EN 100Cr6

EN 100Cr6

Premium EN 100Cr6 Bearing Steel from MetalZenith

EN 100Cr6 is a high-carbon chromium bearing steel renowned for its exceptional hardness, wear resistance, and dimensional stability. This premium grade steel, equivalent to AISI 52100 and JIS SUJ2, represents the gold standard for precision bearing applications across industries worldwide.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art vacuum induction melting and electroslag remelting technologies to produce ultra-clean EN 100Cr6 steel with minimal inclusions and superior metallurgical homogeneity. Our advanced processing capabilities include precision forging, controlled atmosphere heat treatment, and specialized surface finishing techniques that ensure optimal microstructure and performance characteristics.

Critical Applications & Industries

Our EN 100Cr6 steel serves demanding applications across multiple sectors:

  • High-precision ball and roller bearings for automotive, aerospace, and industrial machinery
  • Rolling mill rolls and precision tooling components
  • Valve components and wear-resistant machine parts
  • Measuring instruments and gauge blocks requiring dimensional stability

Quality Assurance & Global Standards

MetalZenith maintains ISO 9001:2015 and AS9100D certifications, ensuring every batch of EN 100Cr6 steel meets stringent international standards. Our comprehensive testing protocols include chemical analysis, mechanical property verification, ultrasonic inspection, and microstructural examination, guaranteeing consistent quality and traceability for mission-critical applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN 100Cr6 is a through-hardening bearing steel with a hypereutectoid carbon content of approximately 1.0%. The steel's microstructure consists of fine pearlite in the annealed condition, transforming to martensite with dispersed chromium carbides upon hardening. The chromium content (1.35-1.65%) provides enhanced hardenability and wear resistance while maintaining dimensional stability during heat treatment.

Heat Treatment Process

MetalZenith's optimized heat treatment cycle includes:

  • Spheroidizing anneal at 750-780°C for stress relief and machinability
  • Austenitizing at 820-860°C with precise temperature control (±5°C)
  • Oil or salt bath quenching for uniform cooling rates
  • Tempering at 150-200°C to achieve target hardness of 60-67 HRC

Manufacturing Process Excellence

Our integrated manufacturing process begins with vacuum induction melting (VIM) followed by electroslag remelting (ESR) to achieve exceptional cleanliness levels. The steel undergoes controlled forging with grain flow optimization, followed by precision machining using advanced CNC equipment. Surface treatments include grinding to Ra 0.1 µm finish and optional coating applications for enhanced performance.

Quality Standards & Certifications

MetalZenith's EN 100Cr6 production complies with international standards including EN 10027-1, ASTM A295, and JIS G4805. Our quality management system encompasses:

  • Chemical composition verification using optical emission spectroscopy
  • Mechanical property testing per ASTM E8 and ASTM E23 standards
  • Ultrasonic inspection for internal soundness per ASTM A388
  • Microstructural analysis and grain size determination per ASTM E112
  • Dimensional inspection using coordinate measuring machines (CMM)

Application Engineering Support

MetalZenith provides comprehensive technical support including material selection guidance, heat treatment optimization, and failure analysis services. Our metallurgical engineers collaborate with customers to develop application-specific solutions, ensuring optimal performance in demanding bearing and tooling applications.

🧪 Chemical Composition

ElementComposition (%)Standard Range
Carbon (C)0.95 - 1.05EN 10027-1
Chromium (Cr)1.35 - 1.65EN 10027-1
Manganese (Mn)0.25 - 0.45EN 10027-1
Silicon (Si)0.15 - 0.35EN 10027-1
Phosphorus (P)≤ 0.025Max
Sulfur (S)≤ 0.015Max
Nickel (Ni)≤ 0.30Max
Copper (Cu)≤ 0.25Max
Aluminum (Al)≤ 0.050Max
Oxygen (O)≤ 0.0015MetalZenith Premium

⚙️ Mechanical Properties

PropertyValueCondition
Tensile Strength2100 - 2400 MPaHardened & Tempered
Yield Strength (0.2%)≥ 1650 MPaHardened & Tempered
Elongation8 - 12%Hardened & Tempered
Reduction of Area25 - 35%Hardened & Tempered
Hardness (HRC)60 - 67Hardened & Tempered
Hardness (Annealed)≤ 255 HBAnnealed
Impact Energy (Charpy V)15 - 25 JRoom Temperature
Fatigue Limit900 - 1100 MPa10&sup7; cycles
Modulus of Elasticity210 GPaRoom Temperature
Poisson's Ratio0.27 - 0.30Room Temperature

🔬 Physical Properties

PropertyValueTemperature
Density7.81 g/cm³20°C
Melting Point1480 - 1520°C-
Thermal Conductivity42.6 W/m·K20°C
Thermal Expansion Coefficient12.1×10-6/K20-100°C
Specific Heat Capacity460 J/kg·K20°C
Electrical Resistivity0.25 µΩ·m20°C
Magnetic PermeabilityFerromagneticRoom Temperature
Curie Temperature750°C-
Thermal Diffusivity11.8 mm²/s20°C
Coefficient of Thermal Expansion13.2×10-6/K20-200°C

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsRound bars, Square bars, Flat bars, Plates, Sheets, Tubes, Wire, ForgingsEN 10027-1
Round Bar Diameter6mm - 500mmEN 10060
Square Bar Size10mm - 200mmEN 10059
Plate Thickness3mm - 100mmEN 10029
Standard Lengths3m, 6m, 12m (Custom lengths available)EN 10060
Surface FinishHot rolled, Cold drawn, Turned, Ground, PolishedEN 10221
Dimensional Toleranceh9, h10, h11 (Precision: ±0.05mm)ISO 286-2
Heat Treatment ConditionAnnealed, Normalized, Hardened & TemperedEN 10027-1
Quality GradesStandard, Premium, Ultra-clean (VIM/ESR)MetalZenith Spec
Equivalent StandardsAISI 52100, JIS SUJ2, DIN 1.3505International

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN 100Cr6

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith employs cutting-edge vacuum induction melting (VIM) and electroslag remelting (ESR) processes to produce ultra-clean EN 100Cr6 steel with exceptional purity levels. Our controlled atmosphere melting reduces oxygen and nitrogen content to ≤ 10 ppm, minimizing non-metallic inclusions and ensuring superior fatigue life and reliability in critical bearing applications.

Precision Heat Treatment & Quality Control

Our state-of-the-art heat treatment facilities feature computer-controlled furnaces with precise temperature uniformity (±3°C) and atmosphere control. Every batch undergoes comprehensive testing including hardness mapping, microstructural analysis, and dimensional verification using advanced coordinate measuring machines (CMM) with ±0.001mm accuracy.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain & Custom Solutions

MetalZenith's integrated supply chain spans multiple continents with strategically located processing centers and inventory hubs. We offer comprehensive customization services including precision machining, surface treatments, and packaging solutions. Our technical team provides application-specific material optimization and rapid prototyping services with typical lead times of 2-4 weeks for custom specifications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo