Metallurgical Characteristics
SA 414 G is a high-strength low-alloy structural steel with a fine-grained ferritic-pearlitic microstructure. The controlled addition of copper, nickel, and chromium provides enhanced atmospheric corrosion resistance and improved mechanical properties. The optimized carbon content ensures excellent weldability while maintaining high strength characteristics essential for structural applications.
Heat Treatment Process
MetalZenith employs controlled rolling at temperatures between 850-950°C followed by air cooling or normalization at 900-920°C. This process ensures optimal grain refinement and uniform mechanical properties throughout the cross-section. The controlled cooling rate prevents excessive hardening while maintaining the desired strength levels.
Manufacturing Process
Our SA 414 G steel production utilizes electric arc furnace melting with secondary refining processes including ladle metallurgy and vacuum degassing. MetalZenith's continuous casting technology ensures homogeneous chemical composition and minimal segregation, followed by precision hot rolling with computerized process control for consistent mechanical properties.
Structural Quality Testing
Comprehensive testing protocols include welding performance evaluation using standard procedures, forming capability assessment through bend testing, fatigue strength determination under cyclic loading, and atmospheric corrosion resistance testing in simulated environmental conditions. All testing meets ASTM A414 requirements and industry best practices.
Application Engineering Considerations
For building structures, SA 414 G provides excellent strength-to-weight ratios and seismic resistance. In bridge engineering, its superior fatigue resistance and weldability enable complex joint designs. For machinery manufacturing, the material offers reliable performance under dynamic loading. In vehicle construction, it provides crash resistance and structural integrity. General engineering applications benefit from its versatile processing capabilities and consistent quality.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.15 - 0.21 |
| Manganese (Mn) | 0.80 - 1.25 |
| Silicon (Si) | 0.15 - 0.40 |
| Phosphorus (P) | ≤ 0.035 |
| Sulfur (S) | ≤ 0.040 |
| Copper (Cu) | 0.20 - 0.50 |
| Nickel (Ni) | 0.25 - 0.50 |
| Chromium (Cr) | 0.40 - 0.65 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Yield Strength (MPa) | ≥ 350 |
| Tensile Strength (MPa) | 485 - 620 |
| Elongation (%) | ≥ 18 |
| Impact Energy at 0°C (J) | ≥ 27 |
| Hardness (HB) | 140 - 190 |
| Fatigue Strength (MPa) | 160 - 180 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density (g/cm3) | 7.85 |
| Melting Point (°C) | 1510 - 1540 |
| Thermal Conductivity (W/m·K) | 50.2 |
| Thermal Expansion (×10??/K) | 11.8 |
| Elastic Modulus (GPa) | 200 |
| Poisson's Ratio | 0.27 - 0.30 |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Plates, Sheets, Beams, Channels, Angles, Bars |
| Thickness Range | 8 - 150mm |
| Width Range | 1200 - 3500mm |
| Length Range | 6000 - 15000mm |
| Standards Compliance | ASTM A414 Grade G, AISC, AWS D1.1 |
| Heat Treatment Condition | Normalized or As-Rolled |
| Surface Finish | Mill Scale, Shot Blasted, Pickled |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing SA 414 G Steel
Advanced Controlled Rolling Technology
MetalZenith utilizes state-of-the-art controlled rolling processes with precise temperature control and optimized reduction schedules to achieve superior grain refinement in SA 414 G steel. Our advanced thermomechanical processing ensures consistent mechanical properties and enhanced structural integrity throughout the material cross-section.
Comprehensive Structural Performance Testing
Our SA 414 G steel undergoes extensive testing protocols including welding performance evaluation, forming capability assessment, fatigue strength testing, and atmospheric corrosion resistance analysis. MetalZenith's advanced testing facilities ensure optimal performance in demanding structural applications with long-term reliability.
Custom Fabrication and Engineering Support
MetalZenith provides comprehensive custom processing services including precision cutting, forming, and heat treatment tailored to specific structural requirements. Our technical team offers expert consultation on material selection, joint design, and fabrication techniques to optimize performance in building and infrastructure projects.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications