Aluminium Properties And Key Applications Glossary
Aluminum 5182: Composition, Properties, Temper ...
Comprehensive Overview 5182 is a member of the aluminum 5xxx series, an alloy class dominated by magnesium as the primary alloying element. The 5xxx family is categorized as non-heat-treatable, deriving...
Aluminum 5182: Composition, Properties, Temper ...
Comprehensive Overview 5182 is a member of the aluminum 5xxx series, an alloy class dominated by magnesium as the primary alloying element. The 5xxx family is categorized as non-heat-treatable, deriving...
Aluminum 5056: Composition, Properties, Temper ...
Comprehensive Overview 5056 is a member of the 5xxx series aluminum-magnesium alloys, characterized by magnesium as the principal alloying element. It belongs to the non-heat-treatable group where strength is primarily...
Aluminum 5056: Composition, Properties, Temper ...
Comprehensive Overview 5056 is a member of the 5xxx series aluminum-magnesium alloys, characterized by magnesium as the principal alloying element. It belongs to the non-heat-treatable group where strength is primarily...
Aluminum 5082: Composition, Properties, Temper ...
Comprehensive Overview 5082 is a member of the 5xxx series of wrought aluminum alloys, characterized primarily by magnesium as the principal alloying element. It is a non-heat-treatable, strain-hardenable alloy that...
Aluminum 5082: Composition, Properties, Temper ...
Comprehensive Overview 5082 is a member of the 5xxx series of wrought aluminum alloys, characterized primarily by magnesium as the principal alloying element. It is a non-heat-treatable, strain-hardenable alloy that...
Aluminum 5456: Composition, Properties, Temper ...
Comprehensive Overview 5456 is a member of the 5xxx series aluminum–magnesium alloys, characterized by moderate-to-high magnesium content and non-heat-treatable strengthening. The alloy sits among higher-magnesium variants used where strength and...
Aluminum 5456: Composition, Properties, Temper ...
Comprehensive Overview 5456 is a member of the 5xxx series aluminum–magnesium alloys, characterized by moderate-to-high magnesium content and non-heat-treatable strengthening. The alloy sits among higher-magnesium variants used where strength and...
Aluminum 5251: Composition, Properties, Temper ...
Comprehensive Overview 5251 is a member of the 5xxx series aluminum alloys, which are magnesium-based, non-heat-treatable alloys offering a balance of strength and corrosion resistance. Its chemistry places it among...
Aluminum 5251: Composition, Properties, Temper ...
Comprehensive Overview 5251 is a member of the 5xxx series aluminum alloys, which are magnesium-based, non-heat-treatable alloys offering a balance of strength and corrosion resistance. Its chemistry places it among...
Aluminum 5154: Composition, Properties, Temper ...
Comprehensive Overview 5154 is a member of the 5xxx series of aluminum–magnesium alloys, characterized by magnesium as the principal alloying element and by non-heat-treatable strengthening behavior. It sits in the...
Aluminum 5154: Composition, Properties, Temper ...
Comprehensive Overview 5154 is a member of the 5xxx series of aluminum–magnesium alloys, characterized by magnesium as the principal alloying element and by non-heat-treatable strengthening behavior. It sits in the...
Aluminum 5050: Composition, Properties, Temper ...
Comprehensive Overview 5050 is a member of the 5xxx series aluminum alloys, which are magnesium-bearing, wrought alloys characterized by non-heat-treatable strengthening. The alloy is formulated around aluminum with magnesium as...
Aluminum 5050: Composition, Properties, Temper ...
Comprehensive Overview 5050 is a member of the 5xxx series aluminum alloys, which are magnesium-bearing, wrought alloys characterized by non-heat-treatable strengthening. The alloy is formulated around aluminum with magnesium as...
Aluminum 5754: Composition, Properties, Temper ...
Comprehensive Overview 5754 is a member of the 5xxx series of aluminum alloys, an Al‑Mg family typified by magnesium as the principal alloying addition. It is commonly supplied in wrought...
Aluminum 5754: Composition, Properties, Temper ...
Comprehensive Overview 5754 is a member of the 5xxx series of aluminum alloys, an Al‑Mg family typified by magnesium as the principal alloying addition. It is commonly supplied in wrought...
Aluminum 5053: Composition, Properties, Temper ...
Comprehensive Overview 5053 is a 5xxx-series aluminum-magnesium alloy, classified primarily under Al-Mg wrought alloys. It belongs to the non-heat-treatable family where strengthening is achieved by solid-solution and strain hardening rather...
Aluminum 5053: Composition, Properties, Temper ...
Comprehensive Overview 5053 is a 5xxx-series aluminum-magnesium alloy, classified primarily under Al-Mg wrought alloys. It belongs to the non-heat-treatable family where strengthening is achieved by solid-solution and strain hardening rather...
Aluminum 5150: Composition, Properties, Temper ...
Comprehensive Overview 5150 is an aluminum alloy placed in the 5xxx series, a family defined by magnesium as the principal alloying element. This series is characterized by alloys that are...
Aluminum 5150: Composition, Properties, Temper ...
Comprehensive Overview 5150 is an aluminum alloy placed in the 5xxx series, a family defined by magnesium as the principal alloying element. This series is characterized by alloys that are...
Aluminum 5080: Composition, Properties, Temper ...
Comprehensive Overview Alloy 5080 is a member of the 5xxx series aluminum-magnesium family, categorized as a non-heat-treatable (work-hardenable) alloy. Its primary strengthening mechanism is solid-solution strengthening from magnesium combined with...
Aluminum 5080: Composition, Properties, Temper ...
Comprehensive Overview Alloy 5080 is a member of the 5xxx series aluminum-magnesium family, categorized as a non-heat-treatable (work-hardenable) alloy. Its primary strengthening mechanism is solid-solution strengthening from magnesium combined with...
Aluminum 5657: Composition, Properties, Temper ...
Comprehensive Overview 5657 is a member of the 5xxx series of wrought aluminum–magnesium alloys, placing it firmly in the non-heat-treatable, strain-hardened family favored for a balance of strength and corrosion...
Aluminum 5657: Composition, Properties, Temper ...
Comprehensive Overview 5657 is a member of the 5xxx series of wrought aluminum–magnesium alloys, placing it firmly in the non-heat-treatable, strain-hardened family favored for a balance of strength and corrosion...
Aluminum 5450: Composition, Properties, Temper ...
Comprehensive Overview 5450 is a member of the 5xxx series aluminum alloys, a family characterized by magnesium as the principal alloying addition. The 5xxx series are non-heat-treatable alloys whose elevated...
Aluminum 5450: Composition, Properties, Temper ...
Comprehensive Overview 5450 is a member of the 5xxx series aluminum alloys, a family characterized by magnesium as the principal alloying addition. The 5xxx series are non-heat-treatable alloys whose elevated...
Aluminum 5152: Composition, Properties, Temper ...
Comprehensive Overview Alloy 5152 is a member of the 5xxx series of aluminum alloys, characterized by magnesium as the principal alloying element. It is a non-heat-treatable, strain-hardenable alloy whose primary...
Aluminum 5152: Composition, Properties, Temper ...
Comprehensive Overview Alloy 5152 is a member of the 5xxx series of aluminum alloys, characterized by magnesium as the principal alloying element. It is a non-heat-treatable, strain-hardenable alloy whose primary...
Aluminum 5051: Composition, Properties, Temper ...
Comprehensive Overview 5051 is a member of the 5xxx series of aluminum alloys, which are magnesium-strengthened, non-heat-treatable alloys. Its primary alloying element is magnesium, typically in the low-to-mid percentage range,...
Aluminum 5051: Composition, Properties, Temper ...
Comprehensive Overview 5051 is a member of the 5xxx series of aluminum alloys, which are magnesium-strengthened, non-heat-treatable alloys. Its primary alloying element is magnesium, typically in the low-to-mid percentage range,...
Aluminum 6020: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6020 belongs to the 6xxx series of aluminium alloys, which are aluminium‑magnesium‑silicon (Al‑Mg‑Si) heat‑treatable alloys. The 6xxx family is characterized by Mg2Si precipitation hardening; 6020 is formulated...
Aluminum 6020: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6020 belongs to the 6xxx series of aluminium alloys, which are aluminium‑magnesium‑silicon (Al‑Mg‑Si) heat‑treatable alloys. The 6xxx family is characterized by Mg2Si precipitation hardening; 6020 is formulated...
Aluminum 6013: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6013 is a member of the 6xxx series aluminum alloys, which are primarily Al-Mg-Si based with additions that promote precipitation hardening. It contains silicon and magnesium as...
Aluminum 6013: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6013 is a member of the 6xxx series aluminum alloys, which are primarily Al-Mg-Si based with additions that promote precipitation hardening. It contains silicon and magnesium as...
Aluminum 6010: Composition, Properties, Temper ...
Comprehensive Overview 6010 is a member of the 6xxx series aluminum alloys, which are primarily Al-Mg-Si systems designed for precipitation hardening. The 6xxx family combines moderate alloying with silicon and...
Aluminum 6010: Composition, Properties, Temper ...
Comprehensive Overview 6010 is a member of the 6xxx series aluminum alloys, which are primarily Al-Mg-Si systems designed for precipitation hardening. The 6xxx family combines moderate alloying with silicon and...
Aluminum 6005A: Composition, Properties, Temper...
Comprehensive Overview 6005A is a member of the 6xxx series aluminum alloys, a family defined by the Mg-Si binary system. This series is known for being heat-treatable by precipitation hardening...
Aluminum 6005A: Composition, Properties, Temper...
Comprehensive Overview 6005A is a member of the 6xxx series aluminum alloys, a family defined by the Mg-Si binary system. This series is known for being heat-treatable by precipitation hardening...
Aluminum 6005: Composition, Properties, Temper ...
Comprehensive Overview 6005 is a member of the 6xxx series aluminum alloys, which are Al-Mg-Si alloys primarily strengthened by precipitate hardening. It sits in the family of heat-treatable aluminum alloys...
Aluminum 6005: Composition, Properties, Temper ...
Comprehensive Overview 6005 is a member of the 6xxx series aluminum alloys, which are Al-Mg-Si alloys primarily strengthened by precipitate hardening. It sits in the family of heat-treatable aluminum alloys...
Aluminum 6060: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6060 is a member of the 6xxx series aluminum-magnesium-silicon family, positioned close to 6063 and 6061 in chemistry and application space. It is principally an Al-Mg-Si alloy...
Aluminum 6060: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6060 is a member of the 6xxx series aluminum-magnesium-silicon family, positioned close to 6063 and 6061 in chemistry and application space. It is principally an Al-Mg-Si alloy...
Aluminum 6082: Composition, Properties, Temper ...
Comprehensive Overview 6082 is a member of the 6xxx series of aluminum alloys, which are primarily aluminum-magnesium-silicon (Al-Mg-Si) compositions. This series is characterized by its ability to be strengthened by...
Aluminum 6082: Composition, Properties, Temper ...
Comprehensive Overview 6082 is a member of the 6xxx series of aluminum alloys, which are primarily aluminum-magnesium-silicon (Al-Mg-Si) compositions. This series is characterized by its ability to be strengthened by...
Aluminum 6063: Composition, Properties, Temper ...
Comprehensive Overview The alloy 6063 belongs to the 6xxx series of aluminum alloys, which are magnesium-silicon (Mg-Si) heat-treatable alloys designed primarily for extrusion and architectural applications. Magnesium and silicon form...
Aluminum 6063: Composition, Properties, Temper ...
Comprehensive Overview The alloy 6063 belongs to the 6xxx series of aluminum alloys, which are magnesium-silicon (Mg-Si) heat-treatable alloys designed primarily for extrusion and architectural applications. Magnesium and silicon form...
Aluminum 6061: Composition, Properties, Temper ...
Comprehensive Overview 6061 is a member of the 6xxx series of aluminum alloys, a family characterized by magnesium and silicon as the primary alloying elements that form the Mg2Si precipitate....
Aluminum 6061: Composition, Properties, Temper ...
Comprehensive Overview 6061 is a member of the 6xxx series of aluminum alloys, a family characterized by magnesium and silicon as the primary alloying elements that form the Mg2Si precipitate....
Aluminum 6063A: Composition, Properties, Temper...
Comprehensive Overview 6063A belongs to the 6xxx series of aluminum alloys, a family characterized by aluminum-magnesium-silicon chemistry optimized for extrusion and moderate strength through precipitation hardening. The principal alloying elements...
Aluminum 6063A: Composition, Properties, Temper...
Comprehensive Overview 6063A belongs to the 6xxx series of aluminum alloys, a family characterized by aluminum-magnesium-silicon chemistry optimized for extrusion and moderate strength through precipitation hardening. The principal alloying elements...
Aluminum 6061A: Composition, Properties, Temper...
Comprehensive Overview 6061A belongs to the 6xxx series of aluminum alloys, a family defined by magnesium and silicon as the principal alloying elements that form Mg2Si precipitates. The 6xxx series...
Aluminum 6061A: Composition, Properties, Temper...
Comprehensive Overview 6061A belongs to the 6xxx series of aluminum alloys, a family defined by magnesium and silicon as the principal alloying elements that form Mg2Si precipitates. The 6xxx series...
Aluminum 6262: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6262 is a member of the 6xxx series aluminum alloys, which are aluminum–magnesium–silicon based and classified as heat‑treatable precipitation‑strengthened alloys. 6262 distinguishes itself from common 6xxx alloys...
Aluminum 6262: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6262 is a member of the 6xxx series aluminum alloys, which are aluminum–magnesium–silicon based and classified as heat‑treatable precipitation‑strengthened alloys. 6262 distinguishes itself from common 6xxx alloys...
Aluminum 6160: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6160 is a member of the 6xxx series aluminum alloys (Al-Mg-Si family) characterized by precipitation hardening through Mg2Si formation. Its principal alloying elements are silicon and magnesium,...
Aluminum 6160: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6160 is a member of the 6xxx series aluminum alloys (Al-Mg-Si family) characterized by precipitation hardening through Mg2Si formation. Its principal alloying elements are silicon and magnesium,...
Aluminum 6151: Composition, Properties, Temper ...
Comprehensive Overview 6151 is a member of the 6xxx series aluminum alloys (Al-Mg-Si class) and is classified as a heat-treatable, precipitation-hardenable alloy. Its chemistry is dominated by magnesium and silicon...
Aluminum 6151: Composition, Properties, Temper ...
Comprehensive Overview 6151 is a member of the 6xxx series aluminum alloys (Al-Mg-Si class) and is classified as a heat-treatable, precipitation-hardenable alloy. Its chemistry is dominated by magnesium and silicon...
Aluminum 6111: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6111 belongs to the 6xxx series of aluminum alloys, a family characterized by the Mg-Si system that forms Mg2Si precipitates during heat treatment. It is a heat-treatable...
Aluminum 6111: Composition, Properties, Temper ...
Comprehensive Overview Alloy 6111 belongs to the 6xxx series of aluminum alloys, a family characterized by the Mg-Si system that forms Mg2Si precipitates during heat treatment. It is a heat-treatable...