Calculadora de Peso de Ângulo de Aço
Steel Angle Weight Calculator
Calculate the weight of steel angle bars based on dimensions, length, and quantity for construction and fabrication projects.
Weight Results
Angle Dimensions:
-
Cross-Sectional Area:
0 cm²
Weight per Unit Length:
0 kg/m
Single Piece Weight:
0 kg
Total Weight:
0 kg
Total Length:
0 m
Material Density:
0 g/cm³
Imperial Weight:
0 lb
Steel Angle Visualization
Steel Angle Reference
Equal Angle Weight Formula
Weight = (A + B - t) × t × density × length
Where:
A = Length of first leg
B = Length of second leg
t = Thickness
density = Material density
length = Length of angle section
Material Density Reference
| Material | Density (g/cm³) | Density (lb/in³) |
|---|---|---|
| Carbon Steel | 7.85 | 0.284 |
| Mild Steel | 7.75 | 0.280 |
| Stainless Steel 304 | 8.00 | 0.289 |
| Stainless Steel 316 | 8.03 | 0.290 |
| Aluminum | 2.70 | 0.098 |
Common Angle Weights (Carbon Steel)
| Angle Size | Weight (kg/m) | Angle Size | Weight (kg/m) |
|---|---|---|---|
| L 25×25×3 mm | 1.12 | L 50×50×5 mm | 3.77 |
| L 30×30×3 mm | 1.36 | L 60×60×6 mm | 5.42 |
| L 40×40×4 mm | 2.42 | L 75×75×6 mm | 6.85 |
| L 45×45×5 mm | 3.38 | L 100×100×10 mm | 15.0 |