DOM Steel Round Tube is a high-quality, cold-drawn tube made from steel that is drawn over a mandrel and through a die to achieve precise dimensions and an excellent surface finish. This manufacturing process results in a seamless, uniform tube with superior mechanical properties, making it ideal for applications requiring strength, accuracy, and reliability, such as in hydraulic components, automotive parts, and general fabrication.

Vollständige Details anzeigen

Dapatkan Penawaran

Alloy ASTM Characteristics
1020 / 1026 / 520 May vary based on size ASTM A513

Mechanical and fluid applications such as hydraulic cylinders and automotive components.

Construction of structural supports and frames in machinery and equipment.

Precision applications requiring high dimensional accuracy and smooth surfaces.

CHEMICAL COMPOSITION

  • The chemical composition is defined by the following elements: Carbon (C) content ranges from 0.17 to 0.23 percent, Iron (Fe) constitutes 99.08 to 99.53 percent, Manganese (Mn) is present in 0.3 to 0.6 percent, Phosphorus (P) is a maximum of 0.04 percent, and Sulfur (S) reaches a maximum of 0.05 percent.

MECHANICAL INFORMATION

  • The mechanical information for this material category indicates an ultimate tensile strength of 132,000 psi (602 MPa) and a yield tensile strength of 74,185 psi (512 MPa). The hardness measurements are recorded as 90 on the Brinell scale and B75 on the Rockwell scale. The chemical composition consists of carbon at 0.17 - 0.23%, iron at 99.08 - 99.53%, manganese at 0.3 - 0.6%, and maximum levels of 0.04% phosphorus and 0.05% sulfur. These values represent approximate averages; please consult our customer service for specific material test reports.

AVAILABLE SIZES

  • The available sizes for this category include: 3/8" x 18ga with an outer diameter (OD) of 3/8", wall thickness of 0.049" (18ga), inner diameter (ID) of 0.277", length of 204.00", and weight of 0.171 Lb/Ft; 3/8" x 16ga with an OD of 3/8", wall thickness of 0.065" (16ga), ID of 0.245", length of 204.00", and weight of 0.220 Lb/Ft; 1/2" x 18ga with an OD of 1/2", wall thickness of 0.049" (18ga), ID of 0.402", length of 204.00", and weight of 0.236 Lb/Ft; 1/2" x 16ga with an OD of 1/2", wall thickness of 0.065" (16ga), ID of 0.37", length of 204.00", and weight of 0.302 Lb/Ft; 1/2" x 14ga with an OD of 1/2", wall thickness of 0.083" (14ga), ID of 0.334", length of 204.00", and weight of 0.370 Lb/Ft; 1/2" x 13ga with an OD of 1/2", wall thickness of 0.095" (13ga), ID of 0.31", length of 204.00", and weight of 0.411 Lb/Ft; 1/2" x 11ga with an OD of 1/2", wall thickness of 0.120" (11ga), ID of 0.26", length of 204.00", and weight of 0.487 Lb/Ft; 9/16" x 14ga with an OD of 9/16", wall thickness of 0.083" (14ga), ID of 0.3965", length of 204.00", and weight of 0.425 Lb/Ft; 9/16" x 13ga with an OD of 9/16", wall thickness of 0.095" (13ga), ID of 0.3725", length of 204.00", and weight of 0.475 Lb/Ft; 9/16" x 12ga with an OD of 9/16", wall thickness of 0.109" (12ga), ID of 0.3445", length of 204.00", and weight of 0.529 Lb/Ft; 5/8" x 14ga with an OD of 5/8", wall thickness of 0.083" (14ga), ID of 0.459", length of 204.00", and weight of 0.480 Lb/Ft; 5/8" x 11ga with an OD of 5/8", wall thickness of 0.120" (11ga), ID of 0.385", length of 204.00", and weight of 0.647 Lb/Ft; 3/4" x 16ga with an OD of 3/4", wall thickness of 0.065" (16ga), ID of 0.62", length of 204.00", and weight of 0.475 Lb/Ft; 3/4" x 14ga with an OD of 3/4", wall thickness of 0.083" (14ga), ID of 0.584", length of 204.00", and weight of 0.591 Lb/Ft; 3/4" x 13ga with an OD of 3/4", wall thickness of 0.095" (13ga), ID of 0.56", length of 204.00", and weight of 0.670 Lb/Ft; 3/4" x 12ga with an OD of 3/4", wall thickness of 0.109" (12ga), ID of 0.532", length of 204.00", and weight of 0.750 Lb/Ft; 3/4" x 11ga with an OD of 3/4", wall thickness of 0.120" (11ga), ID of 0.51", length of 204.00", and weight of 0.807 Lb/Ft; 3/4" x .156" with an OD of 3/4", wall thickness of 0.156", ID of 0.438", length of 204.00", and weight of 0.990 Lb/Ft; 3/4" x 3/16" with an OD of 3/4", wall thickness of 3/16", ID of 0.375", length of 204.00", and weight of 1.130 Lb/Ft; 3/4" x .219" with an OD of 3/4", wall thickness of 0.219", ID of 0.312", length of 204.00", and weight of 1.242 Lb/Ft; 3/4" x 1/4" with an OD of 3/4", wall thickness of 1/4", ID of 0.25", length of 204.00", and weight of 1.335 Lb/Ft.