API 5L X52

API 5L X52

Premium API 5L X52 Pipeline Steel from MetalZenith

API 5L X52, also known as L360 grade pipeline steel, represents MetalZenith's commitment to delivering high-performance carbon steel solutions for critical pipeline infrastructure. This medium-strength line pipe steel is engineered to meet the demanding requirements of oil and gas transportation systems worldwide.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art controlled rolling and accelerated cooling technologies to produce API 5L X52 steel with exceptional mechanical properties and weldability. Our integrated steel production facilities feature advanced electric arc furnaces, continuous casting systems, and precision hot rolling mills that ensure consistent chemical composition and microstructural integrity throughout every batch.

Key Applications and Industries

  • Oil and gas transmission pipelines
  • Natural gas distribution networks
  • Offshore pipeline systems
  • Petrochemical plant piping
  • Water transmission infrastructure

Quality Assurance and Certifications

MetalZenith maintains ISO 9001:2015, API 5L, and ASME certifications, ensuring every API 5L X52 product meets international standards. Our comprehensive testing protocols include chemical analysis, mechanical testing, non-destructive examination, and hydrostatic pressure testing to guarantee superior performance in demanding pipeline applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

API 5L X52 is a low-carbon, high-strength steel with a predominantly ferritic-pearlitic microstructure. The controlled chemical composition, particularly the carbon equivalent (CE) ≤ 0.43%, ensures excellent weldability while maintaining the required mechanical properties. The fine-grained microstructure is achieved through controlled rolling and accelerated cooling processes, resulting in optimal strength-toughness balance.

Heat Treatment and Processing

MetalZenith employs thermomechanical controlled processing (TMCP) for API 5L X52 production. The steel undergoes controlled rolling at temperatures between 850-950°C, followed by accelerated cooling to achieve the desired microstructure. Normalizing heat treatment at 900-950°C may be applied for stress relief and grain refinement. Post-weld heat treatment (PWHT) at 580-650°C is recommended for thick-section welded components.

Manufacturing Process Excellence

Our integrated manufacturing process begins with electric arc furnace steelmaking, utilizing advanced ladle metallurgy for precise chemical composition control. Continuous casting ensures homogeneous structure, followed by hot rolling on state-of-the-art mills with computerized process control. Seamless pipes are produced through rotary piercing and pilger rolling, while welded pipes utilize high-frequency induction welding with 100% seam inspection.

Quality Standards and Compliance

MetalZenith's API 5L X52 steel meets stringent international standards including API 5L PSL1 and PSL2 requirements, NACE MR0175 for sour service applications, and various national standards. Our quality management system encompasses statistical process control, real-time monitoring of critical parameters, and comprehensive testing protocols including chemical analysis, mechanical testing, non-destructive examination, and hydrostatic pressure testing to ensure consistent product quality and reliability.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.26
Manganese (Mn)≤ 1.40
Silicon (Si)≤ 0.45
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Chromium (Cr)≤ 0.30
Nickel (Ni)≤ 0.30
Molybdenum (Mo)≤ 0.15
Copper (Cu)≤ 0.50
Vanadium (V)≤ 0.10
Niobium (Nb)≤ 0.05
Titanium (Ti)≤ 0.04
Aluminum (Al)≤ 0.06
Carbon Equivalent (CE)≤ 0.43

⚙️ Mechanical Properties

PropertyValue
Yield Strength (Rt0.5)360-530 MPa
Tensile Strength (Rm)460-760 MPa
Elongation (A)≥ 22%
Yield to Tensile Ratio≤ 0.93
Hardness (HB)150-250
Impact Energy (CVN at 0°C)≥ 27 J
Impact Energy (CVN at -20°C)≥ 20 J
Fatigue Limit (107 cycles)180-220 MPa
Young's Modulus210 GPa
Poisson's Ratio0.30
Shear Modulus80 GPa
Compression Strength360-530 MPa

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)54 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (20°C)0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity13.8 mm²/s
Emissivity (oxidized surface)0.79
Sound Velocity (longitudinal)5900 m/s
Bulk Modulus160 GPa

📏 Product Specifications

SpecificationAvailable Options
Product FormsSeamless Pipes, Welded Pipes, Plates, Coils, Sheets
Pipe Diameter Range6.35-1422 mm (0.25-56 inches)
Wall Thickness2.11-80 mm (0.083-3.15 inches)
Plate Thickness6-100 mm
Length Range5.8-18.3 m (Random or Fixed Length)
Manufacturing StandardsAPI 5L, ASTM A106, ASME B36.10M, EN 10208
End FinishPlain End, Beveled End, Threaded & Coupled
Surface FinishBlack, Galvanized, 3PE Coated, FBE Coated
Dimensional Tolerance±1% (Diameter), ±12.5% (Wall Thickness)
Testing RequirementsHydrostatic, NDT, Chemical Analysis, Mechanical Testing
CertificationMill Test Certificate, Third Party Inspection
PackagingBundles, Wooden Cases, Steel Frames

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing API 5L X52

Manufacturing Advantage 1

Advanced Controlled Rolling Technology

MetalZenith employs sophisticated controlled rolling and accelerated cooling processes that optimize grain structure and enhance mechanical properties, delivering API 5L X52 steel with superior strength-to-weight ratio and exceptional weldability for critical pipeline applications.

Comprehensive Quality Control Systems

Our integrated quality management system features real-time chemical composition monitoring, automated mechanical testing, and advanced non-destructive examination techniques, ensuring every API 5L X52 product meets stringent API specifications and customer requirements.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain Excellence

MetalZenith's worldwide distribution network and flexible manufacturing capabilities enable rapid delivery of custom API 5L X52 products in various forms including seamless pipes, welded tubes, and plate materials, with tailored dimensions and surface finishes to meet specific project requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo