ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

EH36

EH36

EH36 Marine Steel - Superior Strength for Maritime Applications

EH36 is a high-strength structural steel specifically designed for marine and offshore applications, classified under the higher strength grades of shipbuilding steel. This normalized steel offers exceptional mechanical properties with a minimum yield strength of 355 MPa, making it ideal for critical structural components in harsh marine environments.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art steelmaking technology and precision-controlled rolling processes to produce EH36 steel that consistently exceeds industry standards. Our integrated production facilities feature advanced electric arc furnaces, ladle refining stations, and computer-controlled rolling mills that ensure optimal grain structure and mechanical properties throughout the material.

Key Applications and Industries

  • Ship hulls, decks, and superstructures for commercial vessels
  • Offshore platforms and marine drilling equipment
  • Port infrastructure and harbor construction
  • Heavy-duty structural components in marine environments
  • Shipyard fabrication and repair operations

Quality Assurance and Certification

MetalZenith maintains comprehensive quality control systems with full traceability from raw materials to finished products. Our EH36 steel is certified to major international standards including ABS, DNV-GL, Lloyd's Register, and other leading classification societies, ensuring compliance with the most stringent marine industry requirements.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EH36 marine steel features a fine-grained ferritic-pearlitic microstructure achieved through controlled rolling and normalizing heat treatment. The steel's composition includes microalloying elements such as niobium, vanadium, and titanium, which provide grain refinement and precipitation strengthening. This results in an optimal combination of high strength, excellent toughness, and superior weldability essential for marine structural applications.

Heat Treatment Process

MetalZenith employs a carefully controlled normalizing process where EH36 steel is heated to 900-950°C, held at temperature for uniform austenite formation, then air-cooled to achieve the desired microstructure. This heat treatment ensures consistent mechanical properties throughout the material thickness and eliminates residual stresses from hot rolling. Optional stress relief annealing at 580-650°C may be applied for specific applications requiring dimensional stability.

Manufacturing Process Excellence

Our integrated steelmaking process begins with electric arc furnace melting using premium scrap and direct reduced iron. Secondary refining through ladle metallurgy stations ensures precise chemistry control and inclusion modification. The steel undergoes continuous casting followed by thermomechanical controlled processing (TMCP) with computer-controlled rolling schedules to optimize grain structure and mechanical properties. Advanced ultrasonic testing and automated inspection systems ensure defect-free material delivery.

Quality Standards and Certification

MetalZenith's EH36 steel production adheres to the highest international quality standards including ISO 9001:2015, ISO 14001:2015, and OHSAS 18001. Our quality management system encompasses full material traceability, comprehensive mechanical and chemical testing, non-destructive examination, and third-party verification by major classification societies. Each shipment includes certified mill test certificates with complete test results and compliance documentation for marine industry requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.18
Manganese (Mn)0.90 - 1.60
Silicon (Si)0.10 - 0.50
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.035
Aluminum (Al)≥ 0.015
Niobium (Nb)0.02 - 0.05
Vanadium (V)0.05 - 0.10
Titanium (Ti)0.02 - 0.05
Copper (Cu)≤ 0.35
Chromium (Cr)≤ 0.20
Nickel (Ni)≤ 0.40
Molybdenum (Mo)≤ 0.08

⚙️ Mechanical Properties

PropertyValue
Yield Strength (ReH)≥ 355 MPa
Tensile Strength (Rm)490 - 630 MPa
Elongation (A5)≥ 22%
Impact Energy (KV at 0°C)≥ 34 J
Impact Energy (KV at -20°C)≥ 24 J
Impact Energy (KV at -40°C)≥ 24 J
Brinell Hardness (HB)150 - 220
Young's Modulus210 GPa
Poisson's Ratio0.30
Fatigue Limit (107 cycles)180 MPa
Fracture Toughness (K1C)120 MPa·m1/2

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)54 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (20°C)0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity13.7 mm²/s
Emissivity (oxidized surface)0.79

📏 Product Specifications

SpecificationAvailable Options
Product FormsPlates, Sheets, Bars, Sections, Forgings
Plate Thickness6 - 150 mm
Sheet Thickness1.5 - 6 mm
Width Range1000 - 4000 mm
Length Range2000 - 18000 mm
StandardsABS, DNV-GL, LR, BV, CCS, NK, RINA
Surface FinishHot Rolled, Normalized, Shot Blasted
Edge ConditionMill Edge, Sheared Edge, Flame Cut
Thickness Tolerance± 0.3 mm (t ≤ 40mm), ± 0.05t (t > 40mm)
Width Tolerance± 10 mm
Length Tolerance± 25 mm
Flatness≤ 5 mm/m

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EH36

Manufacturing Advantage 1

Advanced Controlled Rolling Technology

MetalZenith employs precision-controlled thermomechanical rolling processes with real-time temperature monitoring and computer-controlled deformation schedules. This advanced technology ensures optimal grain refinement and uniform mechanical properties throughout the EH36 steel, delivering superior strength-to-weight ratios and enhanced toughness for marine applications.

Comprehensive Marine Certification Program

Our EH36 steel undergoes rigorous testing protocols including Charpy V-notch impact testing at sub-zero temperatures, ultrasonic inspection, and third-party verification by major classification societies. MetalZenith maintains certifications from ABS, DNV-GL, Lloyd's Register, and other leading marine authorities, ensuring full compliance with international shipbuilding standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Flexible Supply Chain and Custom Processing

MetalZenith offers comprehensive supply chain solutions with strategic inventory management, just-in-time delivery, and custom processing services including cutting, machining, and heat treatment. Our global distribution network and flexible production scheduling ensure reliable supply of EH36 steel in various forms and specifications to meet specific project requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo