Premium GB 9Cr18Mo Stainless Bearing Steel

GB 9Cr18Mo is a high-carbon martensitic stainless steel equivalent to AISI 440C, renowned for its exceptional hardness, wear resistance, and corrosion resistance. This premium bearing steel combines high carbon content with chromium and molybdenum additions to deliver superior performance in demanding applications requiring both mechanical strength and environmental resistance.

MetalZenith's Advanced Manufacturing Excellence

As a leading steel manufacturer, MetalZenith employs state-of-the-art vacuum induction melting and electroslag remelting technologies to produce GB 9Cr18Mo with exceptional purity and homogeneity. Our advanced heat treatment facilities ensure precise microstructural control, delivering consistent mechanical properties and dimensional stability across all product forms.

Key Applications & Industries

  • Precision ball and roller bearings for aerospace and automotive applications
  • Surgical instruments and medical devices requiring biocompatibility
  • Cutting tools, knives, and razor blades for industrial applications
  • Valve components and pump parts in corrosive environments
  • Measuring instruments and precision gauges

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control throughout production. Our in-house testing laboratory performs chemical analysis, mechanical testing, and metallographic examination to ensure compliance with GB/T 1220 and international standards. Each shipment includes detailed mill test certificates and traceability documentation.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

GB 9Cr18Mo is a high-carbon martensitic stainless steel with excellent hardenability due to its balanced chromium and molybdenum content. The steel exhibits a fully martensitic structure after hardening, providing exceptional wear resistance and dimensional stability. The molybdenum addition enhances corrosion resistance and improves hardenability, while maintaining good machinability in the annealed condition.

Heat Treatment Process

MetalZenith employs precise heat treatment protocols to optimize GB 9Cr18Mo performance. Annealing is performed at 840-880°C followed by slow cooling to achieve maximum machinability. Hardening involves heating to 1010-1050°C with oil or air quenching, followed by tempering at 150-200°C to achieve target hardness of 58-62 HRC. Stress relieving at 650-700°C may be applied to minimize residual stresses.

Manufacturing Process Excellence

Our manufacturing process begins with vacuum induction melting using premium raw materials to ensure chemical homogeneity and minimize inclusions. Electroslag remelting further refines the steel structure, followed by hot forging and rolling operations under controlled conditions. Cold working processes including drawing, rolling, and machining are performed using advanced equipment to maintain tight dimensional tolerances and superior surface quality.

Quality Standards & Testing

MetalZenith maintains compliance with GB/T 1220, ASTM A276, and EN 10088 standards. Comprehensive testing includes chemical analysis by optical emission spectroscopy, mechanical property verification through tensile and hardness testing, and microstructural examination using metallographic techniques. Non-destructive testing methods including ultrasonic inspection and magnetic particle testing ensure internal soundness. Each production lot undergoes statistical process control monitoring to guarantee consistent quality and performance characteristics.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.85-1.00
Silicon (Si)≤ 0.80
Manganese (Mn)≤ 0.80
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.030
Chromium (Cr)17.0-19.0
Molybdenum (Mo)0.40-0.80
Nickel (Ni)≤ 0.60
Copper (Cu)≤ 0.30
Vanadium (V)≤ 0.15

⚙️ Mechanical Properties

PropertyValueCondition
Tensile Strength≥ 1960 MPaHardened & Tempered
Yield Strength (0.2%)≥ 1570 MPaHardened & Tempered
Elongation≥ 8%Hardened & Tempered
Reduction of Area≥ 25%Hardened & Tempered
Hardness (HRC)58-62Hardened & Tempered
Impact Energy (KV)≥ 15 JRoom Temperature
Fatigue Limit850 MPa10&sup7; cycles
Young's Modulus200 GPaRoom Temperature
Poisson's Ratio0.27-0.30Room Temperature

🔬 Physical Properties

PropertyValueTemperature
Density7.75 g/cm³20°C
Melting Point1480-1530°C-
Thermal Conductivity24.2 W/m·K20°C
Thermal Expansion Coefficient10.4×10-6/K20-100°C
Specific Heat Capacity460 J/kg·K20°C
Electrical Resistivity0.60 µΩ·m20°C
Magnetic PermeabilityFerromagneticHardened
Curie Temperature760°C-
Thermal Diffusivity6.8×10-6 m²/s20°C

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsRound bars, flat bars, plates, sheets, strips, wire, forgingsGB/T 1220, ASTM A276
Round Bar Diameter6-300 mmHot rolled, cold drawn
Flat Bar Dimensions10-100 mm thickness, up to 300 mm widthHot rolled, machined
Plate Thickness6-80 mmHot rolled, annealed
Sheet Thickness0.5-6.0 mmCold rolled, annealed
Wire Diameter0.1-10 mmCold drawn, annealed
Surface FinishBlack, pickled, ground, polished, bright annealedRa 0.1-3.2 µm
Length3-12 meters (standard), custom lengths availableFixed or random
Dimensional Toleranceh9-h11 (bars), ±0.1-0.5 mm (plates/sheets)ISO 2768, GB/T 1804
Heat Treatment ConditionAnnealed, hardened & tempered, solution treatedCustomer specified

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing GB 9Cr18Mo

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes vacuum induction melting (VIM) and electroslag remelting (ESR) processes to achieve ultra-low inclusion content and superior chemical homogeneity in GB 9Cr18Mo production, ensuring consistent performance and extended service life.

Precision Heat Treatment Control

Our computer-controlled heat treatment facilities provide precise temperature and atmosphere control during hardening and tempering processes, delivering optimal microstructure and mechanical properties with minimal distortion and excellent dimensional stability.

Manufacturing Advantage 2
Manufacturing Advantage 3

Comprehensive Customization Capabilities

MetalZenith offers extensive customization options including special dimensions, surface finishes, and heat treatment conditions. Our technical team provides application-specific solutions with rapid prototyping and flexible order quantities to meet diverse customer requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo