Skip to product information
1 of 1

EN S700MC

EN S700MC

High-Strength Cold Forming Steel EN S700MC

EN S700MC is a high-strength, low-alloy structural steel specifically designed for cold forming applications. This thermomechanically rolled steel grade offers exceptional strength-to-weight ratio and excellent formability, making it ideal for demanding structural applications where weight reduction and superior mechanical properties are critical.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art thermomechanical controlled processing (TMCP) technology to produce EN S700MC steel with superior consistency and performance. Our advanced rolling mills and precise temperature control systems ensure optimal microstructure development, delivering steel with enhanced strength, toughness, and formability characteristics that exceed industry standards.

Key Applications and Industries

  • Automotive chassis components and safety structures
  • Construction machinery and heavy equipment frames
  • Mobile crane booms and lifting equipment
  • Transportation vehicle bodies and trailers
  • Agricultural machinery and earth-moving equipment

Quality Assurance and Certification

MetalZenith maintains comprehensive quality control throughout the entire production process, from raw material selection to final product delivery. Our EN S700MC steel is manufactured in accordance with EN 10149-2 standards and certified to ISO 9001:2015, ISO 14001:2015, and OHSAS 18001 management systems, ensuring consistent quality and reliability for critical applications.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN S700MC is a high-strength, low-alloy (HSLA) structural steel produced through thermomechanical controlled processing (TMCP). The steel features a fine-grained ferrite-pearlite microstructure with possible bainitic constituents, achieved through controlled rolling and accelerated cooling. The optimized chemical composition with microalloying elements such as niobium, vanadium, and titanium provides excellent grain refinement and precipitation strengthening.

Manufacturing Process

MetalZenith employs advanced thermomechanical controlled processing technology to manufacture EN S700MC steel. The process begins with careful selection of raw materials followed by electric arc furnace melting and secondary refining. The steel undergoes controlled rolling in the austenite recrystallization and non-recrystallization temperature ranges, followed by accelerated cooling to achieve the desired microstructure and mechanical properties. This process ensures superior strength, toughness, and formability characteristics.

Heat Treatment and Processing

EN S700MC is supplied in the thermomechanically rolled condition and does not require additional heat treatment. The steel exhibits excellent cold forming properties and can be welded using conventional welding processes. Preheating may be required for thick sections or when welding in cold conditions. Post-weld heat treatment is generally not necessary for most applications, maintaining the steel's as-delivered properties.

Quality Standards and Certification

All EN S700MC steel produced by MetalZenith complies with EN 10149-2 standards and is manufactured under ISO 9001:2015 quality management system. Each batch undergoes comprehensive testing including chemical analysis, tensile testing, impact testing, and dimensional inspection. Mill test certificates (EN 10204 Type 3.1) are provided with full traceability documentation. Additional third-party inspection and certification services are available upon request.

Welding and Fabrication Guidelines

EN S700MC exhibits good weldability with proper welding procedures. Carbon equivalent values are controlled to ensure excellent weldability. Recommended welding processes include GMAW, GTAW, SAW, and FCAW. Preheat temperatures of 50-150°C may be required depending on thickness and ambient conditions. The steel maintains its strength characteristics in the heat-affected zone when proper welding parameters are employed.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.12
Manganese (Mn)≤ 2.10
Silicon (Si)≤ 0.60
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.015
Aluminum (Al)≥ 0.015
Chromium (Cr)≤ 1.50
Nickel (Ni)≤ 2.00
Molybdenum (Mo)≤ 0.70
Copper (Cu)≤ 0.50
Niobium (Nb)≤ 0.09
Vanadium (V)≤ 0.20
Titanium (Ti)≤ 0.15
Boron (B)≤ 0.005
Nitrogen (N)≤ 0.015

⚙️ Mechanical Properties

PropertyValue
Yield Strength (ReH)700-850 MPa
Tensile Strength (Rm)750-950 MPa
Elongation (A80)≥ 12%
Elongation (A5)≥ 14%
Impact Energy (KV) at -20°C≥ 30 J
Impact Energy (KV) at -40°C≥ 25 J
Brinell Hardness (HB)230-280
Young's Modulus210 GPa
Poisson's Ratio0.30
Fatigue Limit (10&sup7; cycles)350-400 MPa
Bend Test (180°)3t minimum radius
Reduction of Area≥ 50%

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)52 W/m·K
Thermal Expansion Coefficient (20-100°C)12.5×10-6/K
Thermal Expansion Coefficient (20-200°C)13.0×10-6/K
Thermal Expansion Coefficient (20-400°C)13.8×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity (20°C)0.18 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity (20°C)14.4 mm²/s
Emissivity (oxidized surface)0.79

📏 Product Specifications

SpecificationDetails
Available FormsHot rolled plates, sheets, strips, coils
Thickness Range3.0-100.0 mm
Width Range1000-3200 mm
Length Range6000-18000 mm
Coil WeightUp to 35 tons
Standards ComplianceEN 10149-2, EN 10025
Surface FinishHot rolled, pickled, oiled
Edge ConditionMill edge, trimmed edge
Thickness Tolerance±0.3 mm (t ≤ 20mm), ±1.5% (t > 20mm)
Width Tolerance+0/-5 mm
Length Tolerance+50/-0 mm
Flatness≤ 5 mm/m
Delivery ConditionThermomechanically rolled (M)
Testing StandardsEN 10002-1, EN 10045-1, EN 10204

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN S700MC

Manufacturing Advantage 1

Advanced Thermomechanical Processing

MetalZenith employs cutting-edge TMCP technology with precise temperature control and optimized rolling schedules to achieve superior grain refinement and enhanced mechanical properties in EN S700MC steel, ensuring consistent quality and performance.

Comprehensive Quality Testing

Our state-of-the-art testing laboratory conducts extensive mechanical, chemical, and metallurgical analysis on every batch of EN S700MC steel, including tensile testing, impact testing, and microstructure examination to guarantee compliance with EN 10149-2 standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing and Global Supply

MetalZenith offers extensive customization capabilities including precision cutting, forming, and surface treatment services for EN S700MC steel, supported by our global distribution network ensuring timely delivery worldwide with full traceability documentation.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo