ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

AH32

AH32

AH32 Marine Steel - Premium Shipbuilding Grade

AH32 is a high-strength marine steel grade specifically designed for shipbuilding and offshore structures. This normalized steel offers exceptional strength, toughness, and weldability, making it ideal for critical marine applications where reliability and performance are paramount.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art controlled rolling and normalizing processes to produce AH32 marine steel that exceeds industry standards. Our advanced thermomechanical processing ensures optimal grain refinement and uniform mechanical properties throughout the material thickness. Our integrated production facilities feature precision temperature control systems and real-time monitoring to guarantee consistent quality in every batch.

Key Applications & Industries

  • Ship hulls and marine vessel construction
  • Offshore platforms and drilling equipment
  • Marine structural components and frameworks
  • Shipyard fabrication and repair operations
  • Coastal infrastructure and port facilities

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control systems with full traceability from raw materials to finished products. Our AH32 steel is certified to major classification societies including ABS, DNV-GL, Lloyd's Register, and BV. Each shipment includes detailed mill test certificates and third-party inspection reports, ensuring complete compliance with international marine standards and customer specifications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

AH32 marine steel features a fine-grained ferritic-pearlitic microstructure achieved through controlled rolling and normalizing heat treatment. The steel's composition is optimized with microalloying elements including niobium, vanadium, and titanium to provide grain refinement and precipitation strengthening. This results in excellent strength-to-weight ratio and superior low-temperature toughness essential for marine applications.

Heat Treatment Process

MetalZenith employs a precise normalizing process where AH32 steel is heated to 900-950°C and air-cooled to achieve optimal mechanical properties. Our controlled cooling systems ensure uniform temperature distribution and consistent grain structure throughout the material thickness. Additional stress relief treatments at 580-620°C may be applied for specific applications requiring enhanced dimensional stability.

Manufacturing Excellence

Our state-of-the-art production facilities utilize advanced thermomechanical controlled processing (TMCP) technology. The manufacturing process includes continuous casting, controlled rolling with precise temperature monitoring, and accelerated cooling systems. Real-time quality monitoring ensures consistent chemical composition and mechanical properties. Each production batch undergoes comprehensive testing including tensile testing, impact testing, and ultrasonic examination.

Quality Standards & Compliance

MetalZenith's AH32 marine steel fully complies with international standards including EN 10225, ASTM A131 Grade AH32, and JIS G3136. Our quality management system is certified to ISO 9001:2015 and ISO 14001:2015. All products are manufactured under strict quality control with full traceability from raw materials to finished products. Third-party inspection and testing services are available through accredited laboratories to ensure complete customer satisfaction and regulatory compliance.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.18
Manganese (Mn)0.90 - 1.60
Silicon (Si)0.10 - 0.50
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.035
Aluminum (Al)≥ 0.015
Niobium (Nb)0.02 - 0.05
Vanadium (V)0.05 - 0.10
Titanium (Ti)0.02 - 0.05
Copper (Cu)≤ 0.35
Chromium (Cr)≤ 0.20
Nickel (Ni)≤ 0.40
Molybdenum (Mo)≤ 0.08

⚙️ Mechanical Properties

PropertyValue
Yield Strength (ReH)≥ 315 MPa
Tensile Strength (Rm)440 - 570 MPa
Elongation (A5)≥ 22%
Impact Energy (KV at 0°C)≥ 34 J
Impact Energy (KV at -20°C)≥ 24 J
Brinell Hardness (HB)150 - 190
Young's Modulus210 GPa
Poisson's Ratio0.30
Fatigue Limit (10&sup7; cycles)220 MPa
Fracture Toughness (KIC)150 MPa·m¹⁄²

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)54 W/m·K
Thermal Expansion (20-100°C)12×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Thermal Diffusivity13.8 mm²/s
Curie Temperature770°C

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Coils, Cut-to-size pieces
Thickness Range6 - 150 mm
Width Range1500 - 4000 mm
Length Range6000 - 18000 mm
StandardsEN 10225, ASTM A131, JIS G3136, GB/T 712
Surface FinishHot Rolled, Shot Blasted, Pickled
Edge ConditionMill Edge, Trimmed Edge, Slit Edge
Thickness Tolerance±0.3 mm (6-40mm), ±0.5 mm (>40mm)
Width Tolerance±5 mm
Length Tolerance±10 mm
Flatness≤5 mm/m
Classification SocietiesABS, DNV-GL, LR, BV, CCS, NK, RINA

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing AH32

Manufacturing Advantage 1

Advanced Thermomechanical Processing

MetalZenith employs cutting-edge controlled rolling and normalizing technology with precise temperature control systems, ensuring optimal grain structure and superior mechanical properties in every AH32 steel plate we produce.

Comprehensive Quality Certification

Our AH32 marine steel is certified by all major classification societies including ABS, DNV-GL, and Lloyd's Register, with complete traceability and third-party testing to guarantee compliance with international marine standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Marine Solutions

MetalZenith offers extensive customization capabilities for AH32 steel including precise dimensional cutting, surface treatments, and specialized heat treatments to meet specific shipbuilding and offshore application requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo