20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Structure & Processing
DP 780 features a carefully engineered dual phase microstructure consisting of approximately 70-80% ferrite matrix with 20-30% martensite islands. This unique microstructure is achieved through MetalZenith's advanced intercritical annealing process, where the steel is heated to 750-820°C in the two-phase (ferrite + austenite) region, followed by controlled cooling to transform austenite to martensite while retaining the soft ferrite phase.
Manufacturing Process Excellence
MetalZenith employs state-of-the-art continuous annealing technology with precise atmosphere control (N2-H2 mixture) to prevent oxidation and ensure optimal surface quality. The thermal cycle includes rapid heating at 10-15°C/s, precise temperature control within ±5°C during soaking, and controlled cooling rates of 20-50°C/s to achieve the desired martensite fraction. Post-annealing skin-pass rolling (0.5-1.5% reduction) provides excellent surface finish and shape control.
Quality Standards & Testing
All DP 780 production follows ISO/TS 16949 automotive quality management standards with comprehensive testing protocols. Mechanical properties are verified through tensile testing per ASTM E8, hole expansion testing per ISO 16630, and bend testing per VDA 238-100. Microstructural analysis using optical microscopy and EBSD confirms proper phase distribution and grain size. Surface quality inspection includes visual examination, roughness measurement, and coating weight verification for galvanized products.
Application Engineering Support
MetalZenith provides comprehensive technical support including forming simulation using AutoForm and LS-DYNA software, springback prediction, and tooling design recommendations. Our application engineers work closely with customers to optimize part design, forming parameters, and welding procedures. Specialized testing services include formability assessment, crash simulation, and fatigue analysis to ensure optimal performance in automotive applications.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.05 - 0.12 |
| Manganese (Mn) | 1.20 - 2.50 |
| Silicon (Si) | 0.10 - 0.80 |
| Phosphorus (P) | ≤ 0.025 |
| Sulfur (S) | ≤ 0.015 |
| Chromium (Cr) | 0.10 - 0.50 |
| Molybdenum (Mo) | 0.05 - 0.25 |
| Aluminum (Al) | 0.015 - 0.070 |
| Niobium (Nb) | 0.015 - 0.060 |
| Titanium (Ti) | 0.010 - 0.050 |
| Vanadium (V) | 0.01 - 0.10 |
| Boron (B) | 0.0005 - 0.0050 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength (Rm) | 780 - 950 MPa |
| Yield Strength (Rp0.2) | 420 - 580 MPa |
| Elongation (A80) | ≥ 12% |
| Total Elongation (A50) | ≥ 14% |
| Uniform Elongation | ≥ 7% |
| Hardness (HV10) | 240 - 300 |
| Young's Modulus | 210 GPa |
| Poisson's Ratio | 0.30 |
| Hole Expansion Ratio | ≥ 30% |
| Bending Angle (90°) | 1.0t - 2.0t |
| Fatigue Limit (107 cycles) | 280 - 350 MPa |
| Impact Energy (Charpy V, 20°C) | ≥ 80 J |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.85 g/cm³ |
| Melting Point | 1510°C |
| Thermal Conductivity (20°C) | 50 W/m·K |
| Thermal Expansion Coefficient (20-100°C) | 12×10-6/K |
| Specific Heat Capacity | 460 J/kg·K |
| Electrical Resistivity (20°C) | 0.18 µΩ·m |
| Magnetic Permeability | Ferromagnetic |
| Curie Temperature | 770°C |
| Thermal Diffusivity (20°C) | 13.8 mm²/s |
| Emissivity (oxidized surface) | 0.85 |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Cold-rolled sheet, Hot-dip galvanized, Electrogalvanized, Galvannealed |
| Thickness Range | 0.6 - 3.0 mm |
| Width Range | 600 - 2100 mm |
| Coil Weight | 5 - 35 tons |
| Standards | EN 10338, ASTM A1088, JIS G3135, VDA 239-100 |
| Surface Finish | Bright annealed, Matte finish, Skin-passed |
| Thickness Tolerance | ± 0.02 - 0.05 mm |
| Width Tolerance | +0/-3 mm |
| Flatness | ≤ 10 I-units |
| Edge Condition | Mill edge, Trimmed edge |
| Coating Weight (galvanized) | 60 - 275 g/m² |
| Surface Quality | Automotive grade A, B surface |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing DP 780
Advanced Dual Phase Microstructure Control
MetalZenith's proprietary intercritical annealing technology precisely controls the ferrite-martensite microstructure, achieving optimal balance of strength and formability. Our continuous annealing lines feature advanced atmosphere control and rapid cooling systems for consistent dual phase formation.
Comprehensive Automotive Quality Systems
ISO/TS 16949 certified production with real-time process monitoring, advanced metallurgical testing including EBSD analysis, and full statistical process control. Every coil undergoes mechanical testing, surface inspection, and dimensional verification to automotive industry standards.
Global Supply Chain & Technical Support
Worldwide distribution network with local technical support teams providing forming simulation, tooling recommendations, and application engineering. Flexible production capabilities for custom chemistries, surface treatments, and delivery schedules to meet specific automotive program requirements.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
สอบถามด่วน
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications