Skip to product information
1 of 1

GB 20CrNiMo

GB 20CrNiMo

Premium GB 20CrNiMo Alloy Steel from MetalZenith

GB 20CrNiMo is a high-performance low-alloy steel featuring chromium, nickel, and molybdenum additions that provide exceptional strength, toughness, and hardenability. This versatile alloy steel is designed for demanding applications requiring superior mechanical properties and reliability under extreme conditions.

MetalZenith's Advanced Manufacturing Excellence

As a leading steel manufacturer, MetalZenith employs state-of-the-art electric arc furnace technology and advanced secondary refining processes to produce GB 20CrNiMo with exceptional chemical homogeneity and cleanliness. Our precision-controlled heat treatment facilities ensure optimal microstructure development and consistent mechanical properties throughout each production batch.

Key Applications & Industries

  • Heavy machinery components requiring high strength and impact resistance
  • Automotive transmission gears, crankshafts, and connecting rods
  • Construction equipment parts subjected to dynamic loading
  • Mining and drilling equipment components
  • Industrial machinery shafts and structural elements

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control protocols including spectroscopic analysis, mechanical testing, and non-destructive examination. Every batch undergoes rigorous testing to ensure compliance with GB standards and customer specifications, backed by our complete traceability system and technical documentation.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

GB 20CrNiMo is a low-alloy steel with excellent hardenability due to its balanced chromium, nickel, and molybdenum content. The microstructure typically consists of tempered martensite or bainite after proper heat treatment, providing optimal strength-toughness combination. The nickel content enhances toughness and impact resistance, while chromium improves hardenability and wear resistance. Molybdenum additions prevent temper brittleness and enhance high-temperature strength.

Heat Treatment Process

MetalZenith employs controlled heat treatment cycles optimized for GB 20CrNiMo. Austenitizing is performed at 850-880°C followed by oil quenching to achieve martensitic transformation. Tempering at 550-650°C develops the desired strength-toughness balance. Our computer-controlled furnaces ensure uniform heating, precise temperature control, and consistent cooling rates throughout the cross-section.

Manufacturing Process Excellence

Production begins with electric arc furnace melting using high-quality raw materials, followed by ladle refining and vacuum degassing to achieve superior cleanliness. Continuous casting produces homogeneous billets with minimal segregation. Hot rolling or forging operations are performed within controlled temperature ranges to optimize grain structure and mechanical properties.

Quality Standards & Testing

All GB 20CrNiMo products undergo comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical property verification through tensile and impact testing, hardness measurement, and ultrasonic examination for internal soundness. Grain size analysis and microstructural evaluation ensure conformance to specifications. Complete mill test certificates accompany each shipment with full traceability documentation.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.17-0.23
Silicon (Si)0.17-0.37
Manganese (Mn)0.40-0.70
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.035
Chromium (Cr)0.40-0.70
Nickel (Ni)1.25-1.65
Molybdenum (Mo)0.20-0.30
Copper (Cu)≤ 0.25
Aluminum (Al)≥ 0.015

⚙️ Mechanical Properties

PropertyValueCondition
Tensile Strength980-1180 MPaQuenched & Tempered
Yield Strength (0.2% offset)≥ 785 MPaQuenched & Tempered
Elongation≥ 12%50mm gauge length
Reduction of Area≥ 45%Standard test
Hardness (HB)293-352Quenched & Tempered
Impact Energy (KV)≥ 39 JRoom temperature
Fatigue Limit450-500 MPa10&sup7; cycles
Young's Modulus210 GPaRoom temperature

🔬 Physical Properties

PropertyValueTemperature
Density7.85 g/cm³20°C
Melting Point1480-1520°C-
Thermal Conductivity42 W/m·K20°C
Thermal Expansion Coefficient12.5×10-6/K20-100°C
Specific Heat Capacity460 J/kg·K20°C
Electrical Resistivity0.25 µΩ·m20°C
Magnetic PermeabilityFerromagneticRoom temperature
Curie Temperature770°C-

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsRound bars, square bars, flat bars, plates, sheets, tubes, forgingsGB/T 3077
Round Bar Diameter10-500mmGB/T 702
Plate Thickness6-200mmGB/T 709
LengthUp to 12m (standard), custom lengths availableCustomer specification
Surface FinishHot rolled, cold drawn, peeled, ground, machinedGB/T 3077
Dimensional Toleranceh9, h11 (bars), ±0.5mm (plates)GB/T 702, GB/T 709
Heat Treatment ConditionAnnealed, normalized, quenched & temperedCustomer requirement
Testing StandardsGB/T 228, GB/T 229, GB/T 231National standards

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing GB 20CrNiMo

Manufacturing Advantage 1

Advanced Vacuum Degassing Technology

MetalZenith utilizes state-of-the-art vacuum degassing and ladle refining systems to achieve ultra-low sulfur and phosphorus content in GB 20CrNiMo, resulting in superior cleanliness, improved fatigue resistance, and enhanced mechanical properties that exceed standard specifications.

Precision Heat Treatment Control

Our computer-controlled heat treatment facilities feature precise temperature monitoring and atmosphere control, ensuring optimal austenitizing, quenching, and tempering cycles that deliver consistent microstructure and mechanical properties with minimal variation across production batches.

Manufacturing Advantage 2
Manufacturing Advantage 3

Comprehensive Customization Capabilities

MetalZenith offers extensive customization options including specific chemical compositions, specialized heat treatments, precision machining, and various surface finishes. Our technical team works closely with customers to develop tailored solutions meeting exact application requirements and performance specifications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo