20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
UNS N06022 exhibits a face-centered cubic austenitic structure with exceptional stability across a wide temperature range. The alloy's unique combination of chromium, molybdenum, and tungsten provides outstanding resistance to localized corrosion, including pitting, crevice corrosion, and stress corrosion cracking. MetalZenith's controlled solidification process ensures optimal carbide distribution and grain boundary chemistry.
Heat Treatment Process
Standard solution annealing is performed at 1120°C (2050°F) followed by rapid cooling to prevent carbide precipitation. MetalZenith utilizes precision-controlled atmosphere furnaces with ±5°C temperature uniformity. Post-heat treatment surface conditioning removes oxidation while maintaining dimensional accuracy. Stress relief treatments at 870°C may be applied for welded components.
Manufacturing Process
Production begins with vacuum induction melting of premium raw materials, followed by electroslag remelting for enhanced cleanliness. Hot working operations utilize computer-controlled rolling and forging equipment maintaining precise temperature profiles. Cold working capabilities include precision rolling, drawing, and forming operations with intermediate annealing cycles as required.
Quality Standards & Testing
MetalZenith maintains comprehensive quality systems compliant with ISO 9001:2015, AS9100D, and NADCAP requirements. Testing protocols include chemical analysis via ICP-OES, mechanical property verification, ultrasonic examination, liquid penetrant inspection, and specialized corrosion testing including ASTM G48 and G28 methods. Full material traceability and certification documentation accompany all shipments.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance (56.0 min) |
| Chromium (Cr) | 20.0 - 22.5 |
| Molybdenum (Mo) | 12.5 - 14.5 |
| Tungsten (W) | 2.5 - 3.5 |
| Iron (Fe) | 2.0 - 6.0 |
| Cobalt (Co) | ≤ 2.5 |
| Carbon (C) | ≤ 0.015 |
| Manganese (Mn) | ≤ 0.50 |
| Silicon (Si) | ≤ 0.08 |
| Phosphorus (P) | ≤ 0.02 |
| Sulfur (S) | ≤ 0.010 |
| Vanadium (V) | ≤ 0.35 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength (Room Temperature) | ≥ 690 MPa (100 ksi) |
| Yield Strength (0.2% Offset) | ≥ 310 MPa (45 ksi) |
| Elongation in 50mm | ≥ 45% |
| Hardness (Brinell) | ≤ 223 HB |
| Hardness (Rockwell B) | ≤ 96 HRB |
| Impact Energy (Charpy V-notch) | ≥ 203 J (150 ft-lbs) |
| Fatigue Strength (10&sup7; cycles) | 310 MPa |
| Modulus of Elasticity | 206 GPa (30×10&sup6; psi) |
| Poisson's Ratio | 0.31 |
| Shear Modulus | 81.4 GPa |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 8.69 g/cm³ (0.314 lb/in³) |
| Melting Point | 1370-1400°C (2500-2550°F) |
| Thermal Conductivity (100°C) | 11.1 W/m·K (6.4 Btu/hr·ft·°F) |
| Thermal Expansion (20-100°C) | 12.4×10-6/K (6.9×10-6/°F) |
| Specific Heat Capacity | 394 J/kg·K (0.094 Btu/lb·°F) |
| Electrical Resistivity (20°C) | 1.18 µΩ·m |
| Magnetic Permeability | 1.002 (essentially non-magnetic) |
| Curie Temperature | Not applicable (paramagnetic) |
| Thermal Diffusivity (100°C) | 3.24×10-6 m²/s |
📏 Product Specifications
| Specification | Available Options |
|---|---|
| Product Forms | Plate, Sheet, Strip, Bar, Rod, Wire, Tube, Pipe, Forging |
| Plate Thickness | 6mm - 200mm (0.25' - 8') |
| Sheet Thickness | 0.5mm - 6mm (0.02' - 0.25') |
| Bar Diameter | 6mm - 300mm (0.25' - 12') |
| Tube OD Range | 6mm - 610mm (0.25' - 24') |
| Standards Compliance | ASTM B575, B619, B622, B626, ASME SB-575, EN 2.4602 |
| Surface Finishes | Mill Finish, Pickled, Polished, Ground |
| Dimensional Tolerance | ASTM standard or custom per specification |
| Length Options | Standard lengths or cut-to-size |
| Condition | Solution Annealed (1120°C + Rapid Cool) |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing UNS N06022
Advanced Vacuum Melting Technology
MetalZenith employs state-of-the-art vacuum induction melting (VIM) and electroslag remelting (ESR) processes to produce UNS N06022 with exceptional chemical homogeneity and minimal inclusion content, ensuring superior corrosion resistance and mechanical properties.
Comprehensive Quality Control Systems
Our integrated quality management system features real-time process monitoring, advanced spectroscopic analysis, and comprehensive mechanical testing protocols. Every batch undergoes rigorous corrosion testing and microstructural analysis to guarantee consistent performance.
Custom Processing & Global Supply
MetalZenith offers extensive customization capabilities including specialized heat treatments, precision machining, and custom alloy modifications. Our global distribution network ensures reliable delivery worldwide with full material traceability and certification documentation.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications