ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

SUJ2

SUJ2

SUJ2 High Carbon Chrome Bearing Steel

SUJ2 is a premium high carbon chromium bearing steel specifically engineered for high-performance bearing applications and precision tooling. This through-hardening steel grade delivers exceptional hardness, wear resistance, and dimensional stability, making it the preferred choice for critical bearing components and precision cutting tools operating under demanding conditions.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum degassing and controlled cooling processes to produce SUJ2 steel with superior cleanliness and microstructural uniformity. Our advanced heat treatment facilities ensure optimal carbide distribution and maximum through-hardening capability, critical for achieving consistent performance in bearing and tooling applications.

Key Applications

  • Ball and roller bearing races and rolling elements
  • Precision cutting tools and dies
  • Automotive transmission components
  • High-precision machine tool spindles
  • Industrial pump and compressor bearings

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including ultrasonic testing for internal soundness, comprehensive hardness mapping, and detailed carbide distribution analysis. Our SUJ2 steel meets JIS G4805, ASTM A295, and ISO 683-17 standards, ensuring reliability in critical bearing and precision tooling applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

SUJ2 exhibits a martensitic microstructure after hardening with uniformly distributed chromium carbides that provide exceptional wear resistance. The high carbon content enables through-hardening to 60-65 HRC while maintaining adequate toughness for bearing applications. The controlled chromium content ensures optimal carbide formation without excessive brittleness.

Heat Treatment Process

MetalZenith employs controlled atmosphere hardening at 820-860°C followed by oil quenching and tempering at 150-200°C. Our vacuum furnaces ensure uniform heating and minimize decarburization. Specialized sub-zero treatment at -80°C transforms retained austenite for maximum dimensional stability in precision applications.

Advanced Manufacturing Process

Our production process includes vacuum induction melting, controlled forging with optimized reduction ratios, and stress-relief annealing. Advanced ESR (Electroslag Remelting) technology ensures exceptional cleanliness and homogeneity. Controlled cooling rates during spheroidizing annealing optimize carbide morphology for superior machinability.

Specialized Quality Testing

MetalZenith conducts comprehensive Rockwell hardness distribution mapping, X-ray diffraction analysis for residual austenite content (typically <3%), detailed carbide distribution evaluation using image analysis, and rotating bending fatigue testing per ASTM D7791. Ultrasonic inspection ensures internal soundness critical for bearing applications.

Application-Specific Technical Considerations

For bearing manufacturing, SUJ2 provides optimal contact fatigue resistance and dimensional stability under cyclic loading. In cutting tool applications, the uniform carbide distribution ensures consistent edge retention. Precision machinery components benefit from the excellent surface finish capability and minimal distortion during heat treatment. Automotive applications leverage the superior wear resistance and reliability under high-stress conditions.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.95 - 1.10
Chromium (Cr)1.30 - 1.60
Manganese (Mn)0.50 - 0.80
Silicon (Si)0.15 - 0.35
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.025
Molybdenum (Mo)≤ 0.08
Nickel (Ni)≤ 0.25

⚙️ Mechanical Properties

PropertyValue
Hardness (HRC)60 - 65
Compressive Strength (MPa)≥ 2500
Impact Toughness (J)15 - 25
Wear Resistance IndexExcellent (Grade A)
Hardenability (DI)≥ 80mm
Fatigue Strength (MPa)800 - 1000

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.81
Melting Point (°C)1420 - 1460
Thermal Conductivity (W/m·K)42.7
Thermal Expansion (×10??/K)11.5
Elastic Modulus (GPa)210
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsBars, Rods, Tubes, Forgings, Precision Ground Stock
Diameter Range10 - 300mm
Length Range1000 - 6000mm
Surface FinishHot Rolled, Cold Drawn, Precision Ground
Standards ComplianceJIS G4805, ASTM A295, ISO 683-17, DIN 100Cr6
Heat Treatment ConditionAnnealed, Spheroidized, Hardened & Tempered
Tolerance Classh9, h11 (Cold Drawn), IT11 (Hot Rolled)

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing SUJ2

Manufacturing Advantage 1

Advanced Vacuum Degassing Technology

MetalZenith utilizes advanced vacuum degassing and controlled atmosphere melting to minimize inclusions and achieve exceptional steel cleanliness. Our proprietary heat treatment process ensures uniform carbide distribution and optimal through-hardening characteristics essential for bearing steel performance.

Comprehensive Quality Testing Protocol

Our specialized testing includes Rockwell hardness mapping across sections, residual austenite content analysis, carbide distribution evaluation, and rotating bending fatigue testing. Advanced metallographic analysis ensures consistent microstructure and performance reliability in demanding applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Technical Support

MetalZenith offers tailored heat treatment cycles, precision machining services, and comprehensive technical support. Our metallurgical experts provide application-specific recommendations for optimal performance in bearing manufacturing and precision tooling applications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo