Alloy | ASTM | Characteristics |
---|---|---|
A500 | ASTM A500 |
Traffic control and pedestrian safety in parking lots. Protection of storefronts and building entrances. Boundary definition in industrial and warehouse facilities. |
CHEMICAL COMPOSITION
- The chemical composition of this category includes a maximum of 0.3% carbon (C), 0.18% copper (Cu), 0.063% sulfur (S), and 0.05% phosphorus (P), with a minimum of 99% iron (Fe).
MECHANICAL INFORMATION
- The material consists predominantly of iron with a minimum composition of 99%, complemented by a maximum carbon content of 0.3%, copper at 0.18%, sulfur at 0.063%, and phosphorus at 0.05%. It exhibits a density of 0.282 lb/in3 (7.8 g/cc), an ultimate tensile strength of 58,000 psi (400 MPa), and a yield tensile strength of 46,000 psi (317 MPa). This material has a melting point of approximately 2,750°F (1,510°C) and is produced using the hot-rolled method, classified under Grade B. Available in various sizes, including 4", 6", and 8" Schedule 40 pipes, each with specified outer diameters, wall thicknesses, inner diameters, lengths, and weights per foot. For precise specifications and test reports, please contact the Customer Service Department.
AVAILABLE SIZES
- The available sizes for this category include the following nominal pipe sizes: a 4" SCH 40 x 7' pipe with an outside diameter (OD) of 4.5", wall thickness of 0.337", inside diameter (ID) of 3.826", a length of 84.00", and a weight of 10.789 lb/ft; a 6" SCH 40 x 7' pipe with an OD of 6.625", wall thickness of 0.28", ID of 6.065", the same length of 84.00", and a weight of 18.970 lb/ft; and an 8" SCH 40 x 7' pipe with an OD of 8.625", wall thickness of 0.322", ID of 7.981", a length also of 84.00", and a weight of 28.549 lb/ft.