Premium GB 12Cr1MoVR Pressure Vessel Steel

MetalZenith proudly manufactures GB 12Cr1MoVR, a high-performance low-alloy steel specifically designed for pressure vessel applications operating at elevated temperatures. This chromium-molybdenum-vanadium steel grade offers exceptional creep resistance, thermal stability, and mechanical strength, making it ideal for critical industrial applications requiring reliable performance under demanding conditions.

MetalZenith Manufacturing Excellence

Our state-of-the-art production facilities utilize advanced electric arc furnace technology combined with vacuum degassing and ladle refining processes to ensure superior metallurgical quality. MetalZenith's precision-controlled heat treatment capabilities guarantee optimal microstructure development and consistent mechanical properties throughout each product batch.

Key Applications

  • Pressure vessels and boilers operating up to 540°C
  • Petrochemical processing equipment
  • Power generation components
  • Oil and gas industry applications
  • High-temperature piping systems

Quality Assurance

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control protocols including chemical analysis, mechanical testing, non-destructive examination, and dimensional verification. Our products comply with GB 713 standards and undergo rigorous third-party inspection to ensure complete traceability and certification compliance for critical applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

GB 12Cr1MoVR is a low-alloy steel specifically engineered for pressure vessel applications requiring excellent creep resistance and thermal stability. The chromium content provides oxidation resistance and hardenability, while molybdenum enhances high-temperature strength and creep resistance. Vanadium acts as a grain refiner and carbide former, contributing to improved mechanical properties and thermal stability.

Heat Treatment Process

MetalZenith employs a carefully controlled normalize and temper heat treatment cycle. Normalizing is performed at 920-960°C followed by air cooling to achieve uniform austenite grain structure. Tempering is conducted at 680-720°C to develop optimal strength-toughness balance and stress relief. Our computer-controlled furnaces ensure precise temperature uniformity within ±5°C throughout the heating cycle.

Manufacturing Process

Production begins with electric arc furnace melting using high-quality scrap and alloy additions. The molten steel undergoes ladle refining and vacuum degassing to achieve ultra-low sulfur and phosphorus levels. Continuous casting produces high-quality billets which are hot rolled to final dimensions. Critical process parameters including rolling temperature, reduction ratios, and cooling rates are precisely controlled to ensure optimal microstructure development.

Quality Standards and Testing

All products undergo comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical property verification through tensile and impact testing, and non-destructive examination using ultrasonic testing. Microstructural analysis confirms proper heat treatment and absence of harmful phases. MetalZenith maintains full traceability from raw materials through final inspection, ensuring compliance with GB 713 and international pressure vessel codes.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.08-0.15
Manganese (Mn)0.45-0.70
Silicon (Si)0.17-0.37
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.015
Chromium (Cr)1.00-1.50
Molybdenum (Mo)0.45-0.65
Vanadium (V)0.15-0.30
Nickel (Ni)≤ 0.30
Copper (Cu)≤ 0.20
Aluminum (Al)≥ 0.020

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Rm)510-680 MPa
Yield Strength (Rp0.2)≥ 295 MPa
Elongation (A)≥ 20%
Reduction of Area (Z)≥ 50%
Brinell Hardness (HB)153-207
Impact Energy (KV2) at 20°C≥ 34 J
Impact Energy (KV2) at 0°C≥ 27 J
Fatigue Limit (10^7 cycles)240-280 MPa
Young's Modulus210 GPa
Poisson's Ratio0.30
Creep Rupture Strength (100,000h at 540°C)≥ 137 MPa

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1480-1520°C
Thermal Conductivity (20°C)42 W/m·K
Thermal Conductivity (540°C)35 W/m·K
Thermal Expansion Coefficient (20-100°C)11.5×10-6/K
Thermal Expansion Coefficient (20-540°C)12.8×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity (20°C)0.28 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity (20°C)11.6×10-6 m²/s

📏 Product Specifications

SpecificationAvailable Options
Product FormsPlates, Sheets, Bars, Forgings, Tubes, Pipes
Plate Thickness6-200 mm
Sheet Thickness0.5-6 mm
Bar Diameter10-300 mm
Tube Outer Diameter15-600 mm
Wall Thickness (Tubes)2-50 mm
Standards ComplianceGB 713, ASME SA-387, EN 10028-2
Surface FinishHot Rolled, Normalized, Pickled, Machined
Dimensional Tolerance±0.1-0.5 mm (depending on form)
Length RangeUp to 12 meters
Heat Treatment ConditionNormalized and Tempered
Testing CertificatesMill Test Certificate, Third-Party Inspection

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing GB 12Cr1MoVR

Manufacturing Advantage 1

Advanced Vacuum Degassing Technology

MetalZenith employs cutting-edge vacuum degassing and ladle refining processes that significantly reduce hydrogen, oxygen, and nitrogen content, resulting in superior steel purity and enhanced mechanical properties with improved impact toughness and fatigue resistance.

Precision Heat Treatment Control

Our computer-controlled heat treatment facilities ensure precise temperature uniformity and cooling rates, guaranteeing optimal microstructure development and consistent mechanical properties throughout the entire cross-section of each product with full traceability documentation.

Manufacturing Advantage 2
Manufacturing Advantage 3

Comprehensive Customization Capabilities

MetalZenith offers extensive customization options including non-standard dimensions, special surface finishes, and tailored chemical compositions to meet specific application requirements, supported by our global logistics network ensuring timely delivery worldwide.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo