Skip to product information
1 of 1

S55C Carbon Steel

S55C Carbon Steel

S55C High Carbon Structural Steel

S55C is a high carbon structural steel (equivalent to AISI 1055) designed for applications requiring excellent strength, hardness, and wear resistance. This versatile carbon steel grade offers superior mechanical properties through controlled heat treatment, making it ideal for structural components, machinery parts, and automotive applications where high strength and durability are essential.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs precision controlled rolling and advanced heat treatment processes to produce S55C steel with exceptional mechanical properties and microstructural uniformity. Our state-of-the-art quenching and tempering facilities ensure optimal strength-to-toughness balance, while our controlled cooling processes deliver consistent hardness and dimensional stability throughout the material cross-section.

Key Applications

  • Building structural components and reinforcement elements
  • Bridge construction and heavy-duty structural frameworks
  • Machine tool components and industrial machinery parts
  • Automotive axles, gears, and transmission components
  • General engineering applications requiring high strength

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and complete chemical analysis. Our S55C steel meets JIS G4051, ASTM A29, and ISO 683 standards, ensuring reliability in critical structural and mechanical applications with full traceability and certification documentation.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

S55C exhibits a predominantly pearlitic microstructure in the normalized condition, with fine carbide distribution providing excellent strength and hardness. The high carbon content (0.52-0.58%) enables significant strengthening through heat treatment, while controlled manganese content ensures adequate hardenability and improved mechanical properties. The fine-grained structure achieved through controlled rolling enhances both strength and toughness for structural applications.

Heat Treatment Process

MetalZenith employs optimized heat treatment cycles including normalization at 850-900°C followed by air cooling, or quenching and tempering processes with austenitizing at 820-860°C, oil quenching, and tempering at 400-650°C depending on required hardness levels. Our controlled atmosphere furnaces ensure uniform heating and prevent decarburization, maintaining consistent mechanical properties throughout the cross-section.

Advanced Manufacturing Process

Our production process begins with electric arc furnace melting followed by ladle refining to achieve precise chemical composition. Continuous casting and controlled rolling at optimized temperatures ensure fine grain structure and excellent surface quality. MetalZenith's advanced rolling mills maintain tight dimensional tolerances while our heat treatment facilities provide consistent mechanical properties across all product forms.

Specialized Quality Testing

Comprehensive testing protocols include welding performance evaluation using standard welding procedures, forming capability assessment through bend testing and deep drawing trials, fatigue strength testing under rotating beam and axial loading conditions, and atmospheric corrosion resistance testing in salt spray environments. These specialized tests ensure S55C steel meets demanding structural engineering requirements.

Application Engineering Considerations

For building structural applications, S55C provides excellent strength-to-weight ratio and weldability when proper preheating procedures are followed. In bridge engineering, the material's fatigue resistance and atmospheric corrosion properties make it suitable for dynamic loading conditions. For machinery manufacturing, the high hardness capability enables wear-resistant components, while in automotive applications, the material's response to heat treatment allows optimization for specific component requirements in transmission and drivetrain systems.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.52 - 0.58
Manganese (Mn)0.60 - 0.90
Silicon (Si)0.15 - 0.35
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.035
Chromium (Cr)≤ 0.20
Nickel (Ni)≤ 0.20
Copper (Cu)≤ 0.30

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 490
Tensile Strength (MPa)690 - 850
Elongation (%)≥ 16
Impact Energy at 20°C (J)≥ 39
Hardness (HB)201 - 269
Fatigue Strength (MPa)≥ 310

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.85
Melting Point (°C)1460 - 1520
Thermal Conductivity (W/m·K)49.8
Thermal Expansion (×10??/K)12.3
Elastic Modulus (GPa)210
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsRound Bars, Square Bars, Flat Bars, Plates, Forgings
Diameter Range10 - 300mm
Thickness Range5 - 80mm
Length Range3000 - 12000mm
Standards ComplianceJIS G4051, ASTM A29, ISO 683-1
Heat Treatment ConditionAnnealed, Normalized, Q&T
Surface FinishHot Rolled, Cold Drawn, Machined

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing S55C Carbon Steel

Manufacturing Advantage 1

Precision Heat Treatment Processing

MetalZenith utilizes advanced quenching and tempering processes with precise temperature control and controlled cooling rates to achieve optimal mechanical properties in S55C steel. Our sophisticated heat treatment facilities ensure consistent hardness distribution and superior strength-to-toughness balance throughout the material thickness.

Comprehensive Structural Testing

Our quality assurance program includes specialized testing for structural applications: welding performance evaluation, forming capability assessment, fatigue strength testing under cyclic loading, and atmospheric corrosion resistance testing. These comprehensive evaluations ensure S55C steel meets demanding structural engineering requirements.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Engineering Support

MetalZenith provides tailored heat treatment schedules, custom dimensional processing, and comprehensive technical support for S55C applications. Our metallurgical engineers work closely with customers to optimize material properties for specific structural and mechanical requirements, ensuring optimal performance in end-use applications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo