Technical Specifications
Product Overview
Metallurgical Characteristics
CP 600 complex phase steel features a sophisticated microstructure consisting of ferrite, bainite, and small amounts of retained austenite and martensite. This multi-phase composition is achieved through carefully controlled thermomechanical processing, where precise cooling rates and temperature control during hot rolling create the desired phase distribution. The fine-grained microstructure provides excellent strength while maintaining superior formability compared to conventional high-strength steels.
Manufacturing Process
MetalZenith's production process begins with vacuum degassed steel melting to ensure ultra-low inclusion content and precise chemical composition control. The steel undergoes controlled hot rolling with specific finishing temperatures, followed by accelerated cooling on the run-out table. For cold-rolled variants, the material receives controlled annealing in continuous annealing lines with precise temperature profiles to optimize the complex phase microstructure. Advanced process control systems monitor critical parameters throughout production to ensure consistent quality.
Heat Treatment Considerations
CP 600 steel is supplied in the final heat-treated condition and typically does not require additional heat treatment. However, for specific applications requiring stress relief, heating to 150-200°C for 1-2 hours is recommended. Welding operations should utilize low-heat input techniques with preheating to 100-150°C for thick sections. Post-weld heat treatment at 580-620°C may be beneficial for critical applications to optimize the heat-affected zone properties.
Quality Standards & Testing
All CP 600 production adheres to international standards including EN 10338, ASTM A1088, and JIS G3135. MetalZenith's quality assurance program includes continuous monitoring of chemical composition via optical emission spectroscopy, mechanical property verification through automated tensile testing, and microstructural analysis using advanced metallographic techniques. Each coil receives comprehensive certification documenting chemical analysis, mechanical properties, and dimensional compliance. Traceability systems ensure complete product history from raw materials through final delivery.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.05 - 0.12 |
| Manganese (Mn) | 1.20 - 2.00 |
| Silicon (Si) | 0.10 - 0.50 |
| Phosphorus (P) | ≤ 0.025 |
| Sulfur (S) | ≤ 0.015 |
| Chromium (Cr) | 0.20 - 0.80 |
| Molybdenum (Mo) | 0.05 - 0.25 |
| Vanadium (V) | 0.01 - 0.10 |
| Niobium (Nb) | 0.01 - 0.05 |
| Titanium (Ti) | 0.01 - 0.05 |
| Aluminum (Al) | 0.015 - 0.070 |
| Boron (B) | 0.0005 - 0.0050 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength (Rm) | 600 - 750 MPa |
| Yield Strength (Rp0.2) | 350 - 450 MPa |
| Elongation (A80) | ≥ 18% |
| Total Elongation (At) | ≥ 20% |
| Uniform Elongation (Ag) | ≥ 12% |
| Hardness (HV10) | 180 - 220 |
| Young's Modulus (E) | 210 GPa |
| Impact Energy (Charpy V, 20°C) | ≥ 40 J |
| Fatigue Limit (107 cycles) | 280 MPa |
| Bend Radius (90°) | 1.5t - 2.0t |
| Hole Expansion Ratio (λ) | ≥ 40% |
| n-value (Strain Hardening Exponent) | 0.12 - 0.16 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.85 g/cm³ |
| Melting Point | 1510°C |
| Thermal Conductivity (20°C) | 52 W/m·K |
| Thermal Expansion Coefficient (20-100°C) | 12.5×10-6/K |
| Specific Heat Capacity | 460 J/kg·K |
| Electrical Resistivity (20°C) | 0.18 µΩ·m |
| Magnetic Permeability | Ferromagnetic |
| Curie Temperature | 770°C |
| Thermal Diffusivity (20°C) | 14.4 mm²/s |
| Poisson's Ratio | 0.27 - 0.30 |
| Coefficient of Thermal Expansion (20-200°C) | 13.2×10-6/K |
| Emissivity (Oxidized Surface) | 0.85 - 0.95 |
📏 Product Specifications
| Specification | Available Options |
|---|---|
| Product Forms | Hot Rolled Coil, Cold Rolled Coil, Sheet, Strip |
| Thickness Range | 0.8 - 8.0 mm |
| Width Range | 600 - 2100 mm |
| Coil Weight | 5 - 35 tons |
| Thickness Tolerance | ±0.02 - ±0.05 mm |
| Width Tolerance | ±2.0 mm |
| Surface Finish | Hot Rolled Pickled, Cold Rolled, Oiled, Dry |
| Edge Condition | Mill Edge, Trimmed Edge |
| Flatness | ≤ 10 I-units |
| Standards Compliance | EN 10338, ASTM A1088, JIS G3135 |
| Coating Options | Galvanized (GI), Galvannealed (GA), Organic Coated |
| Packaging | Coil, Cut-to-Length Sheets, Slit Strips |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing CP 600
Advanced Thermomechanical Processing
MetalZenith employs cutting-edge controlled cooling technology and precise temperature management during production to achieve the optimal complex microstructure. Our proprietary processing parameters ensure consistent grain refinement and uniform phase distribution, delivering superior mechanical properties and enhanced formability compared to conventional production methods.
Comprehensive Quality Control Systems
Our integrated quality management system features real-time monitoring of chemical composition, continuous mechanical property testing, and advanced microstructural analysis using scanning electron microscopy. Every coil undergoes rigorous inspection protocols including tensile testing, hardness verification, and dimensional accuracy checks to guarantee consistent performance.
Flexible Customization & Supply Solutions
MetalZenith offers extensive customization capabilities including specific thickness tolerances, surface finish options, and tailored mechanical properties to meet unique application requirements. Our global supply chain network ensures reliable delivery schedules, while our technical support team provides comprehensive engineering assistance for optimal material selection and processing recommendations.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications