Hot Rolled Steel Wide Flange I Beams are structural steel components known for their strength and durability. They feature a distinctive I-shaped cross-section with wide flanges, providing excellent load-bearing capacity and stability. Ideal for construction and architectural applications, these beams support heavy loads and provide a robust framework for buildings, bridges, and other infrastructure projects. Their hot rolling process enhances their mechanical properties, making them resistant to deformation and adaptable to a variety of environmental conditions.

View full details

Get A Quote

Alloy ASTM Characteristics
A992 / A572-50 / A529-50

Structural support in construction projects such as bridges and buildings.

Framework for industrial structures like factories and warehouses.

Support beams in transportation infrastructure, including railways and highways.

CHEMICAL COMPOSITION

  • The chemical composition of the given material includes Carbon (C) at 0.23%, Manganese (Mn) ranging from 0.5% to 1.6%, Silicon (Si) at 0.4%, Vanadium (V) at 0.15%, Cobalt (Co) at 0.05%, Phosphorus (P) at 0.035%, and Sulfur (S) at 0.045%.

MECHANICAL INFORMATION

  • The material in question boasts a diverse chemical composition predominantly featuring 0.23% Carbon, 0.5% to 1.6% Manganese, 0.4% Silicon, 0.15% Vanadium, 0.05% Cobalt, along with Phosphorus and Sulfur at 0.035% and 0.045% respectively. This composition lends the material notable mechanical attributes, including an ultimate tensile strength of 65,000 psi (448 MPa) and a yield tensile strength of 50,000 psi (345 MPa), with a Brinell hardness measured at 143. Available in various sizes, with weights per foot varying from 9 to 48 pounds, the dimensions feature depth ranges from 4.16 to 8.50 inches, flange widths from 4.060 to 8.110 inches, flange thicknesses from 0.205 to 0.685 inches, and web thicknesses from 0.170 to 0.400 inches, making it suitable for a range of applications. These specifications are approximations and users should contact the Customer Service Department for precise material test reports.

AVAILABLE SIZES

  • The available sizes for this category include a range of specifications as follows: The 4" section is available at 13 lbs and has dimensions of a 4.16" depth, 4.060" flange width, with flange and web thicknesses of .345" and .280" respectively. The 5" section offers two variations, with the 16 lbs option having a depth of 5.01", flange width of 5.000", flange thickness of .360" and web thickness of .240", and the 19 lbs option with a 5.15" depth, 5.030" flange width, .430" flange thickness, and .270" web thickness. The 6" section spans multiple configurations, from 9 lbs with a 5.90" depth, 3.940" flange width, .215" flange thickness, and .170" web thickness, to options such as 12 lbs with a 6.03" depth, 4.000" flange width, .280" flange thickness, and .230" web thickness, and even up to 25 lbs with a depth of 6.38", 6.080" flange width, .455" flange thickness, and .320" web thickness. Moving to the 8" category, the range starts from 10 lbs, with an available dimension of 7.89" depth, 3.940" flange width, .205" flange thickness, and .170" web thickness, moving up through offerings such as 18 lbs with an 8.14" depth, 5.250" flange width, .330" flange thickness, and .230" web thickness, with the heftiest 48 lbs option featuring an 8.50" depth, 8.110" flange width, significant .685" flange thickness, and .400" web thickness.