20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
AISI 6150 is a medium-carbon, low-alloy steel with chromium and vanadium additions that provide enhanced hardenability, strength, and fatigue resistance. The chromium content improves corrosion resistance and hardenability, while vanadium acts as a grain refiner and carbide former, contributing to improved toughness and wear resistance. The steel exhibits excellent through-hardening properties in sections up to 100mm diameter.
Heat Treatment Process
MetalZenith employs controlled atmosphere furnaces for optimal heat treatment of AISI 6150. Austenitizing is performed at 845-870°C, followed by oil quenching to achieve martensitic structure. Tempering at 400-650°C develops the desired combination of strength and toughness. Our computer-controlled systems ensure uniform heating rates and precise temperature control throughout the process, resulting in consistent mechanical properties.
Manufacturing Process
Our AISI 6150 steel production begins with electric arc furnace melting using premium scrap and alloy additions. Secondary refining through ladle furnace and vacuum degassing ensures low inclusion content and optimal cleanliness. Continuous casting produces high-quality billets, which are subsequently hot rolled or forged to final dimensions. Advanced rolling mill technology with computerized process control ensures excellent surface quality and dimensional accuracy.
Quality Standards & Testing
MetalZenith maintains strict quality control throughout production, conducting chemical analysis via optical emission spectrometry, mechanical testing including tensile, impact, and fatigue testing, and metallographic examination. All products comply with ASTM A29, SAE J404, and EN 10083-3 standards. Non-destructive testing including ultrasonic and magnetic particle inspection ensures internal soundness. Complete material certification and test reports accompany every shipment.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.48 - 0.53 |
| Manganese (Mn) | 0.70 - 1.00 |
| Silicon (Si) | 0.15 - 0.30 |
| Phosphorus (P) | ≤ 0.035 |
| Sulfur (S) | ≤ 0.040 |
| Chromium (Cr) | 0.80 - 1.10 |
| Vanadium (V) | 0.15 - 0.25 |
| Nickel (Ni) | ≤ 0.25 |
| Copper (Cu) | ≤ 0.25 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength (Quenched & Tempered) | 1380 - 1620 MPa |
| Yield Strength (0.2% Offset) | ≥ 1240 MPa |
| Elongation in 50mm | ≥ 10% |
| Reduction of Area | ≥ 40% |
| Hardness (Quenched & Tempered) | 42 - 48 HRC |
| Impact Energy (Charpy V-notch) | ≥ 27 J |
| Fatigue Limit (10&sup7; cycles) | 620 - 690 MPa |
| Elastic Modulus | 210 GPa |
| Poisson's Ratio | 0.27 - 0.30 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.85 g/cm³ |
| Melting Point | 1480 - 1520°C |
| Thermal Expansion Coefficient (20-100°C) | 11.5×10-6/K |
| Thermal Conductivity (at 20°C) | 42 W/m·K |
| Specific Heat Capacity | 460 J/kg·K |
| Electrical Resistivity | 0.25 µΩ·m |
| Magnetic Permeability | Ferromagnetic |
| Curie Temperature | 770°C |
📏 Product Specifications
| Specification | Available Options |
|---|---|
| Product Forms | Round bars, flat bars, plates, sheets, forgings, wire |
| Round Bar Diameter | 6mm - 300mm |
| Flat Bar Dimensions | 10mm - 150mm thickness, up to 500mm width |
| Plate Thickness | 8mm - 100mm |
| Length | Up to 12 meters (custom lengths available) |
| Standards | ASTM A29, ASTM A322, SAE J404, EN 10083-3 |
| Surface Finish | Hot rolled, cold drawn, peeled, ground, machined |
| Dimensional Tolerance | ±0.1mm to ±0.5mm (depending on size and finish) |
| Heat Treatment Condition | Annealed, normalized, quenched & tempered |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing AISI 6150
Advanced Heat Treatment Technology
MetalZenith utilizes computer-controlled atmosphere furnaces with precise temperature profiling and quench rate optimization to achieve superior microstructure uniformity and mechanical properties in AISI 6150 steel, ensuring consistent performance across all product dimensions.
Comprehensive Quality Testing
Our state-of-the-art testing laboratory performs extensive fatigue testing, Charpy impact analysis, and stress-strain evaluation on every production lot, guaranteeing that our AISI 6150 steel meets or exceeds industry standards for spring applications and high-stress components.
Custom Processing & Global Supply
MetalZenith offers complete customization services including precision cutting, heat treatment to customer specifications, and surface finishing. Our global distribution network ensures reliable delivery of AISI 6150 steel products worldwide with full technical support and engineering consultation.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
สอบถามด่วน
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications