Aluminium Properties And Key Applications Glossary
Aluminum 6101: Composition, Properties, Temper ...
Comprehensive Overview 6101 is an aluminium alloy in the 6xxx series, which is an Al-Si-Mg family of heat-treatable alloys. Its classification places it alongside other Al-Si-Mg alloys where precipitation hardening...
Aluminum 6101: Composition, Properties, Temper ...
Comprehensive Overview 6101 is an aluminium alloy in the 6xxx series, which is an Al-Si-Mg family of heat-treatable alloys. Its classification places it alongside other Al-Si-Mg alloys where precipitation hardening...
Aluminum 6070: Composition, Properties, Temper ...
Comprehensive Overview Aluminum alloy 6070 is a member of the 6xxx series of aluminum alloys, which are characterized by magnesium and silicon as their principal alloying additions. The alloying balance...
Aluminum 6070: Composition, Properties, Temper ...
Comprehensive Overview Aluminum alloy 6070 is a member of the 6xxx series of aluminum alloys, which are characterized by magnesium and silicon as their principal alloying additions. The alloying balance...
Aluminum 6069: Composition, Properties, Temper ...
Comprehensive Overview 6069 is a member of the 6xxx series aluminum alloys, which are alloyed primarily with magnesium and silicon to form the Mg2Si strengthening phase. As a 6xxx series...
Aluminum 6069: Composition, Properties, Temper ...
Comprehensive Overview 6069 is a member of the 6xxx series aluminum alloys, which are alloyed primarily with magnesium and silicon to form the Mg2Si strengthening phase. As a 6xxx series...
Aluminum 6066: Composition, Properties, Temper ...
Comprehensive Overview The 6066 alloy belongs to the 6xxx series of aluminum–magnesium–silicon alloys, which are defined by a Mg-Si alloying system that forms Mg2Si precipitates during heat treatment. As a...
Aluminum 6066: Composition, Properties, Temper ...
Comprehensive Overview The 6066 alloy belongs to the 6xxx series of aluminum–magnesium–silicon alloys, which are defined by a Mg-Si alloying system that forms Mg2Si precipitates during heat treatment. As a...
Aluminum 6026: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6026 is a member of the 6xxx series aluminum alloys, which are Al-Mg-Si systems that respond to precipitation hardening. Its chemistry places it among heat-treatable, medium-strength alloys...
Aluminum 6026: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6026 is a member of the 6xxx series aluminum alloys, which are Al-Mg-Si systems that respond to precipitation hardening. Its chemistry places it among heat-treatable, medium-strength alloys...
Aluminum 6085: Composition, Properties, Temper ...
Comprehensive Overview 6085 is an aluminum alloy that belongs to the 6xxx series (Al-Mg-Si) family, characterized by magnesium and silicon as its primary alloying elements. This series is heat-treatable by...
Aluminum 6085: Composition, Properties, Temper ...
Comprehensive Overview 6085 is an aluminum alloy that belongs to the 6xxx series (Al-Mg-Si) family, characterized by magnesium and silicon as its primary alloying elements. This series is heat-treatable by...
Aluminum 6081: Composition, Properties, Temper ...
Comprehensive Overview 6081 is a member of the 6xxx series aluminum alloys, which are aluminum-magnesium-silicon (Al-Mg-Si) alloys. This family is defined by the Mg2Si strengthening system and is generally heat-treatable...
Aluminum 6081: Composition, Properties, Temper ...
Comprehensive Overview 6081 is a member of the 6xxx series aluminum alloys, which are aluminum-magnesium-silicon (Al-Mg-Si) alloys. This family is defined by the Mg2Si strengthening system and is generally heat-treatable...
Aluminum 7055: Composition, Properties, Temper ...
Comprehensive Overview 7055 is a 7xxx series aluminum alloy, placing it squarely in the high-strength Al-Zn-Mg-Cu family that is widely used in aerospace applications. The alloy is deliberately formulated with...
Aluminum 7055: Composition, Properties, Temper ...
Comprehensive Overview 7055 is a 7xxx series aluminum alloy, placing it squarely in the high-strength Al-Zn-Mg-Cu family that is widely used in aerospace applications. The alloy is deliberately formulated with...
Aluminum 7010: Composition, Properties, Temper ...
Comprehensive Overview 7010 is a high-strength aluminum alloy in the 7xxx series, characterized primarily as an Al-Zn-Mg-Cu system. It belongs to the heat-treatable family of aluminum alloys where precipitation hardening...
Aluminum 7010: Composition, Properties, Temper ...
Comprehensive Overview 7010 is a high-strength aluminum alloy in the 7xxx series, characterized primarily as an Al-Zn-Mg-Cu system. It belongs to the heat-treatable family of aluminum alloys where precipitation hardening...
Aluminum 7049: Composition, Properties, Temper ...
Comprehensive Overview 7049 is a high-strength aluminum alloy in the 7xxx series, which are Al-Zn-Mg(-Cu) alloys primarily used where high specific strength is required. Its chemistry centers on zinc as...
Aluminum 7049: Composition, Properties, Temper ...
Comprehensive Overview 7049 is a high-strength aluminum alloy in the 7xxx series, which are Al-Zn-Mg(-Cu) alloys primarily used where high specific strength is required. Its chemistry centers on zinc as...
Aluminum 7079: Composition, Properties, Temper ...
Comprehensive Overview 7079 is a high-strength, heat-treatable aluminum alloy in the 7xxx series, characterized by zinc as the primary alloying element with significant additions of magnesium and copper. It sits...
Aluminum 7079: Composition, Properties, Temper ...
Comprehensive Overview 7079 is a high-strength, heat-treatable aluminum alloy in the 7xxx series, characterized by zinc as the primary alloying element with significant additions of magnesium and copper. It sits...
Aluminum 7175: Composition, Properties, Temper ...
Comprehensive Overview 7175 is a high-strength aluminum alloy belonging to the 7xxx series, which is characterized by zinc as the principal alloying element. It is designed primarily for aerospace and...
Aluminum 7175: Composition, Properties, Temper ...
Comprehensive Overview 7175 is a high-strength aluminum alloy belonging to the 7xxx series, which is characterized by zinc as the principal alloying element. It is designed primarily for aerospace and...
Aluminum 7039: Composition, Properties, Temper ...
Comprehensive Overview Alloy 7039 belongs to the 7xxx series of aluminum alloys, a family characterized by zinc as the principal alloying element and often alloyed with magnesium and trace copper....
Aluminum 7039: Composition, Properties, Temper ...
Comprehensive Overview Alloy 7039 belongs to the 7xxx series of aluminum alloys, a family characterized by zinc as the principal alloying element and often alloyed with magnesium and trace copper....
Aluminum 7020: Composition, Properties, Temper ...
Comprehensive Overview 7020 is a 7xxx-series aluminum alloy (Al-Zn-Mg family) engineered for high strength with a focus on improved toughness and stress-corrosion performance compared with traditional 7xxx alloys. Its nominal...
Aluminum 7020: Composition, Properties, Temper ...
Comprehensive Overview 7020 is a 7xxx-series aluminum alloy (Al-Zn-Mg family) engineered for high strength with a focus on improved toughness and stress-corrosion performance compared with traditional 7xxx alloys. Its nominal...
Aluminum 7050: Composition, Properties, Temper ...
Comprehensive Overview 7050 is a member of the 7xxx series aluminum alloys, characterized by zinc as the principal alloying element and engineered primarily as a heat-treatable, precipitation-hardening aluminum. It was...
Aluminum 7050: Composition, Properties, Temper ...
Comprehensive Overview 7050 is a member of the 7xxx series aluminum alloys, characterized by zinc as the principal alloying element and engineered primarily as a heat-treatable, precipitation-hardening aluminum. It was...
Aluminum 7075: Composition, Properties, Temper ...
Comprehensive Overview 7075 is a member of the 7xxx series aluminum alloys, which are Zn-Mg-Cu based high-strength alloys designed primarily for structural applications. Its principal alloying elements are zinc (Zn)...
Aluminum 7075: Composition, Properties, Temper ...
Comprehensive Overview 7075 is a member of the 7xxx series aluminum alloys, which are Zn-Mg-Cu based high-strength alloys designed primarily for structural applications. Its principal alloying elements are zinc (Zn)...
Aluminum 6951: Composition, Properties, Temper ...
Comprehensive Overview 6951 is part of the 6xxx series of aluminum alloys, which are broadly classified as Al-Mg-Si alloys and are heat-treatable by precipitation hardening. It belongs to a subgroup...
Aluminum 6951: Composition, Properties, Temper ...
Comprehensive Overview 6951 is part of the 6xxx series of aluminum alloys, which are broadly classified as Al-Mg-Si alloys and are heat-treatable by precipitation hardening. It belongs to a subgroup...
Aluminum 6463: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6463 is a member of the 6xxx series of aluminum alloys, which are aluminum–magnesium–silicon alloys recognized primarily for being heat-treatable through precipitation hardening. The 6xxx family balances...
Aluminum 6463: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6463 is a member of the 6xxx series of aluminum alloys, which are aluminum–magnesium–silicon alloys recognized primarily for being heat-treatable through precipitation hardening. The 6xxx family balances...
Aluminum 6260: Composition, Properties, Temper ...
Comprehensive Overview 6260 is a member of the 6xxx series of aluminum alloys, a family defined by magnesium and silicon as the principal alloying elements that form Mg2Si precipitates. It...
Aluminum 6260: Composition, Properties, Temper ...
Comprehensive Overview 6260 is a member of the 6xxx series of aluminum alloys, a family defined by magnesium and silicon as the principal alloying elements that form Mg2Si precipitates. It...
Aluminum 6201: Composition, Properties, Temper ...
Comprehensive Overview 6201 is a member of the 6xxx series aluminum alloys (Al‑Mg‑Si family) that are heat‑treatable and designed for a combination of moderate strength, good extrudability, and reasonable corrosion...
Aluminum 6201: Composition, Properties, Temper ...
Comprehensive Overview 6201 is a member of the 6xxx series aluminum alloys (Al‑Mg‑Si family) that are heat‑treatable and designed for a combination of moderate strength, good extrudability, and reasonable corrosion...
