The 1045 cold rolled round bar is a precision-machined steel product known for its strength and hardness. Ideal for applications that require high accuracy and smooth surface finishes, this bar is commonly used in industries such as manufacturing, automotive, and construction. It offers a good balance of toughness and wear resistance, making it suitable for a range of structural and mechanical uses.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Technical Description:

1045 Cold Rolled Round Bar is a medium carbon steel with excellent strength and wear resistance properties. This grade offers good machinability and is widely used in applications requiring moderate strength and toughness. The cold rolling process provides improved surface finish, dimensional accuracy, and enhanced mechanical properties compared to hot rolled material.

Key Features:

  • Medium carbon content providing good strength-to-weight ratio
  • Excellent machinability and weldability
  • Good wear resistance and durability
  • Superior surface finish from cold rolling process
  • Heat treatable for enhanced properties
  • Cost-effective solution for structural applications

Manufacturing Process: Cold rolled from hot rolled billets through precision rolling mills, ensuring consistent dimensional accuracy and improved surface quality. Optional heat treatment available for specific property requirements.

Applications: Machinery components, shafts, axles, bolts, studs, gears, automotive parts, construction hardware, agricultural equipment, and general engineering applications requiring moderate strength and good machinability.

🧪 Chemical Composition

Chemical Composition:
Element Min % Max % Typical % ASTM A108 Requirement
Carbon (C) 0.43 0.50 0.46 0.43-0.50
Manganese (Mn) 0.60 0.90 0.75 0.60-0.90
Phosphorus (P) - 0.040 0.025 ≤ 0.040
Sulfur (S) - 0.050 0.030 ≤ 0.050
Silicon (Si) - 0.40 0.25 ≤ 0.40
Chromium (Cr) - 0.25 0.15 ≤ 0.25
Nickel (Ni) - 0.25 0.15 ≤ 0.25
Molybdenum (Mo) - 0.06 0.03 ≤ 0.06
Iron (Fe) Balance Balance 98.1 Balance

⚙️ Mechanical Properties

Mechanical Properties:
Property ASTM Requirement Typical Value Test Method Temperature
Tensile Strength 625 MPa min 690 MPa ASTM A370 Room Temp
Yield Strength (0.2%) 415 MPa min 450 MPa ASTM A370 Room Temp
Elongation 12% min 16% ASTM A370 Room Temp
Reduction of Area 35% min 40% ASTM A370 Room Temp
Hardness (Brinell) 187-229 HB 200 HB ASTM E10 Room Temp
Hardness (Rockwell C) - 20 HRC ASTM E18 Room Temp
Modulus of Elasticity - 205 GPa ASTM E111 Room Temp
Impact Energy (Charpy V) - 54 J ASTM E23 Room Temp

🔬 Physical Properties

Physical Properties:
Property Value Unit Temperature Test Standard
Density 7.87 g/cm3 20¡ãC ASTM B311
Melting Point 1470-1520 ¡ãC - DSC Analysis
Thermal Conductivity 49.8 W/m·K 100¡ãC ASTM E1461
Specific Heat 486 J/kg·K 0-100¡ãC ASTM C351
Linear Expansion 12.2 μm/m·K 0-100¡ãC ASTM E228
Electrical Resistivity 162 nΩ·m 20¡ãC ASTM B193
Magnetic Permeability High μ/μ₀ Room Temp Ferromagnetic
Curie Temperature 770 ¡ãC - Magnetic transition

📏 Product Specifications

Product Specifications:
Specification Available Range Standard Length Custom Available Tolerance
Diameter 6mm - 300mm Various Yes ±0.13mm
Length 1m - 12m 6m Yes +25mm/-0mm
Surface Finish Cold Rolled, Turned, Ground Cold Rolled Yes Ra ≤ 1.6μm
Straightness 0.5mm/m max Standard Precision ASTM A108
End Condition Saw Cut, Machined Saw Cut Yes Square ±1¡ã
Heat Treatment Annealed, Normalized Cold Rolled Yes Customer spec
Standards Compliance ASTM A108, SAE 1045 ASTM A108 Multiple Full compliance
Certification Mill TC, EN 10204 3.1 Mill TC Yes Standard
Test Certificate Chemical, Mechanical Standard Extended Per standard
Packaging Bundles, Crates, Pallets Bundles Custom Export standard

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing 1045 Cold Rolled Round Bar

Manufacturing Advantage 1

Precision Cold Rolling Process

Advanced cold rolling technology ensures superior dimensional accuracy and consistently tight tolerances throughout the bar length. This process creates an exceptionally smooth surface finish while improving the material's mechanical properties through work hardening.

Enhanced Surface Quality

The cold rolling manufacturing process produces bars with excellent surface smoothness and roundness, minimizing the need for additional finishing operations. This results in reduced machining time and cost for end-users.

Manufacturing Advantage 2
Manufacturing Advantage 3

Improved Material Strength

Cold rolling refines the steel's grain structure, significantly increasing its yield strength and hardness compared to hot-rolled alternatives. This manufacturing method delivers superior mechanical properties without requiring additional heat treatment.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo