ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

HY-130 Steel

HY-130 Steel

HY-130 Ultra High Strength Structural Steel

HY-130 is an ultra-high strength, low-alloy structural steel designed for critical applications requiring exceptional strength-to-weight ratios and superior toughness. This quenched and tempered steel grade delivers outstanding performance in demanding structural applications including heavy construction, military vehicles, and high-stress engineering components.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs precision-controlled quenching and tempering processes with advanced vacuum degassing technology to produce HY-130 steel with exceptional mechanical properties and microstructural uniformity. Our state-of-the-art heat treatment facilities ensure optimal strength, toughness, and weldability for critical structural applications.

Key Applications

  • Heavy construction equipment and crane structures
  • Bridge construction and infrastructure projects
  • Military and defense vehicle armor systems
  • High-performance machinery frames and components
  • Pressure vessels and structural supports

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and complete chemical analysis. Our HY-130 steel meets MIL-S-16216 specifications and various international structural standards, ensuring reliability in critical high-strength applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

HY-130 exhibits a tempered martensitic microstructure achieved through controlled quenching and tempering processes. The low-alloy composition with nickel, chromium, and molybdenum additions provides exceptional hardenability and strength while maintaining good toughness. The fine-grained structure ensures uniform mechanical properties throughout the cross-section.

Heat Treatment Process

MetalZenith employs austenitizing at 870-900°C followed by water quenching and tempering at 580-620°C. Our controlled cooling rates and precise temperature monitoring ensure optimal transformation kinetics and mechanical property development. Post-heat treatment stress relief is performed when required for structural applications.

Manufacturing Excellence

Our production process includes vacuum degassing, controlled rolling, and precision heat treatment in computer-controlled furnaces. MetalZenith's advanced manufacturing ensures consistent chemistry, refined grain structure, and superior mechanical properties essential for ultra-high strength structural applications.

Structural Quality Testing

Comprehensive testing includes Charpy V-notch impact testing at various temperatures, fatigue crack growth rate evaluation, weldability testing per AWS D1.1 procedures, and accelerated atmospheric corrosion testing. Our quality assurance ensures reliable performance in critical structural applications.

Engineering Applications

HY-130's exceptional strength-to-weight ratio makes it ideal for weight-critical structural applications. In bridge construction, it enables longer spans with reduced material usage. For machinery manufacturing, it provides superior load-bearing capacity. In vehicle construction, it offers enhanced protection while minimizing weight penalties.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.10 - 0.18
Manganese (Mn)0.60 - 0.90
Silicon (Si)0.15 - 0.35
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.025
Nickel (Ni)2.00 - 3.25
Chromium (Cr)1.00 - 1.80
Molybdenum (Mo)0.20 - 0.60

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 895
Tensile Strength (MPa)965 - 1105
Elongation (%)≥ 16
Impact Energy at -46°C (J)≥ 20
Hardness (HRC)28 - 35
Fatigue Strength (MPa)450 - 500

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.85
Melting Point (°C)1480 - 1520
Thermal Conductivity (W/m·K)42.7
Thermal Expansion (×10??/K)12.3
Elastic Modulus (GPa)200
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Bars, Forgings, Structural Shapes
Thickness Range12 - 150mm
Width Range1200 - 3500mm
Length Range6000 - 15000mm
Standards ComplianceMIL-S-16216, ASTM A514, EN 10025-6
Heat Treatment ConditionQuenched and Tempered
Surface FinishHot Rolled, Pickled, Shot Blasted

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing HY-130 Steel

Manufacturing Advantage 1

Advanced Quench & Temper Processing

MetalZenith utilizes precision-controlled quenching and tempering with real-time temperature monitoring and controlled cooling rates to achieve optimal martensitic transformation and tempering. Our advanced heat treatment ensures consistent ultra-high strength properties while maintaining excellent toughness throughout the material cross-section.

Comprehensive Structural Testing

Our HY-130 steel undergoes extensive testing including Charpy V-notch impact testing, fatigue strength evaluation, weldability assessment using standardized procedures, and atmospheric corrosion resistance testing. MetalZenith ensures superior performance in structural applications through rigorous quality validation.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Structural Solutions

MetalZenith provides tailored processing services including precision cutting, forming, and heat treatment optimization for specific structural applications. Our technical team offers comprehensive engineering support for complex projects requiring ultra-high strength steel solutions.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo