our comprehensive testing protocols include tensile testing, impact testing, hardness verification, and ultrasonic inspection to guarantee material integrity and performance consistency across all product batches.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

HSLA 350 steel features a fine-grained ferrite-pearlite microstructure with controlled precipitation of microalloying elements including vanadium, niobium, and titanium. The thermomechanical controlled processing (TMCP) employed by MetalZenith promotes grain refinement and precipitation strengthening, resulting in enhanced strength without compromising ductility and toughness.

Heat Treatment & Processing

MetalZenith's HSLA 350 is produced through controlled rolling in the austenite recrystallization temperature range (1000-1100°C), followed by accelerated cooling to optimize the final microstructure. The steel is typically supplied in the as-rolled condition and does not require additional heat treatment. Stress relieving can be performed at 580-650°C if required for specific applications.

Manufacturing Process Excellence

Our integrated production process begins with electric arc furnace steelmaking, followed by ladle refining and continuous casting. The hot rolling process utilizes computer-controlled rolling schedules to achieve precise mechanical properties. Advanced process control systems monitor temperature, reduction ratios, and cooling rates to ensure consistent quality throughout production.

Quality Standards & Testing

MetalZenith maintains comprehensive quality assurance protocols including chemical analysis via optical emission spectroscopy, mechanical testing per ASTM standards, ultrasonic testing for internal soundness, and dimensional verification. All products are supplied with certified test reports and full material traceability documentation. Our quality management system complies with ISO 9001:2015, ISO 14001, and OHSAS 18001 standards.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.23
Manganese (Mn)0.90 - 1.65
Silicon (Si)0.15 - 0.50
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Chromium (Cr)≤ 0.50
Nickel (Ni)≤ 0.50
Molybdenum (Mo)≤ 0.35
Copper (Cu)≤ 0.35
Aluminum (Al)0.015 - 0.065
Nitrogen (N)≤ 0.015
Vanadium (V)≤ 0.10
Niobium (Nb)≤ 0.05
Titanium (Ti)≤ 0.15

⚙️ Mechanical Properties

PropertyValue
Minimum Yield Strength350 MPa (51 ksi)
Tensile Strength450 - 590 MPa (65 - 86 ksi)
Elongation (50mm gauge)≥ 20%
Elongation (200mm gauge)≥ 18%
Brinell Hardness (HB)140 - 180
Charpy V-Notch Impact (at 0°C)≥ 27 J (20 ft-lbs)
Charpy V-Notch Impact (at -20°C)≥ 20 J (15 ft-lbs)
Fatigue Limit (107 cycles)180 - 220 MPa
Young's Modulus210 GPa (30.5 Msi)
Poisson's Ratio0.27 - 0.30
Shear Modulus80 GPa (11.6 Msi)
Reduction of Area≥ 50%

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³ (0.284 lb/in³)
Melting Point1510°C (2750°F)
Thermal Conductivity (at 20°C)54 W/m·K (31 BTU/hr·ft·°F)
Thermal Expansion Coefficient (20-100°C)12×10-6/K (6.7×10-6/°F)
Specific Heat Capacity500 J/kg·K (0.12 BTU/lb·°F)
Electrical Resistivity (at 20°C)0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C (1418°F)
Thermal Diffusivity13.8×10-6 m²/s
Emissivity (oxidized surface)0.79
Sound Velocity (longitudinal)5900 m/s
Damping Capacity0.004 - 0.008

📏 Product Specifications

SpecificationAvailable Options
Product FormsHot Rolled Plate, Hot Rolled Sheet, Cold Rolled Sheet, Coil, Strip
Thickness Range1.2 - 100 mm (0.047 - 3.94 in)
Width Range600 - 2500 mm (23.6 - 98.4 in)
Length Range1000 - 12000 mm (39.4 - 472 in)
Coil WeightUp to 35 tons
Surface FinishHot Rolled, Pickled & Oiled, Cold Rolled, Galvanized
Edge ConditionMill Edge, Slit Edge, Trimmed Edge
Thickness Tolerance±0.05 - ±0.50 mm (per ASTM A656)
Width Tolerance±3.0 - ±6.0 mm
Length Tolerance±6.0 - ±25 mm
Flatness≤ 5 mm/m
Standards ComplianceASTM A656, EN 10149-2, JIS G3106, GB/T 16270

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing HSLA 350

Manufacturing Advantage 1

Advanced Thermomechanical Processing

MetalZenith employs cutting-edge controlled rolling and accelerated cooling technologies to achieve optimal microstructure refinement, ensuring superior mechanical properties and consistent grain size distribution throughout the material cross-section.

Comprehensive Quality Control Systems

Our integrated quality management system features real-time monitoring, automated testing protocols, and statistical process control to guarantee material consistency. Every batch undergoes rigorous mechanical testing, chemical analysis, and non-destructive evaluation.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Global Supply

MetalZenith offers extensive customization capabilities including precision cutting, forming, and heat treatment services. Our global distribution network ensures reliable delivery worldwide with full traceability and technical support throughout the supply chain.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo