420B Stainless Steel: Properties and Key Applications
Share
Table Of Content
Table Of Content
420B stainless steel is a martensitic stainless steel known for its high strength and moderate corrosion resistance. Classified under the martensitic family, it primarily contains chromium as its main alloying element, which contributes to its corrosion resistance and hardness. The typical composition includes approximately 12-14% chromium, along with carbon (around 0.15-0.25%), and smaller amounts of manganese, silicon, and phosphorus. This composition allows 420B to achieve a balance of hardness and toughness, making it suitable for various applications.
Comprehensive Overview
420B stainless steel is characterized by its ability to be hardened through heat treatment, which enhances its mechanical properties. The steel exhibits excellent wear resistance and is often used in applications requiring high strength and moderate corrosion resistance. Its unique combination of properties makes it particularly valuable in the manufacturing of cutting tools, surgical instruments, and various industrial components.
Advantages of 420B Stainless Steel:
- High Hardness: Achieves high hardness levels after heat treatment, making it suitable for cutting and wear-resistant applications.
- Moderate Corrosion Resistance: Offers reasonable resistance to corrosion, particularly in mildly corrosive environments.
- Good Mechanical Properties: Retains strength and toughness, even at elevated temperatures.
Limitations of 420B Stainless Steel:
- Lower Corrosion Resistance Compared to Austenitic Grades: While it has decent corrosion resistance, it is not as resistant as austenitic stainless steels like 304 or 316.
- Brittleness in Certain Conditions: Can become brittle if not properly heat-treated or if subjected to extreme conditions.
- Difficult to Weld: Welding can be challenging due to its high carbon content, which may lead to cracking.
Historically, 420B has been significant in the development of stainless steels, particularly in applications where a combination of hardness and corrosion resistance is required. Its market position remains relevant, especially in industries focused on manufacturing tools and components that endure wear and tear.
Alternative Names, Standards, and Equivalents
| Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
|---|---|---|---|
| UNS | S42000 | USA | Closest equivalent to AISI 420 |
| AISI/SAE | 420B | USA | Minor compositional differences to AISI 420 |
| ASTM | A276 | USA | Standard specification for stainless steel bars |
| EN | 1.4021 | Europe | Equivalent to AISI 420 with slight variations |
| JIS | SUS420J2 | Japan | Similar properties but with different carbon content |
The table above highlights various standards and equivalents for 420B stainless steel. Notably, while 420B and AISI 420 are often considered equivalent, the specific carbon content can influence their performance in applications. For instance, AISI 420 typically has a higher carbon content, which can enhance hardness but may also affect ductility.
Key Properties
Chemical Composition
| Element (Symbol) | Percentage Range (%) |
|---|---|
| Carbon (C) | 0.15 - 0.25 |
| Chromium (Cr) | 12.0 - 14.0 |
| Manganese (Mn) | 1.0 max |
| Silicon (Si) | 1.0 max |
| Phosphorus (P) | 0.04 max |
| Sulfur (S) | 0.03 max |
The primary alloying elements in 420B stainless steel include chromium, which enhances corrosion resistance and hardness, and carbon, which increases strength and wear resistance. Manganese and silicon are present in minor amounts to improve toughness and deoxidation during steelmaking.
Mechanical Properties
| Property | Condition/Temper | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
|---|---|---|---|---|
| Tensile Strength | Annealed | 600 - 800 MPa | 87 - 116 ksi | ASTM E8 |
| Yield Strength (0.2% offset) | Annealed | 400 - 600 MPa | 58 - 87 ksi | ASTM E8 |
| Elongation | Annealed | 12 - 20% | 12 - 20% | ASTM E8 |
| Hardness (Rockwell C) | Annealed | 30 - 40 HRC | 30 - 40 HRC | ASTM E18 |
| Impact Strength | - | 30 J at -20°C | 22 ft-lbf at -4°F | ASTM E23 |
The mechanical properties of 420B stainless steel make it suitable for applications requiring high strength and wear resistance. Its tensile and yield strengths indicate that it can withstand significant loads, while its elongation percentage suggests reasonable ductility, which is essential for forming processes.
Physical Properties
| Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
|---|---|---|---|
| Density | - | 7.75 g/cm³ | 0.28 lb/in³ |
| Melting Point | - | 1450 - 1510 °C | 2642 - 2750 °F |
| Thermal Conductivity | 20 °C | 25 W/m·K | 14.5 BTU·in/h·ft²·°F |
| Specific Heat Capacity | 20 °C | 500 J/kg·K | 0.12 BTU/lb·°F |
| Electrical Resistivity | 20 °C | 0.74 µΩ·m | 0.0000013 Ω·in |
| Coefficient of Thermal Expansion | 20 - 100 °C | 16.5 µm/m·K | 9.2 µin/in·°F |
The density of 420B stainless steel indicates it is relatively heavy, which is typical for martensitic steels. Its melting point is significant for applications involving high-temperature operations. The thermal conductivity and specific heat capacity suggest that while it can conduct heat, it is not as efficient as some other materials, which is a consideration in thermal applications.
Corrosion Resistance
| Corrosive Agent | Concentration (%) | Temperature (°C/°F) | Resistance Rating | Notes |
|---|---|---|---|---|
| Chlorides | 3-10 | 20-60 / 68-140 | Fair | Risk of pitting corrosion |
| Sulfuric Acid | 10-20 | 20-40 / 68-104 | Poor | Not recommended |
| Acetic Acid | 5-10 | 20-40 / 68-104 | Good | Moderate resistance |
| Atmospheric | - | - | Good | Performs well in dry air |
420B stainless steel exhibits moderate resistance to corrosion, particularly in atmospheric conditions and diluted acids. However, it is susceptible to pitting in chloride environments, which can be a critical consideration in marine applications. Compared to austenitic grades like 316, which offer superior corrosion resistance, 420B may not be suitable for highly corrosive environments.
Heat Resistance
| Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
|---|---|---|---|
| Max Continuous Service Temp | 400 °C | 752 °F | Suitable for intermittent service |
| Max Intermittent Service Temp | 600 °C | 1112 °F | Limited oxidation resistance at high temps |
| Scaling Temperature | 700 °C | 1292 °F | Risk of scaling beyond this temperature |
At elevated temperatures, 420B stainless steel maintains its strength but may begin to lose hardness and toughness. Oxidation can occur at high temperatures, necessitating careful consideration in applications involving heat exposure.
Fabrication Properties
Weldability
| Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
|---|---|---|---|
| TIG | ER420 | Argon | Preheat recommended |
| MIG | ER420 | Argon + CO2 | Post-weld heat treatment may be required |
Welding 420B stainless steel can be challenging due to its high carbon content, which can lead to cracking. Preheating before welding and post-weld heat treatment are often recommended to mitigate these issues.
Machinability
| Machining Parameter | 420B Stainless Steel | AISI 1212 | Notes/Tips |
|---|---|---|---|
| Relative Machinability Index | 50 | 100 | Moderate machinability |
| Typical Cutting Speed (Turning) | 30 m/min | 60 m/min | Use carbide tools for best results |
420B stainless steel has moderate machinability, which can be improved with appropriate tooling and cutting speeds. It is advisable to use carbide tools for effective machining.
Formability
420B stainless steel is not particularly formable due to its high strength and hardness. Cold forming is possible but may require significant force, and care must be taken to avoid cracking. Hot forming is more feasible, allowing for better shaping without compromising the material's integrity.
Heat Treatment
| Treatment Process | Temperature Range (°C/°F) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
|---|---|---|---|---|
| Annealing | 800 - 900 / 1472 - 1652 | 1 - 2 hours | Air cooling | Reduce hardness, improve ductility |
| Hardening | 1000 - 1100 / 1832 - 2012 | 30 - 60 minutes | Oil quenching | Increase hardness |
| Tempering | 200 - 600 / 392 - 1112 | 1 hour | Air cooling | Reduce brittleness, enhance toughness |
Heat treatment processes significantly affect the microstructure and properties of 420B stainless steel. Hardening increases hardness through martensitic transformation, while tempering helps reduce brittleness, making it more suitable for practical applications.
Typical Applications and End Uses
| Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection (Brief) |
|---|---|---|---|
| Medical | Surgical instruments | High hardness, corrosion resistance | Durability and sterilization |
| Manufacturing | Cutting tools | Wear resistance, strength | Longevity in use |
| Automotive | Valve components | High strength, moderate corrosion resistance | Performance under stress |
420B stainless steel is commonly used in the medical field for surgical instruments due to its hardness and ability to be sterilized. In manufacturing, it is favored for cutting tools where wear resistance is critical.
Important Considerations, Selection Criteria, and Further Insights
| Feature/Property | 420B Stainless Steel | AISI 440C | AISI 316 | Brief Pro/Con or Trade-off Note |
|---|---|---|---|---|
| Key Mechanical Property | High hardness | Higher hardness | Lower hardness | 440C offers better wear resistance |
| Key Corrosion Aspect | Moderate resistance | Poor | Excellent | 316 is better for corrosive environments |
| Weldability | Challenging | Difficult | Good | 316 is easier to weld |
| Machinability | Moderate | Poor | Good | 316 is easier to machine |
| Formability | Limited | Limited | Good | 316 offers better formability |
| Approx. Relative Cost | Moderate | Higher | Moderate | 440C is typically more expensive |
| Typical Availability | Common | Less common | Common | 316 is widely available |
When selecting 420B stainless steel, considerations include its mechanical properties, corrosion resistance, and fabrication characteristics. While it offers a good balance of hardness and corrosion resistance, alternatives like AISI 440C may provide better wear resistance, and AISI 316 may be preferred for applications in highly corrosive environments. Cost and availability also play crucial roles in material selection, with 420B being a cost-effective option for many applications.