API 5L X60, also known as L415 grade steel, is a high-strength low-alloy (HSLA) pipeline steel specifically engineered for oil and gas transmission systems. MetalZenith manufactures this critical infrastructure steel using advanced controlled rolling and accelerated cooling technologies, ensuring superior mechanical properties and excellent weldability for demanding pipeline applications.

MetalZenith's Manufacturing Excellence

Our state-of-the-art production facilities utilize thermomechanical controlled processing (TMCP) and precise chemical composition control to produce API 5L X60 steel that consistently exceeds industry standards. Our advanced rolling mills and heat treatment systems ensure uniform microstructure and optimal grain refinement, delivering exceptional toughness and strength properties.

Key Applications & Industries

  • High-pressure oil and gas transmission pipelines
  • Offshore pipeline systems and subsea applications
  • Natural gas distribution networks
  • Petrochemical plant piping systems
  • Cross-country pipeline infrastructure

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control throughout the manufacturing process, including chemical analysis, mechanical testing, non-destructive testing, and dimensional verification. Our API 5L X60 steel is certified to international standards including API 5L, ISO 3183, and ASTM A1018, with full traceability documentation and third-party inspection available.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

API 5L X60 steel features a fine-grained ferrite-pearlite microstructure achieved through controlled rolling and accelerated cooling processes. The optimized chemical composition with microalloying elements such as niobium and vanadium provides excellent strength-toughness balance and superior weldability. The steel exhibits excellent resistance to hydrogen-induced cracking (HIC) and sulfide stress cracking (SSC) in sour service environments.

Manufacturing Process

MetalZenith produces API 5L X60 steel through advanced steelmaking processes including electric arc furnace (EAF) melting, ladle refining, and continuous casting. The hot rolling process utilizes thermomechanical controlled processing (TMCP) with precise temperature control during rolling and accelerated cooling to achieve optimal mechanical properties. Seamless pipes are manufactured using rotary piercing and pilger rolling, while welded pipes employ high-frequency electric resistance welding (HFW) or submerged arc welding (SAW).

Heat Treatment & Processing

The steel is typically supplied in the as-rolled or normalized condition, depending on specific requirements. Stress relieving heat treatment at 580-650°C may be applied to reduce residual stresses. For specialized applications, quenching and tempering processes can be employed to achieve enhanced mechanical properties. Post-weld heat treatment (PWHT) guidelines are provided for field welding operations.

Quality Standards & Testing

All API 5L X60 steel products undergo comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical testing per ASTM A370, non-destructive testing (ultrasonic, magnetic particle, dye penetrant), dimensional inspection, and hydrostatic pressure testing. Products are certified to API 5L PSL1 and PSL2 requirements, with full material traceability and third-party inspection available. Advanced testing capabilities include CTOD fracture toughness testing, fatigue testing, and corrosion resistance evaluation.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.28
Manganese (Mn)≤ 1.40
Silicon (Si)≤ 0.45
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Chromium (Cr)≤ 0.30
Nickel (Ni)≤ 0.30
Molybdenum (Mo)≤ 0.15
Copper (Cu)≤ 0.50
Vanadium (V)≤ 0.10
Niobium (Nb)≤ 0.05
Titanium (Ti)≤ 0.04
Carbon Equivalent (CE)≤ 0.43

⚙️ Mechanical Properties

PropertyValue
Yield Strength (Rt0.5)415-565 MPa
Tensile Strength (Rm)520-760 MPa
Elongation (A)≥ 18%
Yield to Tensile Ratio≤ 0.93
Hardness (HRC)22-28
Impact Energy (CVN at 0°C)≥ 27 J
Impact Energy (CVN at -20°C)≥ 20 J
Fatigue Limit (10&sup7; cycles)180-220 MPa
Young's Modulus210 GPa
Poisson's Ratio0.30
Shear Modulus80 GPa

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)54 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (20°C)0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity13.7 mm²/s
Emissivity (oxidized surface)0.79

📏 Product Specifications

SpecificationAvailable Options
Product FormsSeamless Pipes, Welded Pipes, Plates, Coils
Pipe Diameter Range6.35-1422 mm (1/4"-56")
Wall Thickness2.11-80 mm
Plate Thickness6-100 mm
Length Range5.8-18.3 m (Random/Fixed)
Manufacturing StandardsAPI 5L, ISO 3183, ASTM A1018, EN 10208
End FinishPlain End, Beveled End
Surface FinishBlack, Varnished, 3PE Coated, FBE Coated
Testing RequirementsHydrostatic, NDT, Chemical Analysis, Mechanical Testing
Dimensional Tolerance±1% (Diameter), ±12.5% (Wall Thickness)
Delivery ConditionAs-Rolled, Normalized, TMCP

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing API 5L X60

Manufacturing Advantage 1

Advanced TMCP Manufacturing Technology

MetalZenith employs cutting-edge Thermomechanical Controlled Processing (TMCP) with precise temperature control and accelerated cooling systems, ensuring optimal microstructure refinement and superior mechanical properties in our API 5L X60 steel production.

Comprehensive Quality Control Systems

Our integrated quality management system includes real-time chemical composition monitoring, automated mechanical testing, advanced NDT inspection, and full dimensional verification, guaranteeing consistent API 5L X60 steel quality that exceeds international standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain & Custom Solutions

MetalZenith offers flexible customization options for API 5L X60 steel including specialized dimensions, surface treatments, and delivery schedules, supported by our worldwide distribution network and technical engineering services for project-specific requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo