GB L485

GB L485

GB L485 High-Strength Pipeline Steel

GB L485 is a high-strength low-alloy (HSLA) pipeline steel manufactured according to Chinese national standards, equivalent to API 5L X70 grade. This advanced steel material is specifically designed for high-pressure oil and gas transmission pipelines, offering exceptional strength-to-weight ratio and superior weldability for critical energy infrastructure applications.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith leverages state-of-the-art controlled rolling and accelerated cooling (TMCP) technology to produce GB L485 steel with optimized microstructure and enhanced mechanical properties. Our integrated production facilities feature advanced electric arc furnaces, ladle refining stations, and continuous casting systems, ensuring consistent chemical composition and superior metallurgical quality throughout the manufacturing process.

Key Applications & Industries

  • High-pressure natural gas transmission pipelines
  • Crude oil and refined petroleum product pipelines
  • Offshore pipeline systems and subsea applications
  • Pressure vessels and storage tanks
  • Structural components for energy infrastructure

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control systems including real-time chemical analysis, mechanical testing laboratories, and non-destructive testing capabilities. Our GB L485 steel is manufactured under ISO 9001:2015 quality management systems and complies with international standards including API 5L, ASTM A106, and EN 10208. Each product batch undergoes rigorous testing for chemical composition, mechanical properties, and dimensional accuracy, with full traceability documentation provided to ensure complete quality assurance for our global customers.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

GB L485 is a high-strength low-alloy (HSLA) steel featuring a fine-grained ferrite-pearlite microstructure with controlled precipitation strengthening. The steel achieves its superior mechanical properties through microalloying with niobium, vanadium, and titanium, which form fine carbides and nitrides that provide grain refinement and precipitation hardening. The optimized chemical composition ensures excellent weldability while maintaining high strength and toughness characteristics essential for pipeline applications.

Advanced Manufacturing Process

MetalZenith employs state-of-the-art Thermo-Mechanical Controlled Processing (TMCP) technology for GB L485 production. The process begins with electric arc furnace melting followed by ladle refining for precise chemical composition control. Continuous casting produces high-quality billets with minimal segregation. The controlled rolling process involves reheating to 1200-1250°C, followed by multi-pass rolling with finish rolling temperatures of 780-850°C. Accelerated cooling (ACC) at rates of 5-30°C/s achieves the desired microstructure and mechanical properties without conventional heat treatment.

Heat Treatment & Processing

GB L485 steel is typically supplied in the as-rolled condition after TMCP, eliminating the need for additional heat treatment. For specific applications requiring stress relief, the material can be subjected to controlled heating at 580-620°C. Welding procedures require preheating to 100-150°C for thick sections, with interpass temperatures maintained below 250°C. Post-weld heat treatment is generally not required due to the steel's excellent weldability characteristics and low carbon equivalent.

Quality Standards & Testing

MetalZenith's GB L485 steel production adheres to stringent quality standards including GB/T 9711, API 5L PSL2, and ISO 3183 requirements. Comprehensive testing protocols include chemical analysis using optical emission spectrometry, mechanical testing with universal testing machines, Charpy impact testing at specified temperatures, and non-destructive testing including ultrasonic inspection and magnetic particle testing. Hydrostatic testing ensures pressure integrity, while dimensional inspection verifies compliance with specified tolerances. All products are supplied with complete material traceability documentation and mill test certificates confirming compliance with applicable standards.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.12
Manganese (Mn)1.40 - 1.70
Silicon (Si)0.15 - 0.45
Phosphorus (P)≤ 0.020
Sulfur (S)≤ 0.010
Chromium (Cr)≤ 0.30
Nickel (Ni)≤ 0.30
Molybdenum (Mo)≤ 0.15
Copper (Cu)≤ 0.35
Niobium (Nb)0.02 - 0.08
Vanadium (V)≤ 0.06
Titanium (Ti)≤ 0.04
Aluminum (Al)≥ 0.015
Nitrogen (N)≤ 0.012
Carbon Equivalent (CE)≤ 0.43

⚙️ Mechanical Properties

PropertyValue
Yield Strength (Rp0.2)485 - 635 MPa
Tensile Strength (Rm)570 - 760 MPa
Elongation (A)≥ 18%
Yield to Tensile Ratio≤ 0.85
Impact Energy (Charpy V-notch at 0°C)≥ 41 J
Impact Energy (Charpy V-notch at -20°C)≥ 27 J
Hardness (HV10)200 - 280
Young's Modulus210 GPa
Poisson's Ratio0.30
Fatigue Limit (107 cycles)240 MPa
Fracture Toughness (KIC)150 - 200 MPa·m1/2
Reduction of Area≥ 60%

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (at 20°C)54 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (at 20°C)0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity13.7×10-6 m²/s
Emissivity (oxidized surface)0.85
Sound Velocity (longitudinal)5900 m/s
Coefficient of Linear Expansion (0-100°C)11.5×10-6/K

📏 Product Specifications

SpecificationAvailable Options
Product FormsSeamless Pipes, Welded Pipes, Plates, Sheets, Bars, Forgings
Pipe Outer Diameter21.3 - 1422 mm
Wall Thickness2.0 - 80.0 mm
Plate Thickness6 - 150 mm
Plate Width1500 - 4000 mm
Length6 - 18 m (or as required)
Standards ComplianceGB/T 9711, API 5L, ASTM A106, EN 10208, ISO 3183
Surface FinishBlack, Pickled, Oiled, Galvanized, Epoxy Coated
End PreparationPlain End, Beveled End, Threaded, Flanged
Dimensional Tolerance±0.5% (thickness), ±1.0% (diameter)
Testing RequirementsHydrostatic Test, NDT, Chemical Analysis, Mechanical Testing
CertificationMill Test Certificate, Third Party Inspection, Material Traceability

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing GB L485

Manufacturing Advantage 1

Advanced TMCP Processing Technology

MetalZenith employs cutting-edge Thermo-Mechanical Controlled Processing (TMCP) technology with precise temperature control and accelerated cooling systems. This advanced manufacturing process optimizes grain refinement and precipitation strengthening, delivering GB L485 steel with superior mechanical properties, enhanced toughness, and excellent weldability for demanding pipeline applications.

Comprehensive Quality Control Systems

Our integrated quality assurance program features real-time chemical analysis using advanced spectrometers, automated mechanical testing systems, and comprehensive non-destructive testing capabilities including ultrasonic and magnetic particle inspection. Every batch of GB L485 steel undergoes rigorous testing protocols with full material traceability and certification documentation.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain Excellence

MetalZenith offers flexible customization capabilities for GB L485 steel including various product forms, dimensions, and surface finishes. Our global logistics network ensures reliable delivery worldwide, supported by strategic inventory management and just-in-time delivery services. We provide comprehensive technical support and engineering consultation for project-specific requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo