Steel Properties And Key Applications Glossary

1008 Steel: Properties and Key Applications

1008 steel is classified as a low-carbon mild steel, primarily composed of iron with a carbon content of approximately 0.08%. This grade falls under the AISI/SAE classification system and is...

3 comments

1008 Steel: Properties and Key Applications

1008 steel is classified as a low-carbon mild steel, primarily composed of iron with a carbon content of approximately 0.08%. This grade falls under the AISI/SAE classification system and is...

3 comments

1006 Steel: Properties and Key Applications

1006 steel is classified as a low-carbon mild steel, primarily composed of iron with a carbon content typically around 0.06%. This steel grade is known for its excellent ductility, weldability,...

18 comments

1006 Steel: Properties and Key Applications

1006 steel is classified as a low-carbon mild steel, primarily composed of iron with a carbon content typically around 0.06%. This steel grade is known for its excellent ductility, weldability,...

18 comments

1005 Steel: Properties and Key Applications Ove...

1005 steel is classified as a low-carbon steel, primarily composed of iron with a carbon content of approximately 0.05%. This grade falls under the category of mild steel, which is...

2 comments

1005 Steel: Properties and Key Applications Ove...

1005 steel is classified as a low-carbon steel, primarily composed of iron with a carbon content of approximately 0.05%. This grade falls under the category of mild steel, which is...

2 comments

1004 Steel: Properties and Key Applications

1004 steel is classified as a low-carbon steel, specifically falling under the category of medium-carbon alloy steels. This grade typically contains a carbon content of approximately 0.04%, which contributes to...

3 comments

1004 Steel: Properties and Key Applications

1004 steel is classified as a low-carbon steel, specifically falling under the category of medium-carbon alloy steels. This grade typically contains a carbon content of approximately 0.04%, which contributes to...

3 comments

10.9 Steel: Properties, Hardness & Applications

10.9 Steel, commonly referred to as Bolt Grade 10.9, is a high-strength steel grade primarily used in the manufacturing of bolts and fasteners. It is classified as a medium-carbon alloy...

3 comments

10.9 Steel: Properties, Hardness & Applications

10.9 Steel, commonly referred to as Bolt Grade 10.9, is a high-strength steel grade primarily used in the manufacturing of bolts and fasteners. It is classified as a medium-carbon alloy...

3 comments

1.2312 Steel (P20+S): Properties and Key Applic...

1.2312 Steel (P20+S Type) is a high-performance tool steel primarily classified as a medium-carbon alloy steel. This grade is specifically designed for applications requiring high toughness and good machinability, making...

1.2312 Steel (P20+S): Properties and Key Applic...

1.2312 Steel (P20+S Type) is a high-performance tool steel primarily classified as a medium-carbon alloy steel. This grade is specifically designed for applications requiring high toughness and good machinability, making...

1.0718 Steel (11SMnPb30): Properties and Key Ap...

1.0718 Steel (11SMnPb30) is a low-alloy steel grade primarily classified as a free-cutting steel. It is characterized by its excellent machinability, making it a preferred choice in applications where precision...

1.0718 Steel (11SMnPb30): Properties and Key Ap...

1.0718 Steel (11SMnPb30) is a low-alloy steel grade primarily classified as a free-cutting steel. It is characterized by its excellent machinability, making it a preferred choice in applications where precision...

S235JR Steel: Properties and Key Applications

1.0037 Steel (S235JR) is a low-carbon structural steel grade that is widely used in construction and engineering applications. Classified under the European standard EN 10025, S235JR is known for its...

S235JR Steel: Properties and Key Applications

1.0037 Steel (S235JR) is a low-carbon structural steel grade that is widely used in construction and engineering applications. Classified under the European standard EN 10025, S235JR is known for its...

O1 Tool Steel: Properties and Key Applications

O1 Tool Steel, classified as a high-carbon, cold work tool steel, is primarily composed of iron with significant alloying elements such as carbon, chromium, and manganese. This steel grade is...

O1 Tool Steel: Properties and Key Applications

O1 Tool Steel, classified as a high-carbon, cold work tool steel, is primarily composed of iron with significant alloying elements such as carbon, chromium, and manganese. This steel grade is...