Technical Specifications
Product Overview
Metallurgical Characteristics
GB Q690 is a low carbon, high strength structural steel featuring a fine-grained microstructure achieved through controlled rolling and accelerated cooling processes. The steel exhibits a predominantly ferritic-bainitic microstructure with dispersed carbide precipitates, providing excellent combination of strength, toughness, and weldability. The controlled addition of microalloying elements such as vanadium, niobium, and titanium enables precipitation strengthening and grain refinement.
Heat Treatment & Processing
MetalZenith employs advanced Thermomechanical Controlled Processing (TMCP) as the primary production route for GB Q690 steel. The process involves controlled rolling at temperatures between 850-950°C followed by accelerated cooling to achieve optimal mechanical properties. Alternative heat treatment options include normalizing at 900-950°C or quenching and tempering with austenitizing at 900-930°C, quenching in water or oil, and tempering at 580-650°C depending on specific application requirements.
Manufacturing Process Excellence
Our manufacturing process begins with careful selection of raw materials and precise charge calculation to achieve target chemistry. Steel is melted in electric arc furnaces with secondary refining through ladle furnace and vacuum degassing to ensure low inclusion content and optimal cleanliness. Continuous casting produces high-quality billets and slabs, which are subsequently processed through our state-of-the-art rolling mills equipped with advanced process control systems for precise temperature and deformation control.
Quality Standards & Certifications
GB Q690 steel manufactured by MetalZenith complies with GB/T 1591-2018 standard and equivalent international specifications including EN 10025-6 S690QL and ASTM A514. Our quality management system is certified to ISO 9001:2015, and we maintain additional certifications including ISO 14001 for environmental management and OHSAS 18001 for occupational health and safety. Each production batch undergoes comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical property verification, ultrasonic testing for internal soundness, and dimensional inspection.
Welding & Fabrication Guidelines
GB Q690 steel exhibits excellent weldability when proper procedures are followed. Preheating to 100-150°C is recommended for sections thicker than 25mm. Low hydrogen welding consumables should be used with interpass temperatures maintained below 250°C. Post-weld heat treatment may be beneficial for stress relief in critical applications. The steel can be readily formed, machined, and fabricated using conventional methods, though higher cutting forces may be required due to its high strength level.
🧪 Chemical Composition
| Element | Content (%) | Purpose |
|---|---|---|
| Carbon (C) | ≤ 0.18 | Strength and hardness |
| Manganese (Mn) | 1.00-1.70 | Strength and hardenability |
| Silicon (Si) | 0.15-0.60 | Deoxidation and strength |
| Phosphorus (P) | ≤ 0.025 | Controlled impurity |
| Sulfur (S) | ≤ 0.015 | Controlled impurity |
| Chromium (Cr) | 0.30-1.50 | Hardenability and strength |
| Nickel (Ni) | 0.30-2.00 | Toughness and strength |
| Molybdenum (Mo) | 0.15-0.70 | Hardenability and creep resistance |
| Vanadium (V) | 0.02-0.12 | Grain refinement |
| Niobium (Nb) | 0.015-0.060 | Precipitation strengthening |
| Titanium (Ti) | 0.006-0.050 | Grain refinement |
| Aluminum (Al) | ≥ 0.015 | Deoxidation and grain refinement |
⚙️ Mechanical Properties
| Property | Value | Test Standard |
|---|---|---|
| Yield Strength (ReL) | ≥ 690 MPa | GB/T 228.1 |
| Tensile Strength (Rm) | 770-940 MPa | GB/T 228.1 |
| Elongation (A50) | ≥ 14% | GB/T 228.1 |
| Impact Energy (KV2) at 20°C | ≥ 47 J | GB/T 229 |
| Impact Energy (KV2) at -20°C | ≥ 34 J | GB/T 229 |
| Impact Energy (KV2) at -40°C | ≥ 27 J | GB/T 229 |
| Brinell Hardness (HBW) | 230-280 | GB/T 231.1 |
| Young's Modulus | 210 GPa | GB/T 22315 |
| Poisson's Ratio | 0.30 | GB/T 22315 |
| Fatigue Limit (10&sup7; cycles) | 350 MPa | GB/T 4337 |
| Fracture Toughness (KIC) | 120 MPa·m1/2 | GB/T 4161 |
| Cold Bend Test (180°) | 3t (t = thickness) | GB/T 232 |
🔬 Physical Properties
| Property | Value | Temperature/Conditions |
|---|---|---|
| Density | 7.85 g/cm³ | 20°C |
| Melting Point | 1510°C | Solidus temperature |
| Thermal Conductivity | 54 W/m·K | 20°C |
| Thermal Expansion Coefficient | 12×10-6/K | 20-100°C |
| Specific Heat Capacity | 500 J/kg·K | 20°C |
| Electrical Resistivity | 0.16 µΩ·m | 20°C |
| Magnetic Permeability | Ferromagnetic | Room temperature |
| Curie Temperature | 770°C | Magnetic transition |
| Thermal Diffusivity | 13.7×10-6 m²/s | 20°C |
| Emissivity | 0.85 | Oxidized surface |
| Sound Velocity (Longitudinal) | 5900 m/s | 20°C |
| Sound Velocity (Transverse) | 3200 m/s | 20°C |
📏 Product Specifications
| Specification | Available Options | Standards |
|---|---|---|
| Product Forms | Plates, Sheets, Bars, Tubes, Forgings, Custom shapes | GB/T 1591, GB/T 3274 |
| Plate Thickness | 8-100 mm | GB/T 3274 |
| Plate Width | 1500-4200 mm | GB/T 3274 |
| Plate Length | 6000-18000 mm | GB/T 3274 |
| Bar Diameter | 16-300 mm | GB/T 702 |
| Tube Outer Diameter | 25-600 mm | GB/T 8162 |
| Tube Wall Thickness | 3-50 mm | GB/T 8162 |
| Surface Finish | Hot rolled, Normalized, Quenched & Tempered, Shot blasted, Pickled | GB/T 1591 |
| Dimensional Tolerance | Class A, B, C per GB standards | GB/T 3274, GB/T 702 |
| Flatness Tolerance | ≤ 5 mm/m | GB/T 3274 |
| Edge Condition | Mill edge, Trimmed edge, Slit edge | GB/T 3274 |
| Delivery Condition | TMCP, N (Normalized), Q+T (Quenched & Tempered) | GB/T 1591 |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing GB Q690
Advanced TMCP Technology
MetalZenith employs cutting-edge Thermomechanical Controlled Processing (TMCP) technology with precise temperature control and optimized rolling schedules to achieve superior grain refinement and enhanced mechanical properties in GB Q690 steel production.
Comprehensive Quality Control
Our integrated quality management system features real-time chemical composition monitoring, automated mechanical testing, and advanced non-destructive testing equipment to ensure every batch of GB Q690 steel meets the highest quality standards with full traceability.
Flexible Customization Capabilities
MetalZenith offers extensive customization options for GB Q690 steel including various product forms, dimensions, surface treatments, and special processing requirements, supported by our global supply chain network and technical engineering services.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
สอบถามด่วน
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications