Alloy | ASTM | Characteristics |
---|---|---|
A36 | ASTM A36 |
Construction and structural support in building frameworks. Manufacturing of trailers and heavy equipment. Fabrication of industrial shelving and storage solutions. |
CHEMICAL COMPOSITION
- The chemical composition of this material is predominantly Iron (Fe) at 99%, with Carbon (C) at 0.26%, Manganese (Mn) at 0.75%, Copper (Cu) at 0.2%, and Phosphorus (P) and Sulfur (S) present in maximum amounts of 0.04% and 0.05% respectively.
MECHANICAL INFORMATION
- The mechanical information for this material indicates a density of 0.282 lb/in3 (7.8 g/cc) with ultimate tensile strength and yield tensile strength measured at 58,000 psi (400 MPa) and 47,700 psi (315 MPa) respectively. It possesses a shear strength of 43,500 psi (300 MPa) and a melting point ranging from 2,590 to 2,670°F (1,420 to 1,460°C). The material exhibits a hardness Brinell of 140 and is produced using the hot rolled method. The specifications provided should be regarded as general approximations; for precise material test reports, please contact our Customer Service Department.
AVAILABLE SIZES
- The available sizes for this category include: 3/4 inch by 3/8 inch by 1/8 inch with a depth of 0.75 inches, width of 0.375 inches, thickness of 1/8 inch, length of 240 inches, and weight of 0.560 lbs/ft; 1 inch by 1/2 inch by 1/8 inch with a depth of 1 inch, width of 0.5 inches, thickness of 1/8 inch, length of 240 inches, and weight of 0.840 lbs/ft; 1-1/4 inch by 1/2 inch by 1/8 inch with a depth of 1.25 inches, width of 0.5 inches, thickness of 1/8 inch, length of 240 inches, and weight of 0.990 lbs/ft; 1-1/2 inch by 1/2 inch by 1/8 inch with a depth of 1.5 inches, width of 0.5 inches, thickness of 1/8 inch, length of 240 inches, and weight of 1.119 lbs/ft; 1-1/2 inch by 9/16 inch by 3/16 inch with a depth of 1.5 inches, width of 0.563 inches, thickness of 3/16 inch, length of 240 inches, and weight of 1.440 lbs/ft; 1-1/2 inch by 3/4 inch by 1/8 inch with a depth of 1.5 inches, width of 0.75 inches, thickness of 1/8 inch, length of 240 inches, and weight of 1.170 lbs/ft; 2 inch by 1/2 inch by 1/8 inch with a depth of 2 inches, width of 0.5 inches, thickness of 1/8 inch, length of 240 inches, and weight of 1.430 lbs/ft; 2 inch by 9/16 inch by 3/16 inch with a depth of 2 inches, width of 0.563 inches, thickness of 3/16 inch, length of 240 inches, and weight of 1.860 lbs/ft; 2 inch by 5/8 inch by 1/4 inch with a depth of 2 inches, width of 0.625 inches, thickness of 1/4 inch, length of 240 inches, and weight of 2.280 lbs/ft; 2 inch by 1 inch by 1/8 inch with a depth of 2 inches, width of 1 inch, thickness of 1/8 inch, length of 240 inches, and weight of 1.590 lbs/ft; 2 inch by 1 inch by 3/16 inch with a depth of 2 inches, width of 1 inch, thickness of 3/16 inch, length of 240 inches, and weight of 2.319 lbs/ft; and 2-1/2 inch by 5/8 inch by 3/16 inch with a depth of 2.5 inches, width of 0.625 inches, thickness of 3/16 inch, length of 240 inches, and weight of 2.270 lbs/ft.