Aluminum 6181: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6181 is a member of the 6xxx series of aluminum alloys (Al-Mg-Si family) and is principally strengthened by precipitation hardening following solution heat treatment and artificial aging....
Aluminum 6181: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6181 is a member of the 6xxx series of aluminum alloys (Al-Mg-Si family) and is principally strengthened by precipitation hardening following solution heat treatment and artificial aging....
Aluminum 6067: Composition, Properties, Temper ...
Comprehensive Overview AA 6067 is a member of the 6xxx series of aluminum alloys, which are Al-Mg-Si heat-treatable alloys commonly used for structural and extrusion applications. The alloy is primarily...
Aluminum 6067: Composition, Properties, Temper ...
Comprehensive Overview AA 6067 is a member of the 6xxx series of aluminum alloys, which are Al-Mg-Si heat-treatable alloys commonly used for structural and extrusion applications. The alloy is primarily...
Aluminum 6042: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6042 is a member of the 6xxx series of aluminum alloys, which are primarily Al-Mg-Si systems amenable to precipitation hardening. Its chemistry places it among heat-treatable, medium-strength...
Aluminum 6042: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6042 is a member of the 6xxx series of aluminum alloys, which are primarily Al-Mg-Si systems amenable to precipitation hardening. Its chemistry places it among heat-treatable, medium-strength...
Aluminum 6065: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6065 is a member of the 6xxx series of wrought aluminum-magnesium-silicon alloys that are principally strengthened by precipitation of Mg2Si precipitates during heat treatment. Major alloying elements...
Aluminum 6065: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6065 is a member of the 6xxx series of wrought aluminum-magnesium-silicon alloys that are principally strengthened by precipitation of Mg2Si precipitates during heat treatment. Major alloying elements...
Aluminum 7072: Composition, Properties, Temper ...
Comprehensive Overview Alloy 7072 belongs to the 7xxx series family of aluminum alloys and is best described as an aluminum–zinc-bearing cladding alloy developed to provide enhanced corrosion protection for high-strength...
Aluminum 7072: Composition, Properties, Temper ...
Comprehensive Overview Alloy 7072 belongs to the 7xxx series family of aluminum alloys and is best described as an aluminum–zinc-bearing cladding alloy developed to provide enhanced corrosion protection for high-strength...
Aluminum 7042: Composition, Properties, Temper ...
Comprehensive Overview 7042 is a 7xxx-series aluminum alloy within the Al-Zn-Mg family that leans to medium–high strength through precipitation hardening. Its principal alloying elements are zinc and magnesium with minor...
Aluminum 7042: Composition, Properties, Temper ...
Comprehensive Overview 7042 is a 7xxx-series aluminum alloy within the Al-Zn-Mg family that leans to medium–high strength through precipitation hardening. Its principal alloying elements are zinc and magnesium with minor...
Aluminum 7034: Composition, Properties, Temper ...
Comprehensive Overview 7034 is a 7xxx-series aluminum alloy, placed in the high-strength Al-Zn-Mg(-Cu) family where zinc is the primary alloying addition. Its designation indicates a Zn–Mg–Cu precipitation-hardenable system that is...
Aluminum 7034: Composition, Properties, Temper ...
Comprehensive Overview 7034 is a 7xxx-series aluminum alloy, placed in the high-strength Al-Zn-Mg(-Cu) family where zinc is the primary alloying addition. Its designation indicates a Zn–Mg–Cu precipitation-hardenable system that is...
Aluminum 7150: Composition, Properties, Temper ...
Comprehensive Overview 7150 is a 7xxx-series aluminum alloy belonging to the high-strength Al‑Zn‑Mg‑Cu family used extensively in aerospace-grade structural applications. Its chemistry centers on zinc as the principal alloying element...
Aluminum 7150: Composition, Properties, Temper ...
Comprehensive Overview 7150 is a 7xxx-series aluminum alloy belonging to the high-strength Al‑Zn‑Mg‑Cu family used extensively in aerospace-grade structural applications. Its chemistry centers on zinc as the principal alloying element...
Aluminum 7056: Composition, Properties, Temper ...
Comprehensive Overview 7056 is a high-strength aluminum alloy in the 7xxx series (Al-Zn-Mg-Cu) family, formulated for applications that require very high static and fatigue strength combined with aerospace-quality toughness. The...
Aluminum 7056: Composition, Properties, Temper ...
Comprehensive Overview 7056 is a high-strength aluminum alloy in the 7xxx series (Al-Zn-Mg-Cu) family, formulated for applications that require very high static and fatigue strength combined with aerospace-quality toughness. The...
Aluminum 7015: Composition, Properties, Temper ...
Comprehensive Overview Alloy 7015 is a member of the 7xxx series of aluminum alloys, a family dominated by zinc as the principal alloying element and typically augmented with magnesium and...
Aluminum 7015: Composition, Properties, Temper ...
Comprehensive Overview Alloy 7015 is a member of the 7xxx series of aluminum alloys, a family dominated by zinc as the principal alloying element and typically augmented with magnesium and...