ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

EN1A Steel

EN1A Steel

EN1A High Quality Structural Steel

EN1A is a premium low carbon structural steel specifically engineered for general engineering and construction applications requiring excellent machinability, weldability, and formability. This normalized mild steel grade offers optimal balance of strength, ductility, and workability for diverse structural applications.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art controlled rolling and normalization processes to produce EN1A steel with superior mechanical properties and exceptional surface quality. Our advanced thermomechanical processing ensures optimal grain refinement and enhanced formability, critical for structural fabrication and machining operations.

Key Applications

  • Building structures and construction frameworks
  • Bridge components and infrastructure projects
  • Mechanical engineering components and machinery parts
  • Automotive chassis and vehicle manufacturing
  • General engineering applications and fabrication

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control throughout production, including dimensional inspection, mechanical testing, and complete chemical analysis. Our EN1A steel meets BS EN 10025, ASTM A36, and other international structural steel standards, ensuring reliability in critical construction and engineering applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN1A is a low carbon structural steel with a predominantly ferritic-pearlitic microstructure. The controlled carbon content and balanced chemistry provide excellent machinability while maintaining adequate strength for structural applications. The fine grain structure achieved through controlled rolling enhances both strength and toughness properties.

Heat Treatment Process

MetalZenith employs controlled hot rolling followed by air cooling or normalization at 850-900°C. This process ensures uniform microstructure and optimal mechanical properties. The controlled cooling rate prevents excessive grain growth while promoting uniform carbide distribution for enhanced machinability.

Manufacturing Excellence

Our advanced manufacturing process includes continuous casting, controlled rolling with precise temperature monitoring, and quality-controlled cooling. MetalZenith's state-of-the-art facilities ensure consistent chemical composition and mechanical properties throughout each production batch.

Structural Performance Testing

EN1A undergoes comprehensive testing including welding performance evaluation using standard procedures, bend testing for formability assessment, rotating beam fatigue testing for structural durability, and salt spray testing for atmospheric corrosion resistance. These tests ensure optimal performance in demanding structural environments.

Application Engineering

For building structures, EN1A provides excellent weldability and formability for complex architectural designs. In bridge engineering, its balanced strength and ductility ensure long-term structural integrity. For mechanical manufacturing, the superior machinability reduces processing costs while maintaining dimensional accuracy. In vehicle manufacturing, the excellent forming characteristics enable complex component fabrication. For general engineering applications, the versatile properties support diverse fabrication requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.15 - 0.25
Manganese (Mn)0.30 - 0.60
Silicon (Si)0.10 - 0.40
Phosphorus (P)≤ 0.050
Sulfur (S)≤ 0.050
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)250 - 280
Tensile Strength (MPa)400 - 550
Elongation (%)≥ 23
Impact Energy at 20°C (J)≥ 27
Hardness (HB)120 - 160
Reduction of Area (%)≥ 40

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.87
Melting Point (°C)1510 - 1540
Thermal Conductivity (W/m·K)50.2
Thermal Expansion (×10??/K)11.8
Elastic Modulus (GPa)200
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Bars, Rods, Tubes, Structural Sections
Thickness Range3 - 150mm
Width Range500 - 3000mm
Length Range3000 - 12000mm
Standards ComplianceBS EN 10025, ASTM A36, DIN 17100
Heat Treatment ConditionHot Rolled, Normalized
Surface FinishMill Scale, Pickled, Shot Blasted

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN1A Steel

Manufacturing Advantage 1

Advanced Controlled Rolling Technology

MetalZenith utilizes precision controlled rolling with optimized temperature profiles to achieve uniform grain structure and enhanced mechanical properties. Our advanced processing ensures consistent strength and excellent formability throughout the material cross-section, ideal for structural fabrication.

Comprehensive Structural Testing

Our EN1A steel undergoes rigorous testing including welding performance evaluation, bend testing for formability, fatigue strength analysis, and atmospheric corrosion resistance testing. This ensures optimal performance in demanding structural applications with superior long-term durability.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Fabrication Services

MetalZenith provides comprehensive custom processing including precision cutting, forming, welding preparation, and surface treatment. Our technical support team offers expert guidance for structural design optimization and fabrication best practices.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo