HY-100 High Yield Structural Steel

HY-100 is a high-strength, low-alloy structural steel specifically engineered for demanding applications requiring exceptional strength-to-weight ratios and superior toughness. This quenched and tempered steel grade delivers outstanding mechanical properties for critical structural components in construction, heavy machinery, and high-performance engineering applications.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs precision-controlled quenching and tempering processes with advanced heat treatment technology to produce HY-100 steel with exceptional uniformity and reliability. Our state-of-the-art facilities ensure optimal microstructural development, delivering consistent high-strength properties throughout the material cross-section for superior structural performance.

Key Applications

  • High-rise building structural frameworks and critical load-bearing components
  • Heavy-duty bridge construction and infrastructure projects
  • Mining and construction equipment manufacturing
  • Military and defense vehicle armor applications
  • Pressure vessels and high-stress mechanical components

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and complete chemical analysis. Our HY-100 steel meets ASTM A514/A517 specifications and military standards, ensuring exceptional reliability in critical structural applications requiring maximum strength and durability.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

HY-100 exhibits a tempered martensitic microstructure achieved through controlled quenching and tempering processes. The low-alloy composition with nickel, chromium, and molybdenum additions provides exceptional hardenability and toughness. The fine-grained structure ensures uniform strength distribution and excellent impact resistance, making it ideal for high-stress structural applications requiring superior mechanical properties.

Heat Treatment Process

MetalZenith employs precision austenitizing at 870-900°C followed by controlled water quenching to achieve full martensitic transformation. Subsequent tempering at 580-620°C optimizes the strength-toughness balance while maintaining excellent structural integrity. Our advanced heat treatment facilities ensure uniform temperature distribution and controlled cooling rates for consistent mechanical properties.

Manufacturing Process Excellence

Our manufacturing process begins with electric arc furnace melting followed by ladle refining and vacuum degassing to achieve superior cleanliness. Continuous casting and controlled rolling optimize the microstructure before heat treatment. Advanced process control systems monitor temperature, time, and cooling rates throughout production to ensure consistent quality and performance.

Specialized Quality Testing

MetalZenith conducts comprehensive testing specific to structural applications including: welding performance evaluation using standard procedures, forming capability assessment through bend testing, fatigue strength determination under cyclic loading conditions, and atmospheric corrosion resistance testing in simulated environmental conditions. These specialized tests ensure optimal performance in demanding structural environments.

Structural Application Engineering

For building construction, HY-100's high strength-to-weight ratio enables lighter structural designs while maintaining safety factors. In bridge engineering, excellent fatigue resistance ensures long-term durability under dynamic loading. For machinery manufacturing, superior toughness prevents brittle failure in high-stress components. Vehicle manufacturing benefits from weight reduction without compromising structural integrity. General engineering applications leverage the combination of high strength, good weldability, and reliable performance across temperature ranges.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.12 - 0.18
Manganese (Mn)0.95 - 1.30
Silicon (Si)0.20 - 0.35
Phosphorus (P)≤ 0.015
Sulfur (S)≤ 0.015
Chromium (Cr)0.40 - 0.65
Nickel (Ni)2.00 - 3.50
Molybdenum (Mo)0.15 - 0.25

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 690
Tensile Strength (MPa)760 - 895
Elongation (%)≥ 16
Impact Energy at -40°C (J)≥ 20
Hardness (HB)235 - 285
Fatigue Strength (MPa)345 - 380

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.85
Melting Point (°C)1480 - 1520
Thermal Conductivity (W/m·K)44.5
Thermal Expansion (×10??/K)12.3
Elastic Modulus (GPa)200
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Bars, Structural Shapes, Forgings
Thickness Range6 - 150mm
Width Range1200 - 4500mm
Length Range6000 - 20000mm
Standards ComplianceASTM A514, ASTM A517, MIL-S-16216
Heat Treatment ConditionQuenched and Tempered
Surface FinishHot Rolled, Pickled, Shot Blasted

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing HY-100 Steel

Manufacturing Advantage 1

Precision Quench & Temper Processing

MetalZenith utilizes advanced quenching and tempering technology with precise temperature control and uniform cooling rates to achieve optimal microstructural refinement. Our controlled heat treatment process ensures consistent high-strength properties and superior toughness throughout the material thickness, critical for structural applications.

Comprehensive Structural Testing

Our quality assurance program includes specialized testing for structural applications: advanced welding performance evaluation, forming capability assessment, fatigue strength testing under cyclic loading, and atmospheric corrosion resistance testing. These comprehensive evaluations ensure optimal performance in demanding structural environments.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Structural Solutions

MetalZenith provides tailored processing services including precision cutting, forming, and heat treatment modifications to meet specific structural requirements. Our technical team offers comprehensive engineering support for complex projects, ensuring optimal material selection and processing for each unique application.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo