AISI H21

AISI H21

AISI H21 Tungsten Hot Work Tool Steel

AISI H21 is a premium tungsten-type hot work tool steel renowned for its exceptional high-temperature strength, thermal shock resistance, and superior wear characteristics. This chromium-tungsten-vanadium alloy steel is specifically engineered for demanding hot work applications where tools must maintain their properties under extreme thermal cycling conditions.

MetalZenith Manufacturing Excellence

At MetalZenith, we leverage our state-of-the-art vacuum induction melting and electroslag remelting technologies to produce AISI H21 with exceptional cleanliness and homogeneity. Our advanced metallurgical processes ensure optimal carbide distribution and grain structure refinement, delivering superior mechanical properties and extended tool life. Our precision-controlled heat treatment facilities enable us to achieve consistent hardness profiles and dimensional stability across all product forms.

Key Applications & Industries

  • Hot forging dies and punches for automotive and aerospace components
  • Extrusion dies for aluminum and copper alloys
  • Die casting dies for non-ferrous metals
  • Hot shearing blades and trimming tools
  • Mandrels and piercing tools for tube manufacturing

Quality Assurance & Global Supply

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control protocols including ultrasonic testing, chemical analysis, and mechanical property verification. Our global distribution network ensures reliable supply chain management with technical support services available worldwide. We offer complete customization capabilities including precision machining, heat treatment services, and application-specific engineering solutions.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

AISI H21 is a tungsten-type hot work tool steel characterized by its high tungsten content (8.5-10.0%) which provides exceptional high-temperature strength and thermal shock resistance. The steel's microstructure consists of a tempered martensitic matrix with uniformly distributed tungsten and vanadium carbides. These carbides maintain their hardness and wear resistance at elevated temperatures, making H21 ideal for hot work applications. The chromium content (3.0-3.75%) enhances hardenability and provides moderate corrosion resistance.

Heat Treatment Process

MetalZenith employs precision-controlled heat treatment cycles optimized for AISI H21. Annealing is performed at 870-900°C followed by slow cooling to achieve maximum machinability. Hardening involves preheating to 650-700°C, then heating to 1000-1030°C in a protective atmosphere, followed by air cooling or oil quenching depending on section size. Tempering is conducted at 540-650°C to achieve the desired working hardness of 42-48 HRC. Double tempering is recommended to ensure dimensional stability and stress relief.

Manufacturing Process Excellence

Our manufacturing process begins with vacuum induction melting (VIM) using high-purity raw materials, followed by electroslag remelting (ESR) to eliminate inclusions and achieve exceptional cleanliness. The ingots undergo controlled forging and rolling operations to refine the grain structure and ensure uniform carbide distribution. Hot working is performed within the temperature range of 1150-850°C with careful control of deformation rates to prevent cracking. All products undergo comprehensive ultrasonic testing, chemical analysis, and mechanical property verification.

Quality Standards & Certifications

MetalZenith maintains ISO 9001:2015 certification and complies with international standards including ASTM A681, EN ISO 4957, and JIS SKD61. Our quality control laboratory is equipped with advanced testing equipment including optical emission spectrometers, universal testing machines, hardness testers, and metallographic analysis systems. Each batch undergoes rigorous testing including chemical composition verification, mechanical property testing, microstructure examination, and dimensional inspection. Complete material traceability and certification documentation is provided with every shipment.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.28 - 0.35
Manganese (Mn)0.15 - 0.40
Silicon (Si)0.15 - 0.40
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Chromium (Cr)3.00 - 3.75
Tungsten (W)8.50 - 10.00
Vanadium (V)0.30 - 0.60
Nickel (Ni)≤ 0.30
Molybdenum (Mo)≤ 0.30
Copper (Cu)≤ 0.25

⚙️ Mechanical Properties

PropertyValueCondition
Tensile Strength1380 - 1520 MPaHardened & Tempered
Yield Strength (0.2% offset)1240 - 1380 MPaHardened & Tempered
Elongation8 - 12%Hardened & Tempered
Reduction of Area25 - 35%Hardened & Tempered
Hardness (HRC)42 - 48Working Hardness
Hardness (HRC)52 - 58Maximum Hardness
Impact Energy (Charpy V-notch)15 - 25 JRoom Temperature
Fatigue Limit620 - 690 MPa10&sup7; cycles
Modulus of Elasticity210 - 220 GPaRoom Temperature
Poisson's Ratio0.27 - 0.30Room Temperature

🔬 Physical Properties

PropertyValueTemperature
Density8.15 g/cm³20°C
Melting Point1480 - 1520°C-
Thermal Conductivity24.5 W/m·K20°C
Thermal Conductivity28.8 W/m·K400°C
Thermal Expansion Coefficient11.2×10-6/K20-100°C
Thermal Expansion Coefficient12.8×10-6/K20-400°C
Specific Heat Capacity460 J/kg·K20°C
Electrical Resistivity0.65 µΩ·m20°C
Magnetic PermeabilityFerromagneticRoom Temperature
Thermal Diffusivity6.5×10-6 m²/s20°C

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsRound bars, flat bars, plates, blocks, forgingsASTM A681
Round Bar Diameter10 - 500 mmASTM A681
Flat Bar Thickness8 - 150 mmASTM A681
Plate Thickness20 - 300 mmASTM A681
Block DimensionsUp to 1000×500×300 mmCustom
Surface FinishHot rolled, annealed, turned, groundASTM A681
Dimensional Tolerance±0.5 mm (standard), ±0.1 mm (precision)ISO 2768
LengthUp to 6000 mm (standard), longer availableCustom
Heat Treatment ConditionAnnealed, normalized, hardened & temperedASTM A681
Quality StandardsISO 9001:2015, ASTM A681, EN ISO 4957International

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing AISI H21

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith employs vacuum induction melting (VIM) and electroslag remelting (ESR) processes to produce AISI H21 with exceptional cleanliness and homogeneity. Our controlled atmosphere melting eliminates inclusions and ensures optimal carbide distribution, resulting in superior mechanical properties and extended tool life performance.

Precision Heat Treatment Control

Our state-of-the-art heat treatment facilities feature computer-controlled furnaces with precise temperature uniformity and atmosphere control. We implement proprietary heat treatment cycles optimized for AISI H21, ensuring consistent hardness profiles, dimensional stability, and maximum thermal shock resistance across all product forms.

Manufacturing Advantage 2
Manufacturing Advantage 3

Complete Customization & Technical Support

MetalZenith offers comprehensive customization services including precision machining, surface treatments, and application-specific heat treatment. Our metallurgical engineering team provides technical consultation, failure analysis, and tool optimization services, supported by our global supply chain and rapid delivery capabilities.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo