Skip to product information
1 of 1

A2 Tool Steel

A2 Tool Steel

A2 Air-Hardening Tool Steel

A2 is a premium air-hardening tool steel renowned for its exceptional combination of toughness, wear resistance, and dimensional stability. This versatile cold work tool steel offers superior machinability in the annealed condition and excellent hardenability, making it ideal for precision tooling applications requiring consistent performance and extended service life.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum melting and controlled forging processes to produce A2 tool steel with superior cleanliness and microstructural uniformity. Our advanced heat treatment facilities ensure optimal carbide distribution and precise hardness control, delivering consistent mechanical properties throughout the material cross-section.

Key Applications

  • Cutting tools including punches, dies, and shear blades
  • Cold forming and stamping dies for automotive components
  • Precision bearing races and rolling elements
  • Machine tool components and spindles
  • Measuring instruments and gauges

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including ultrasonic testing, comprehensive hardness mapping, and detailed carbide analysis. Our A2 tool steel meets ASTM A681 specifications and undergoes specialized testing for dimensional stability and fatigue resistance, ensuring reliability in critical precision applications.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

A2 tool steel exhibits a martensitic microstructure with uniformly distributed chromium and molybdenum carbides after proper heat treatment. The controlled carbide morphology provides excellent wear resistance while maintaining adequate toughness. The air-hardening characteristic eliminates quench cracking risks and ensures dimensional stability during heat treatment.

Heat Treatment Process

MetalZenith employs controlled atmosphere hardening at 925-980°C followed by air cooling to achieve optimal hardness. Tempering at 150-540°C allows precise hardness adjustment while maintaining dimensional stability. Our vacuum heat treatment capabilities ensure consistent results and superior surface quality.

Manufacturing Process

Our A2 production utilizes vacuum induction melting followed by electroslag remelting for exceptional cleanliness. Controlled forging with precise temperature monitoring ensures optimal carbide distribution and grain refinement. Advanced machining capabilities provide tight tolerances and superior surface finishes for demanding tool applications.

Specialized Quality Testing

MetalZenith conducts comprehensive Rockwell hardness distribution mapping across tool cross-sections, X-ray diffraction analysis for residual austenite content verification, detailed metallographic examination of carbide size and distribution, and rotating beam fatigue testing to validate tool life expectations in service conditions.

Application-Specific Considerations

For cutting tool applications, our A2 provides excellent edge retention and dimensional stability. In die manufacturing, the superior toughness prevents premature failure while maintaining wear resistance. For bearing applications, the fine carbide structure ensures smooth operation and extended service life. Precision machinery components benefit from the excellent machinability and dimensional stability, while automotive tooling applications leverage the consistent hardness and fatigue resistance.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.95 - 1.05
Chromium (Cr)4.75 - 5.50
Molybdenum (Mo)0.90 - 1.40
Vanadium (V)0.15 - 0.50
Manganese (Mn)0.40 - 1.00
Silicon (Si)0.10 - 0.60
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.025

⚙️ Mechanical Properties

PropertyValue
Hardness (HRC)57 - 62
Compressive Strength (MPa)2800 - 3200
Impact Toughness (J)15 - 25
Wear Resistance Index8.5 - 9.2
Hardenability (mm)75 - 100
Fatigue Strength (MPa)850 - 950

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.86
Melting Point (°C)1480 - 1520
Thermal Conductivity (W/m·K)24.3
Thermal Expansion (×10??/K)11.9
Elastic Modulus (GPa)210
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsBars, Plates, Blocks, Precision Ground Stock
Diameter Range6 - 300mm
Thickness Range3 - 200mm
Length Range100 - 6000mm
Standards ComplianceASTM A681, AISI A2, DIN 1.2363
Heat Treatment ConditionAnnealed, Hardened & Tempered
Surface FinishHot Rolled, Cold Drawn, Precision Ground

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing A2 Tool Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes vacuum induction melting followed by electroslag remelting to achieve exceptional cleanliness and homogeneity in A2 tool steel. Our controlled forging process with precise temperature monitoring ensures optimal carbide distribution and grain structure refinement for superior tool performance.

Comprehensive Quality Testing Protocol

Our specialized testing includes Rockwell hardness distribution mapping, residual austenite content analysis via X-ray diffraction, carbide distribution evaluation through metallographic analysis, and rotating beam fatigue testing to ensure consistent performance in demanding tool applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Heat Treatment Services

MetalZenith offers tailored heat treatment solutions including controlled atmosphere hardening, precision tempering, and stress relieving services. Our technical team provides comprehensive support for tool design optimization and performance enhancement based on specific application requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo