Technical Specifications
Product Overview
Metallurgical Characteristics
EN S960QL is a fine-grained structural steel produced through controlled rolling followed by quenching and tempering heat treatment. The steel features a tempered martensitic microstructure with fine carbide precipitates, providing exceptional strength while maintaining good toughness and weldability. The low carbon equivalent (CEV ≤ 0.65%) ensures excellent weldability without preheating in most applications.
Heat Treatment Process
MetalZenith employs a precisely controlled quenching and tempering process. The steel is austenitized at 900-950°C, followed by water quenching to achieve a martensitic structure. Subsequent tempering at 580-650°C develops the final mechanical properties while relieving internal stresses. Our computer-controlled furnaces ensure uniform heating and cooling rates throughout the material cross-section.
Manufacturing Process
Production begins with electric arc furnace melting followed by ladle refining and vacuum degassing to achieve ultra-low sulfur and phosphorus contents. Continuous casting produces high-quality billets which undergo controlled rolling in our state-of-the-art rolling mills. The thermomechanical controlled processing (TMCP) refines the grain structure and optimizes mechanical properties.
Quality Standards & Certifications
All EN S960QL products are manufactured in accordance with EN 10025-6 standard and undergo comprehensive testing including chemical analysis, tensile testing, impact testing, and hardness verification. MetalZenith maintains ISO 9001:2015, ISO 14001:2015, and OHSAS 18001 certifications. Each delivery includes complete mill test certificates with full traceability documentation and compliance with CE marking requirements.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | ≤ 0.20 |
| Manganese (Mn) | ≤ 1.70 |
| Silicon (Si) | ≤ 0.80 |
| Phosphorus (P) | ≤ 0.020 |
| Sulfur (S) | ≤ 0.010 |
| Chromium (Cr) | ≤ 1.50 |
| Nickel (Ni) | ≤ 2.00 |
| Molybdenum (Mo) | ≤ 0.70 |
| Vanadium (V) | ≤ 0.12 |
| Niobium (Nb) | ≤ 0.06 |
| Titanium (Ti) | ≤ 0.05 |
| Boron (B) | ≤ 0.005 |
| Aluminum (Al) | ≥ 0.015 |
| Copper (Cu) | ≤ 0.50 |
⚙️ Mechanical Properties
| Property | Value | Test Standard |
|---|---|---|
| Yield Strength (ReH) | ≥ 960 MPa | EN ISO 6892-1 |
| Tensile Strength (Rm) | 980-1150 MPa | EN ISO 6892-1 |
| Elongation (A5) | ≥ 10% | EN ISO 6892-1 |
| Impact Energy (KV) at -40°C | ≥ 30 J | EN ISO 148-1 |
| Brinell Hardness (HBW) | 300-380 | EN ISO 6506-1 |
| Young's Modulus | 210 GPa | EN ISO 6892-1 |
| Poisson's Ratio | 0.30 | ASTM E132 |
| Fatigue Limit (2×106 cycles) | 480 MPa | EN 6072 |
| Reduction of Area (Z) | ≥ 35% | EN ISO 6892-1 |
🔬 Physical Properties
| Property | Value | Temperature Range |
|---|---|---|
| Density | 7.85 g/cm³ | 20°C |
| Melting Point | 1510°C | - |
| Thermal Conductivity | 54 W/m·K | 20°C |
| Specific Heat Capacity | 500 J/kg·K | 20°C |
| Thermal Expansion Coefficient | 12×10-6/K | 20-100°C |
| Electrical Resistivity | 0.16 µΩ·m | 20°C |
| Magnetic Permeability | Ferromagnetic | 20°C |
| Curie Temperature | 770°C | - |
| Thermal Diffusivity | 13.7 mm²/s | 20°C |
📏 Product Specifications
| Specification | Available Options | Standards |
|---|---|---|
| Product Forms | Plates, Sheets, Bars, Profiles, Tubes | EN 10025-6 |
| Plate Thickness | 3-100 mm | EN 10029 |
| Sheet Thickness | 0.5-3 mm | EN 10131 |
| Bar Diameter | 10-300 mm | EN 10060 |
| Width Range | 600-3200 mm | EN 10025-6 |
| Length Range | 2000-18000 mm | Customer Specified |
| Surface Finish | Hot Rolled, Pickled, Shot Blasted | EN 10163 |
| Dimensional Tolerance | Class A, B, C | EN 10029 |
| Edge Condition | Mill Edge, Cut Edge, Slit Edge | EN 10025-6 |
| Heat Treatment | Quenched and Tempered (Q+T) | EN 10025-6 |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing EN S960QL
Advanced Quenching & Tempering Technology
MetalZenith employs precision-controlled quenching and tempering processes with automated temperature monitoring systems, ensuring consistent mechanical properties and optimal grain structure throughout the entire steel section thickness.
Comprehensive Quality Control Laboratory
Our state-of-the-art testing facility features advanced optical emission spectrometers, universal testing machines, and Charpy impact testers, providing complete chemical and mechanical property verification for every production batch.
Custom Processing & Global Supply Chain
MetalZenith offers extensive customization including precision cutting, machining, and surface treatments, backed by our global distribution network ensuring reliable delivery to customers worldwide with full traceability documentation.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
สอบถามด่วน
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications